Wurtzite ferroelectrics are an emerging material class that expands the functionality and application space of wide bandgap semiconductors. Promising physical properties of binary wurtzite semiconductors include a large, reorientable spontaneous polarization, direct band gaps that span from the infrared to ultraviolet, large thermal conductivities and acoustic wave velocities, high mobility electron and hole channels, and low optical losses. The ability to reverse the polarization in ternary wurtzite semiconductors at room temperature enables memory and analog type functionality and quasi-phase matching in optical devices and boosts the ecosystem of wurtzite semiconductors, provided the appropriate combination of properties can be achieved for any given application. In this article, advances in the design, synthesis, and characterization of wurtzite ferroelectric materials and devices are discussed. Highlights include: the direct and quantitative observation of polarization reversal of ∼135 μC/cm2 charge in Al1−xBxN via electron microscopy, Al1−xBxN ferroelectric domain patterns poled down to 400 nm in width via scanning probe microscopy, and full polarization retention after over 1000 h of 200 °C baking and a 2× enhancement relative to ZnO in the nonlinear optical response of Zn1−xMgxO. The main tradeoffs, challenges, and opportunities in thin film deposition, heterostructure design and characterization, and device fabrication are overviewed.
The effective large signal longitudinal piezoelectric coefficient (d33,f∗) of piezoelectric thin films on rigid substrates has been widely investigated. Unclamped piezoelectric thin films are predicted to have a higher d33,f∗ coefficient due to reduced constraints on piezoelectric strain, domain reorientation, and domain wall motion, but quantitative measurements of this coefficient have been limited. This study uses microfabrication techniques along with double-beam laser interferometry (DBLI) to accurately determine the longitudinal piezoelectric coefficient of Pb(Zr,Ti)O3 thin films in partially released piezomicroelectromechanical structures. A two-step backside release process was used: first, deep reactive ion etching to create backside vias and second, wet etching of the ZnO sacrificial layer to release the area beneath the Pb(Zr,Ti)O3 thin films. Post wet etching, optical profilometry showed concavely deformed diaphragms resulting from asymmetrical stress profiles through the diaphragm thickness. DBLI was then used to examine diaphragm deflection under an applied unipolar voltage ranging from 0 to 10 V. Devices with 50% and 75% of the area beneath the top electrode released exhibited large signal d33,f∗ values of 410 ± 6 and 420 ± 8 pm/V, respectively, more than three times higher than the d33,f∗ value of the clamped samples: 126 ± 13 pm/V. The reasons contributing to the large d33,f∗ include (i) the change in stress levels due to the release process, (ii) the elimination of mechanical constraints from substrate clamping, and (iii) enhanced domain reorientation. These findings confirm that substrate declamping significantly boosts the piezoelectric coefficient, bringing d33,f∗ closer to the bulk longitudinal piezoelectric coefficient (d33).
The discovery of ferroelectricity in hafnium zirconium oxide (HfxZr1-xO2) and related fluorite materials has spurred interest in ferroelectric devices suitable for integration with silicon integrated circuits (ICs), especially those that can be embedded in the back-end-of-line (BEOL) process. More recently, ferroelectricity has been found in wurtzite aluminum nitride-based materials, such as scandium and boron-doped aluminum nitride (Al1-xScxN and Al1-xBxN). Although these materials currently have undesirably large coercive electric fields, and small breakdown electric field-to-coercive electric field ratio, their low processing temperatures and large remanent polarization offer intriguing possibilities for device applications. Here, we report ferroelectric field-effect transistors (FeFETs) with a 15 nm thick Al0.88B0.12N layer and an 11 nm ZnO semiconductor channel, achieving a memory window >1 V and switching voltages (Vswitch) <±10 V.