The influence of electron-beam facing modes on the structure of Ti-Ta layers formed on the surface of commercially pure titanium VT1-0 has been studied in the paper. The mode of the electron-beam treatment of alloying powder mixture, by which there were no defects in the pad, has been identified. The methods of optical microscopy and scanning electron microscopy have shown that in pads there is dendritic segregation typical for the process of initial crystallisation. At greater magnifications it is possible to observe a structure of the laminar type. The X-ray phase analysis of titanium-tantalum layers justifies the presence of two phases: a hexagonal α'-phase and a cubic (β-phase of titanium.
Cast iron with 3 wt. % Cu was prepared by induction melting and casting in sand molds. The structure of the samples was studied using light microscopy (LM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The addition of Cu promoted formation of pearlite and slightly decreased the volume fraction of graphite. No Cu inclusions were found by LM and SEM. The nanoprecipitations of ε-Cu in lamellar pearlite were observed by TEM. The properties of the Cu-alloyed cast iron were compared with the properties of cast iron not alloyed with Cu. The hardness of cast iron after alloying with Cu increased and the friction coefficient decreased in comparison with the reference sample.
The cladding of titanium and graphite powders on the cp-titanium workpieces using the electron beam injected to the atmosphere provided the formation of the surface layers with a high content of high-strength carbide particles. The main structural components in cladded layers are α-Ti (αʹ-Ti), titanium carbide and graphite. Electron beam current is the main technological parameter defining a thickness of the hardened layer. An increasing beam current ranged from 20 to 23 mA leads to the cladded layer growth up to 2.9 mm. However, in this case a significant decrease of the microhardness level and the wear resistance level of the cladded layer is not observed. An average microhardess value of the hardened layer is of 430 HV. Under the conditions of friction against fixed abrasive particles, a wear resistance level of the cladded layers is by 32-45 % larger than that of cp-titanium.