11 August 2021 in IEEE Transactions on Electron Devices
Novel normally-OFF AlGaN/GaN MIS-high electron mobility transistors (HEMTs) with a ZrO x charge trapping layer are proposed. The deposition of the ZrO x charge trapping layer on the partially recessed AlGaN in conjunction with the Al 2 O 3 gate dielectric has been accomplished. The developed MIS-HEMTs exhibit a threshold voltage of 1.55 ± 0.4 V and a maximum drain current of 730 ± 6 mA/mm, while associated low ON-resistance of 7.1 ± 0.2 Ω·mm, for a gate to drain separation of 3 μm. The TCAD simulation results are presented to explore the charge trapping and de-trapping behaviors. Moreover, the devices exhibit a high breakdown voltage. The results indicate the merits of employing ZrO x charge trapping layer to realize the normally-OFF GaN devices with low ON-state resistance.
21 May 2020 in IEEE Access
In this paper, the GaN-based MIS-HEMTs with Si 3 N 4 single-layer passivation, Al 2 O 3 /SiN x bilayer passivation, and ZrO 2 /SiN x bilayer passivation are demonstrated. High-k dielectrics are adopted as the passivation layer on MIS-HEMTs to suppress the shallow traps on the GaN surface. Besides, high permittivity dielectrics passivated MIS-HEMTs also show an improved breakdown voltage characteristic, and that is explained by 2-D simulation analysis. The fabricated devices with high-k dielectrics/SiN x bilayer passivation exhibit higher power properties than the devices with plasma enhanced chemical vapor deposition-SiNx single layer passivation, including smaller current collapse and higher breakdown voltage. The Al 2 O 3 /SiN x passivated MIS-HEMTs exhibit a breakdown voltage of 1092 V, and the dynamic R on is only 1.14 times the static R on after off-state VDS stress of 150 V. On the other hand, the ZrO 2 /SiN x passivated MIS-HEMTs exhibit a higher breakdown voltage of 1207 V, and the dynamic Ron is 1.25 times the static R on after off-state VDS stress of 150 V.
12 March 2020 in Japanese Journal of Applied Physics
This research proposes an economical and effective method of 1-octadecanethiol (ODT) treatment on GaN surfaces prior to Al 2 O 3 gate dielectric deposition. GaN-based metal–insulator–semiconductor (MIS) devices treated by HCl, O 2 plasma and ODT are demonstrated. ODT treatment was found to be capable of suppressing native oxide and also of passivating the GaN surface effectively; hence the interface quality of the device considerably improved. The interface trap density of Al 2 O 3 /GaN was calculated to be around 3.0 × 10 12 cm −2 eV −1 for devices with ODT treatment, which is a relatively low value for GaN-based MIS devices with Al 2 O 3 as the gate dielectric. Moreover, there was an improvement in the gate control characteristics of MIS-HEMTs fabricated with ODT treatment.