29 July 2025 in Scientific Reports
The decomposition of an anhydride-cured epoxy resin by subcritical hydrolysis is studied under variation of reaction temperature, decomposition duration and water volume using a batch reactor. Within the framework of a design of experiment, the process is evaluated by the gravimetric decomposition of the epoxy resin clearly showing that temperature is the most important factor. Duration and water volume have only smaller positive effects. The mass loss mechanism of the cube-shaped specimens corresponds to a heterogeneous surface degradation where material is only lost from the outer areas. The determination of glass transition temperatures after the experiments demonstrates that the water hardly affects the center of the epoxy cubes. Therefore, a core-shrinking model is successfully applied for analysis of the decomposition kinetics. The product distribution in the aqueous phase reveals a large number of organic compounds. Higher temperatures, longer durations and lower water volumes lead to an increase in decomposition product complexity and concentrations, but the degradation pathways are apparently not affected.
30 April 2026 in Journal of Polymer Research
Amine-cured epoxy resins (EP) are highly hydrophilic, particularly due to alcohol groups in the polymer network. The water absorption in humid environments leads to a reduction in the glass transition temperature (T g ) and to a deterioration in the mechanical properties. These effects have been extensively studied in the past by exposure experiments carried out at temperatures of no more than 100 °C, usually below the T g of the polymer. In this work, however, an amine-cured EP is subjected to water at 100, 150, 200 and 250 °C, all above the polymer’s T g . Thus, it is possible to achieve water absorptions of more than 10% in less than three hours. This is due to the reduced density and viscosity of the liquid phase at these temperatures, and the rubbery state of the EP. Test times can therefore be minimized compared to conventional exposure experiments in this regard. The results of dynamic mechanical analyses and tensile tests confirm the expected depression in T g (up to nearly 50 %) and decrease in tensile strength and modulus with increasing aging temperature and water absorption, respectively. This change in properties is accompanied by a light to strong yellowing of the polymer. The formation of carbonyl groups responsible for this discoloration is confirmed by infrared spectroscopy. For further application of this accelerated hydrothermal aging, however, these findings still need to be validated by comparison with conventional exposure experiments.
3 June 2025 in Materials Testing
When testing double cantilever beam (DCB) specimens, the distance between the load line and the crack tip corresponds to the lever arm, thereby affecting the load necessary to propagate the crack. While ASTM D5528 defines an initial delamination length (IDL) from this load line to the end of the inserted release film, there is no such specification in DIN EN 6033. The question, therefore, arises as to whether the IDL affects the interlaminar fracture toughness energy – Mode I – GIC determined from DCB specimens. This is especially important to know for the positioning and application of the hinges. In the present work, the influence of two different IDL (5 and 20 mm) on the GIC of vacuum-infused quasi-unidirectional glass fiber reinforced plastic is studied according to DIN EN 6033. It is shown that there are significant differences in the load–displacement curves. After evaluation, however, the results of the two series are quite comparable because the differences even out in the course of the tests.
11 May 2024 in Journal of the Mechanical Behavior of Biomedical Materials
Although total hip replacements (THR) can be considered one of the most successful implantable medical devices in history, wear remains the ultimate challenge in order to further increase clinical success. Wear assessment on retrieved implants is the most reliable way to perform research into failure mechanisms. Therefor the bearing surface of the explant is measured geometrically by coordinate measuring machine (CMM). Wear determination in geometrical data is carried out in 3 steps: (1) identifying the worn area, (2) reconstructing the pre-wear geometry and (3) quantify wear as the difference between worn area and pre-wear geometry. In previous studies, assumptions to pre-wear geometry had been made for wear determination (step 2) and the worn area was identified by deviations between measured data and assumed form. Thus, the original form of the retrieved endoprostheses, including form deviations due to the manufacturing process and implantation, was not considered which leads to uncertainties in the wear computed. This work introduces a method which allows to identify the wear area without making assumptions to the original form. Instead, the curvature of the bearing surface obtained by simple computations on the measurement data is analysed and the edge of the wear region is recognized by its deviation in curvature. The method is applied to a retrieved Metal-on-Metal prosthetic head and the results are compared to those of the well-known method introduced by Jaeger et al., in 2013. With the new approach the wear region is identified more accurately.