This investigation was attempted to introduce carbon nanotubes (CNTs) onto surface of copper powders in order to improve heat transfer performance of copper matrix for engineering application of electrical packaging materials. The Ni/MgO catalyst was formed on the copper powders surface by means of codeposition method. CVD technique was executed to fabricate uniform CNTs on copper powders and effect of reaction temperature on the morphology of CNTs was surveyed. The results showed that CNTs products on the copper powder surface were distributed uniformly even if reaction temperature was different. The diameter dimension of CNTs was within the scope of 30~60 nm. Growth behaviors of CNTs by CVD method were considered to be “tip-growth” mechanism. Raman spectra of CNTs proved that intensity ratio of D-band to G-band () increased as deposition reaction temperature increased, which implied that order degree of graphitic structure in synthesized CNTs improved.
25 February 2021 in International Journal of Photoenergy
In view of the surface engineering application of electrical contact materials, SiC ceramic particles were introduced into copper matrix composites by the hot-press sintering method for the sake of enhancing the service life of copper matrix electrical contact materials. Magnetron sputtering technology was exploited to form the continuous copper film on the β-SiC powders in order to improve interface wettability between SiC powder and copper matrix. The SiC@Cu powders were treated by magnetron sputtering technology. Then, dynamic deposit behavior was described according to SEM results. The phase constitution, fracture morphology, relative density, porosity, Vickers hardness, and coefficient of thermal expansion of SiC@Cu/Cu composites with different SiC@Cu addition were analyzed in detail. The results showed that SiC@Cu powders with higher fraction in the SiC@Cu/Cu composites would decrease relative density and increase porosity, so it resulted in improvement of Vickers hardness. The addition of SiC@Cu decreased CTE values of the SiC@Cu/Cu composite, especially at high-level fraction SiC@Cu powder.