1 July 2010 in Welding in the World
1 May 2020 in Marine Structures
1 August 2020 in Engineering Fracture Mechanics
19 November 2019 in Journal of Marine Science and Technology
12 August 2020 in Materials Performance and Characterization
The crack tip opening displacement (CTOD) concept describing cleavage embrittlement failure proposed by Wells is an important technology supporting the reliability of steel structures around the world. In 2002, ASTM E1290, Standard Test Method for Crack-Tip Opening Displacement (CTOD) Fracture Toughness Measurement, proposed a CTOD calculation formula based on a J-integral different from the previous integral that reflected the work-hardening characteristics and was triggered by the appearance of a case where evaluation values significantly different from the conventional British Standard (BS) formula are given. The authors attempted to construct an accurate CTOD calculation formula by performing actual measurements in CTOD experiments and systematic numerical analyses. Detailed observation of the plastic deformation mode in the ligament demonstrates the validity of the plastic hinge model that BS has adopted to date. In 2016, it was possible to propose a highly accurate formula that considers the work-hardening characteristics for edge-cracked bending test piece specimens and is adopted into the Japanese and ISO standard. Here, the outline of the CTOD calculation formula for the compact specimen (denoted as C(T)) constructed in the same manner will be described. The authors also suggested that the CTOD and J-integral conversion factor can be expressed in a simpler form than the form indicated by ASTM E1820, Test Method for Measurement of Fracture Toughness. In this study, we discovered that the same conversion factor can be applied to a compact specimen, which is quite reasonable considering the energy release rate of the J value.
2 August 2018 in Journal of Pressure Vessel Technology
The drop weight tear test (DWTT) has been widely used to evaluate the resistance of linepipe steels against brittle fracture propagation. Although there is an ambiguity in the evaluation of DWTT results if inverse fracture appears on the fracture surfaces, the cause of inverse fracture is not yet fully understood. In the present work, DWTTs were performed with X65, X70, and X80 steel linepipes. In addition to the conventional DWTT specimen with a pressed notch (PN), PN specimens with a back slot (BS) and specimens with a chevron notch (CN) or static precrack (SPC) were also examined, and the fracture appearances in different strengths and different initial notch types were compared. Although the frequency of inverse fracture in these DWTTs was different with each material and each specimen type, there was no material or specimen type that was entirely free from inverse fracture. The purpose of the DWTT is to evaluate the brittle crack arrestability of the material in a pressurized linepipe. Therefore, the DWTT results should be examined with a running brittle crack arrest (BCA) test. A large-scale BCA test with temperature gradient was also performed with the X65 mother plate, and the shear area fraction measured in the DWTT fracture surface was compared with the local shear lip thickness fraction in the BCA test. Based on the results, the count of inverse fracture in the DWTT was discussed in comparison with the long BCA behavior in the BCA test.