1 January 2008 in Operative Dentistry
Verified
Journal Article
Closed access
ERE. G. Reston
E. G. Reston
SFS. C. Filho
S. C. Filho
GAGuilherme Anziliero Arossi
Guilherme Anziliero Arossi
RCR. B. Cogo
R. B. Cogo
CRC. S. Rocha
C. S. Rocha
LCL. Q. Closs
L. Q. Closs
PURPOSE: This article provides an overview of dental ceramics. It addresses possible modes of failure and factors that may influence the decision to either repair or replace ceramic restorations. The authors' intention was to present ceramic repair as a reliable, low-cost, low-risk technique.

1 September 2020 in Brazilian Dental Journal
Verified
Journal Article
Open access
PDF file
JDJúlio César Lemos Duarte
Júlio César Lemos Duarte
ACAna Rosa Costa
Ana Rosa Costa
CVCrisnicaw Veríssimo
Crisnicaw Veríssimo
RDRenata Webster Duarte
Renata Webster Duarte
SFSaturnino Calabrez Filho
Saturnino Calabrez Filho
LCLourenço Correr-Sobrinho
Lourenço Correr-Sobrinho
The aim was to evaluate the microtensile bond strength (mTBS) to dentin and interfacial stress in a class II cavity restored with bulk-fill or conventional composite resins and the margin interfaces. Vertical slot class II cavities in the mesial face, with the gingival end in dentin, were prepared in 72 third molars, being divided into groups (n=24): G1-Tetric N-Ceram; G2-Tetric N-Ceram Bulk-Fill; G3-SonicFill. Clearfil SE Bond adhesive system was used in all groups. Half of the teeth in each group (n=12) were submitted to thermo-mechanical cycling (TMC). Restored teeth (n=9) were cut perpendicular to obtain beams, which were submitted to a mTBS test in an EMIC machine. The cervical margins in dentin of the restored teeth (n=3) were assessed using SEM through epoxy resin replicas as well as the section of the restoration. Interfacial stresses after load application were calculated by 2D finite element analysis. The mTBS means-MPa followed by different letters represent statistical difference by ANOVA and Games-Howell’s test (p<0.05): Without TMC: G1-15.68±6.10a; G2-10.08±5.21ab; G3-7.98±3.76b. With TMC: G1-9.70±5.52a; G2-5.79±1.42a; G3-4.37±1.87a. Interfacial stress (MPa) was 4.4 for SonicFill, 3.9 for Tetric N-Ceram, and 3.5 for Tetric N-Ceram Bulk-Fill. SEM images showed continuous margins for all composite resin restorations. It was possible to conclude that SonicFill obtained a slightly higher interfacial stress and lower bond strength to dentin in comparison with Tetric N-Ceram and Tetric N-Ceram Bulk-Fill. Continuous margin interfaces were obtained for Tetric N-Ceram, Tetric N-Ceram Bulk-Fill, and SonicFill. However, voids were observed in the SonicFill restorations.

21 February 2013 in Laser Physics
Verified
Journal Article
Open access
MGM R Galvão
M R Galvão
SCS G F R Caldas
S G F R Caldas
SCS Calabrez-Filho
S Calabrez-Filho
ECE A Campos
E A Campos
VBVanderlei Salvador Bagnato
Vanderlei Salvador Bagnato
MAM F Andrade
M F Andrade

1 May 2018 in Brazilian Dental Journal
Verified
Journal Article
Open access
PDF file
LCLara Almeida Cyrillo Cerqueira
Lara Almeida Cyrillo Cerqueira
ACAna Rosa Costa
Ana Rosa Costa
ASAna Maria Spohr
Ana Maria Spohr
EMEduardo Miyashita
Eduardo Miyashita
BMBenito André Silveira Miranzi
Benito André Silveira Miranzi
GBGilberto Antonio Borges
Gilberto Antonio Borges
The aim was to evaluate the influence of different dentin preparation mode in the smear layer characteristics (SL), hybrid layer (HL), and microtensile bond strength (µTBS) to dentin with two resin cements. The occlusal dentin of 120 third molars was exposed. The teeth were divided into 4 groups (n=30) according to the dentin preparation mode: 1- fine grain diamond bur; 2- coarse grain diamond bur; 3- multi laminate carbide steel bur; and, 4- ultrasonic CV Dentus diamond bur. Each treated dentin group was divided into 2 sub-groups (n=15) according to the resin cement: (1) RelyX U200 and (2) RelyX ARC. Resin composite blocks were cemented on dentin. After storage at 37o C for 24 h, beams with a cross section area of 1.0 mm2 were obtained, and tested in a universal testing machine at a crosshead speed of 0.5 mm/min. Two additional teeth for each sub-group were prepared to analyze the SL and HL on a scanning electron microscopy. According to Kruskal-Wallis test and Dunn tests, there was no significant difference in µTBS among the rotary instruments within each resin cement group. RelyX ARC obtained higher µTBS values compared to RelyX U200 (p<0.05). RelyX ARC formed evident HL, which was not observed for RelyX U200. The dentin mode preparation did not influence the µTBS of the resin cements. The SL was different for all instruments. The cementing agent is more determinant in the hybrid layer formation and bond strength to dentin than the instruments applied on dentin.

1 May 2009 in Operative Dentistry
Verified
Journal Article
Closed access
SCS. Calabrez-Filho
S. Calabrez-Filho
VCV. C. N. Calabrez
V. C. N. Calabrez
ERE. G. Reston
E. G. Reston
MAM. F. Andrade
M. F. Andrade
LBL. H. Borges
L. H. Borges
Clinical Relevance: An efficient polymerization of resin composite inlays associated with treatment of the surface and luting with dual resinous cement and flowable resin composites presents better longevity of restorations.

3 May 2011 in Laser Physics
Verified
Journal Article
Closed access
PDF file
TVT. A. Valentino
T. A. Valentino
SCS. Calabrez-Filho
S. Calabrez-Filho
FMF. C. H. Menezes
F. C. H. Menezes
LCL. M. A. Cavalcante
L. M. A. Cavalcante
LPL. A. F. Pimenta
L. A. F. Pimenta
ARAlessandra Nara Souza Rastelli
Alessandra Nara Souza Rastelli
This study evaluated the influence of light-curing units (LCUs) on Knoop microhardness (KHN) of different composite resins formulations. Four LCUs, one Quartz-Tungsten-Halogen (QTH) for 20 s, one Argon-Ion-Laser (AL) for 10 s, one Plasma-Arc-Curing (PAC) for 9 s, and one Light-Emitting-Diode (LED) for 20 s, and three composite resins, nanofill and easy cure (Filtek™ Supreme), microhybrid and medium cure (Herculite XRV), and microfill and difficult cure (Heliomolar) were used. Discs (4 × 2 mm2) of each composite resin were divided in 12 Groups and KHN was measured at the top (T) and bottom (B) surfaces. Data were analyzed using two-way ANOVA and Tukey’s test (p < 0.05). Top presented significantly higher KHN than bottom surface for all composite resins and LCUs tested. Statistical significant differences were observed among the LCUs. At the bottom surface QTH and LED presented higher KHN than PAC and LA. However, at the top surface PAC and LA presented similar results than QTH for nanofill and microhybrid composite resins. Different LCUs play an important effect on Knoop microhardness and the composite resin formulations were significant factor on the photosensitivity.