The mechanical behavior of titanium alloys has been mostly studied in quasi-static conditions when the strain rate does not exceed 10 s−1, while the studies performed in dynamic settings specifically for Ti-based composites are limited. Such data are critical to prevent the “strength margin” approach, which is used to assure the part performance under dynamic conditions in the absence of relevant data. The purpose of this study was to obtain data on the mechanical behavior of Ti-based composites under dynamic condition. The Metal Matrix Composites (MMC) on the base of the alloy Ti-6Al-4V (wt.%) were made using Blended Elemental Powder Metallurgy with different amounts of reinforcing particles: 5, 10, and 20% of TiC or 5, 10% (vol.) of TiB. Composites were studied at high strain rate compression ~1–3 × 103·s−1 using the split Hopkinson pressure bar. Mechanical behavior was analyzed considering strain rate, phase composition, microstructure, and strain energy (SE). It is shown that for the strain rates up to 1920 s−1, the strength and SE of MMC with 5% TiC are substantially higher compared to particles free alloy. The particles TiC localize the plastic deformation at the micro level, and fracturing occurs mainly by crushing particles and their aggregates. TiB MMCs have a finer grain structure and different mechanical behavior. MMC with 5 and 10% TiB do not break down at strain rates up to almost 3000 s−1; and 10% MMC surpasses other materials in the SE at strain rates exceeding 2200 s−1. The deformation mechanism of MMCs was evaluated.
The goal of the present work is a systematic study on an influence of a strain rate on the mechanical response and microstructure evolution of the selected titanium-based materials, i.e., commercial pure titanium, Ti-6Al-4V alloy with lamellar and globular microstructures produced via a conventional cast and wrought technology, as well as Ti-6Al-4V fabricated using blended elemental powder metallurgy (BEPM). The quasi-static and high-strain-rate compression tests using the split Hopkinson pressure bar (SHPB) technique were performed and microstructures of the specimens were characterized before and after compression testing. The strain rate effect was analyzed from the viewpoint of its influence on the stress–strain response, including the strain energy, and a microstructure of the samples after compressive loading. It was found out that the Ti-6Al-4V with a globular microstructure is characterized by high strength and high plasticity (ensuring the highest strain energy) in comparison to alloy with a lamellar microstructure, whereas Ti6-Al-4V obtained with BEPM reveals the highest plastic flow stress with good plasticity at the same time. The microstructure observations reveal that a principal difference in high-strain-rate behavior of the tested materials could be explained by the nature of the boundaries between the structural components through which plastic deformation is transmitted: α/α boundaries prevail in the globular microstructure, while α/β boundaries prevail in the lamellar microstructure. The Ti-6Al-4V alloy obtained with BEPM due to a finer microstructure has a significantly better balance of strength and plasticity as compared with conventional Ti-6Al-4V alloy with a similar type of the lamellar microstructure.
1 May 2014 in Transactions of Nonferrous Metals Society of China
This study is focused on the development and comprehensive analysis of the structural state and mechanical properties of a high-strength wrought aluminum alloy of the Al–Zn–Mg–Cu system, additionally alloyed with scandium (Sc) and zirconium (Zr). Alloys of this system are critically important materials for the aviation and defense industries due to their exceptional specific strength. The research addresses common challenges inherent to high-alloyed systems, such as susceptibility to hot cracking and dendritic segregation, by optimizing alloying element content and implementing innovative casting techniques. The scientific novelty of this work lies in the investigation of the synergistic effect of Sc and Zr on the alloy's microstructure specifically in the as-cast state, an area less explored compared to wrought semi-finished products. It was established that the formation of Al3(Sc, Zr) intermetallic compounds ensures significant grain refinement, enhances anti-recrystallization stability, and contributes to additional strengthening through the precipitation of secondary coherent nanoparticles that remain stable during subsequent heat treatment. The practical part of the research involved the production of a large-scale industrial ingot (150 mm in diameter) using a vacuum magnetohydrodynamic (MHD) installation and continuous casting into a short crystallizer with a thermal filling. This approach facilitated a uniform globular structure free of gas porosity, achieving a record-low hydrogen content (0.04–0.05 cm³/100 g). The evolution of the microstructure and phase transformations was studied using SEM, EDS, and DSC methods. Mechanical testing results demonstrated that the applied casting technology ensures high isotropy of properties in both longitudinal and transverse directions. The alloy was found to exhibit high technological plasticity (elongation up to 53%) at temperatures of 300–400 °C, allowing for the optimization of further thermomechanical processing parameters, such as forging and rolling. The initial interphase melting temperature was determined to be 471–477 °C, serving as a fundamental parameter for establishing precise homogenization and solution treatment regimes for the experimental alloy.
The microstructure, physical, and mechanical characteristics of 3D-printed metal products can be improved with high-energy heat treatment included in the manufacturing process. In the present study, Ti-6Al-4V titanium alloy products were 3D-printed with electron beam melting of wire of appropriate composition, while surface laser treatment of 3D-printed material was studied to determine the potential of microstructure modification and characteristics improvement. It was found that certain laser processing modes make it possible to eliminate micro defects (pores) in the samples that are harmful to structural materials. The obtained results also open the prospect of creating 3D-printed metal parts with specified profiles of physical and chemical properties, including gradients, as they model the change in material properties depending on the depth of the deposited layer during high-energy processing of each layer during its application. As demonstrated, both the condition of 3D printing as the velocity of deposition and thickness of each layer, the chemical composition and amount of impurities added to the matrix material during deposition, and the high-energy processing (heating or remelting) parameters are important to form the phase composition and mechanical properties of the final products. The high-energy processing also can be used to control the physicochemical properties of the product’s surface.