24 June 2021 in Non-ferrous Metals
For the manufacture of thin-walled precision structures with complex geometry, the method of brazing is used. It allows to obtain joints with a given structural-phase state, high mechanical characteristics and resistance to corrosion. This overview examines alloys based on copper, precious metals, nickel and iron, which are actively used for joining steels. The data on the operational characteristics of the joints obtained by brazing using nickel-based filler metals are presented and structured. Special attention is paid to nickel braze alloys based on Ni – B, Ni – Si – B, Ni – Cr – B, Ni – Cr – Si, Ni – Cr – Si – B, Ni – Mn, Ni – Cr – P, Ni – Si – Be systems. Such alloys are the most widespread and applicable throughout the world. The overview describes the main phases that are formed in the seams and the heat-affected zones of joints. The dependences of the technological parameters of the process, such as the temperature-time mode of brazing and the size of the gap on the microstructure of the joints and their mechanical characteristics, are shown. The corrosion resistance of steel joints brazed by various nickel-based filler metals is considered. The overview is based on the extensive experience of MEPhI in the production and development of rapidly solidified amorphous-crystalline foils based on nickel. In addition to the world experience, the overview considers works of the research team of the MEPhI laboratory, which has been working on this topic since 1995. This overview will help technologists and designers of energy-intensive equipment to determine the trajectory for the selection of the filler metal composition to obtain the optimal technological parameters, mechanical characteristics and corrosion resistance of the joints applicable to a specific design problem. The reported study was funded by RFBR, project number 20-12-50106.
28 December 2018 in Non-ferrous Metals
Manufacturers of nozzles for liquid rocket engines from heat-resistant austenitic and austenitic-ferritic steels faced the problem of brittle boron nitride formation in the joints. Joints are obtained using hightemperature diffusion brazing in vacuum by filler metal based on Ni – Cr – Fe – Si – B system. This technology is based on the isothermal solidification of the filler metal melt, occurring due to the diffusion of boron into the base material. The developed boron-free nanocrystalline thin film filler metal Ni – 8Si – 5Nb wt.% was proposed to solve the brittle boron nitride problem. The melting interval 1103–1120 oC of the filler metal is determined by the method of differential thermal analysis. It’s structural and phase state was revealed by X-ray methods. Technological modes of high-temperature diffusion brazing of austenitic and austenitic-ferritic steels have been developed in the temperature range of 1150–1200 oС. The metallographic studies of the brazed joint were carried out. To determine the joint strength characteristics, the microhardness was investigated in the brazed zone and mechanical uniaxial tension tests were carried out according to GOST (Russian State Standard) 28830–90. The best result on the tensile strength 450±30 MPa was achieved on samples obtained at an isothermal holding temperature of 1150 oC for 30 min. As a result of this work, the possibility of using boron-free nanocrystalline thin film filler metal for brazing heat-resistant nitrogen-containing steels has been demonstrated. High-strength joints were obtained. This work was supported by the MEPhI Academic Excellence Project.
1 May 2014 in Inorganic Materials: Applied Research
The changes in the structure, phase composition, and topology of the surface of rapidly solidified metallic glasses Ni71.5Cr6.8Fe2.7B11.9Si7.1 and Ni63.4Cr7.4Fe4.3Mn0.8B15.6Si8.5 are investigated after three stages of crystallization. The surface topology changes are found to be correlated with the processes occurring at different stages of crystallization. The character of the redistribution of chemical elements in the crystallized alloys is ascertained.
29 December 2020 in Non-ferrous Metals
Two titanium alloys, OT4 and VT6-c, with a pseudo-α and α + β structure, respectively, were brazed using transient liquid phase (TLP) bonding. To obtain high strength joints an amorphous foil (Ti – 12Zr – 22Cu – 12Ni – 1.5 Be – 0.8V wt.%) was used. Based on microstructural studies and analysis of two- and three-component phase diagrams, the mechanism of the microstructural evolution of the brazed seams of titanium alloys OT4 and VT6-c is described. Brazing at 800 °C with exposure for 0.5 h leads to the formation of a heterogeneous structure consisting of Widmanstätten, eutectoid, and eutectic. Brazed OT4 and VT6-c joints with the presence of a eutectic layer in the centre show low mechanical properties; their ultimate strength lies in a range from 200 to 550 MPa. Increasing the brazing temperature to 840 °C and the exposure time to 2 h, leads to the disappearance of the brittle eutectic component from the seam. This structure typically consists of Widmanstätten with a small number of eutectoid fractions. Joints with the absence of a eutectic layer in the brazed seam demonstrate a strength equal to the base titanium alloys. In this case, failure occurs in the base metal. For brazed samples from the OT4 alloy, the tensile strength value is σb = 750 ± 3 MPa, and for samples from VT6-c, σb = 905 ± 3 MPa. This work was supported by Competitiveness Growth Programme of the Federal Autonomous Educational Institution of Higher Education National Research Nuclear University MEPhI (Moscow Engineering Physics Institute).