The aim of this study was to evaluate the μTBS in different dentin substrates and water-storage periods. Twenty-four dentin blocks obtained from sound third molars were randomly divided into 3 groups: Sound dentin (Sd), Caries-affected dentin (Ca) and Caries-infected dentin (Ci). Dentin blocks from Ca and Ci groups were subjected to artificial caries development (S. mutans biofilm). The softest carious tissue was removed using spherical drills under visual inspection with Caries Detector solution (Ca group). It was considered as Ci (softer and deeply red stained dentin) and Ca (harder and slightly red stained dentin). The Adper Single Bond 2 adhesive system was applied and Z350 composite blocks were built in all groups. Teeth were stored in deionized water for 24 h at 37 ºC and sectioned into beams (1.0 mm2 section area). The beams from each tooth were randomly divided into three storages periods: 24 h, 6 months or 1 year. Specimens were submitted to µTBS using EZ test machine at a crosshead speed of 1.0 mm/min. Failure mode was examined by SEM. Data from µTBS were submitted to split plot two-way ANOVA and Tukey’s HSD tests (a=0.05). The µTBS (MPa) of Sd (41.2) was significantly higher than Ca (32.4) and Ci (27.2), regardless of storage. Ca and Ci after 6 months and 1 year, presented similar µTBS. Mixed and adhesive failures predominated in all groups. The highest µTBS values (48.1±9.1) were found for Sd at 24 h storage. Storage of specimens decreased the µTBS values for all conditions.
The aim was to evaluate the microtensile bond strength (mTBS) to dentin and interfacial stress in a class II cavity restored with bulk-fill or conventional composite resins and the margin interfaces. Vertical slot class II cavities in the mesial face, with the gingival end in dentin, were prepared in 72 third molars, being divided into groups (n=24): G1-Tetric N-Ceram; G2-Tetric N-Ceram Bulk-Fill; G3-SonicFill. Clearfil SE Bond adhesive system was used in all groups. Half of the teeth in each group (n=12) were submitted to thermo-mechanical cycling (TMC). Restored teeth (n=9) were cut perpendicular to obtain beams, which were submitted to a mTBS test in an EMIC machine. The cervical margins in dentin of the restored teeth (n=3) were assessed using SEM through epoxy resin replicas as well as the section of the restoration. Interfacial stresses after load application were calculated by 2D finite element analysis. The mTBS means-MPa followed by different letters represent statistical difference by ANOVA and Games-Howell’s test (p<0.05): Without TMC: G1-15.68±6.10a; G2-10.08±5.21ab; G3-7.98±3.76b. With TMC: G1-9.70±5.52a; G2-5.79±1.42a; G3-4.37±1.87a. Interfacial stress (MPa) was 4.4 for SonicFill, 3.9 for Tetric N-Ceram, and 3.5 for Tetric N-Ceram Bulk-Fill. SEM images showed continuous margins for all composite resin restorations. It was possible to conclude that SonicFill obtained a slightly higher interfacial stress and lower bond strength to dentin in comparison with Tetric N-Ceram and Tetric N-Ceram Bulk-Fill. Continuous margin interfaces were obtained for Tetric N-Ceram, Tetric N-Ceram Bulk-Fill, and SonicFill. However, voids were observed in the SonicFill restorations.
31 July 2021 in Journal of Materials Science: Materials in Medicine
This in vitro study evaluates the influence of pressed lithium disilicate thickness, shade and translucency on the transmitted irradiance and the Knoop microhardness (KHN) of a light-cured resin cement at two depths. One hundred and thirty-five ceramic discs of IPS e.max Press (Ivoclar Vivadent) were fabricated and divided into twenty-seven groups (n = 5) according to the association between translucency: HT (hight translucency), LT (low translucency), and MO (medium opacity); shade: BL2, A1 and A3.5; and thickness: 0.5 mm, 1.5 mm, and 2.0 mm. One side of each ceramic disc was finished, polished and glazed. The irradiance (mW/cm²) of a multiwave LED light curing unit (Valo, Ultradent) was evaluated with a potentiometer (Ophir 10ª-V2-SH, Ophir Optronics) without (control group) or with interposition of ceramic samples. The microhardness of Variolink Esthetic LC resin cement (Ivoclar Vivadent) was evaluated after 24 h at two depths (100 μm and 700 μm). Data were submitted to ANOVA followed by Tukey’s test (α = 0.05). Irradiance and KHN were significantly influenced by ceramic thickness (p < 0.0001), shade (p < 0.001), translucency (p < 0.0001) and depth (p < 0.0001). Conclusions: the interposition of increasing ceramic thicknesses significantly reduced the irradiance and microhardness of resin cement. Increased depth in the resin cement showed significantly reduced microhardness for all studied groups. Increased ceramic opacity reduced the KHN of the resin cement at both depths for all ceramic thicknesses and shades.
The aim of this study was to evaluate the effect of 2% chlorhexidine digluconate (CHX) on microtensile bond strength (µTBS) between an adhesive system and under 3 dentin conditions. For that, this study evaluated the adhesive interface at initial, after 6 months and 1 year of storage. Forty-eight human third molars were prepared and randomly divided into 3 groups, according to dentin substrates: sound dentin (Sd), caries-infected dentin (Ci) and caries-affected dentin (Ca). The groups were subdivided into two according to the dentin pre-treatment: application of 2% CHX or without pre-treatment (control). The dentin surfaces were etched with 35% phosphoric acid gel and bonded with Adper Single Bond 2 (3M ESPE) adhesive system according to manufacturer’s instructions. Subsequently, the specimens were stored in deionized water at 37°C for 24h, 6 months and 1 year. Two additional teeth were used to analyze the bonding interfaces by SEM. Data was submitted to three-way ANOVA in a split plot design and Tukey’s test (α = 0.05). The results showed that Ci decreased µTBS values when compared to Ca and Sd, regardless storages time or treatment. Stored samples for 6 months and 1 year decreased the µTBS for the control group, but no difference was found between storages time for the CHX group. As a conclusion, the 2% CHX application after etching showed improved dentin bond strength in the storage time, regardless of the substrates evaluated.
Introduction In recent years, there has been an increasing demand for esthetic treatments, especially among orthodontic patients. Objective This study determined the fracture strength of monocrystalline and polycrystalline ceramic brackets of different manufacturers during archwire torque. Material and method Sixty ceramic brackets (Roth, right upper central incisors, 0.022 x 0.028-inch slot) were allocated into two groups (30 specimens per group) according to the type of ceramics: monocrystalline and polycrystalline. Subsequently, the groups were divided into three subgroups (n = 10) according to the manufacturer: Orthometric, Eurodonto and Ortho Technology. Sixty PVC cylinders were filled with chemically activated acrylic resin (CAAR), the brackets were fixed with CAAR onto the cylinder surface and the excess material was used to partially cover the base of the bracket. After 24h, the U-shaped wire base (0.019 x 0.025 inches; 6 mm height and width) was inserted into the bracket slot and fixed thereon with a stainless-steel wire. Vertical folds were made at the ends of the “U” to support the universal test machine chisel. The fracture strength test was performed at a speed of 1.0 mm/min until fracture into a universal test machine (Instron). The data were recorded, transformed into g.mm and submitted to two-way ANOVA followed by Tukey’s post-hoc test (SAS Institute Inc., Cary, NC, USA, version 9.3) (α=5%). Result Monocrystalline brackets showed a higher fracture strength than polycrystalline brackets, regardless of the manufacturer (p0.05). Conclusion Monocrystalline ceramic brackets have a higher fracture strength than polycrystalline brackets, with significant manufacturer-dependent differences.