The growing interest in the development of next-generation net zero energy systems has led to the expansion of molybdenum disulfide (MoS2) research in this area. This activity has resulted in a wide range of manufacturing/synthesis methods, controllable morphologies, diverse carbonaceous composite structures, a multitude of applicable characterization techniques, and multiple energy applications for MoS2. To assess the literature trends, 37,347 MoS2 research articles from Web of Science were text scanned to classify articles according to energy application research and characterization techniques employed. Within the review, characterization techniques are grouped under the following categories: morphology, crystal structure, composition, and chemistry. The most common characterization techniques identified through text scanning are recommended as the base fingerprint for MoS2 samples. These include: scanning electron microscopy (SEM), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), and Raman spectroscopy. Similarly, XPS and Raman spectroscopy are suggested for 2H or 1T MoS2 phase confirmation. We provide guidance on the collection and presentation of MoS2 characterization data. This includes how to effectively combine multiple characterization techniques, considering the sample area probed by each technique and their statistical significance, and the benefit of using reference samples. For ease of access for future experimental comparison, key numeric MoS2 characterization values are tabulated and major literature discrepancies or currently debated characterization disputes are highlighted.
The two common characterization techniques that can distinguish between the metastable 1T and stable 2H phase of molybdenum disulfide (MoS2) are Raman spectroscopy and X-ray photoelectron spectroscopy (XPS). Argon ion etching within XPS offers the possibility to explore sample composition as a function of depth. However, for 2H MoS2 samples this results in sample alteration via the creation of sulfur vacancies and leads to local areas of MoS2‑x and 1T/2H MoS2. XPS MoS2‑x generation (228.1 eV) and laboratory nanoscale 1T MoS2 synthesis (228.4 eV) are easily mistaken in XPS, as both signals exhibit downshifted Mo 3d binding energies relative to 2H MoS2 (229.3 eV). Thus, we applied a four split orbit peak XPS model that enables distinction between MoS2‑x alteration and successful 1T phase synthesis. In argon etching induced MoS2‑x the pristine S 2p peaks remain dominant (162.0 eV) and the S/Mo atomic ratio decreases from 2.5 to 1.1 after electrode ion bombardment. When nanoscale 1T MoS2 forms during lithiation in a lithium-ion battery, the dominant S 2p peaks are found at lower binding energies (161.5 eV) and the S/Mo atomic ratio is elevated (>2.0). Depth profiling of ex situ 1T/2H MoS2 electrodes showcases lithiation beyond the electrode surface, clearly distinguished from solely MoS2‑x alteration through the S 2p component percentage, which exceeds the 1T MoS2 limiting threshold (1T > 13% of S 2p) for ion bombarding of as-cast electrodes.
Lithiation of MoS2 electrodes in coin cells (100–200 mA g−1) results in incomplete lithiation and MoS2 phase inhomogeneities. Upon deep discharge (0.01 V) the outer ring has better contact with the counter electrode and forms a gel-like layer.
27 October 2026 in Journal of Materials Chemistry A