27 March 2024 in IEEE Electron Device Letters
In this work, we demonstrate the enlargement of the memory window of Si channel FeFET with ferroelectric Hf 0.5 Zr 0.5 O 2 by gate-side dielectric interlayer engineering. By inserting a 3 nm Al 2 O 3 dielectric interlayer between TiN gate metal and ferroelectric Hf 0.5 Zr 0.5 O 2 , we achieve a memory window of 4.1 V with endurance of ~10 4 cycles and retention over 10 years. The physical origin of memory window enlargement is clarified to be charge trapping at the Al 2 O 3 /Hf 0.5 Zr 0.5 O 2 interface, which has an opposite charge polarity to the trapped charges at the Hf 0.5 Zr 0.5 O 2 /SiO x interface.
25 September 2024 in IEEE Transactions on Electron Devices
We study the impact of top SiO2 interlayer thickness on the memory window (MW) of Si channel ferroelectric field-effect transistor (FeFET) with TiN/SiO2/ Hf0.5Zr0.5O2/SiOx/Si (MIFIS) gate structure. We find that the MW increases with the increasing thickness of the top SiO2 interlayer, and such an increase exhibits a two-stage linear dependence. The physical origin is the presence of the different interfacial charges trapped at the top SiO2/Hf0.5Zr0.5O2 interface. Moreover, we investigate the dependence of endurance characteristics on initial MW. We find that the endurance characteristic degrades with increasing the initial MW. Meanwhile, we study the impact of the top SiO2 interlayer thickness on the retention characteristics of the MIFIS structure. The results of retention characteristics show that the MIFIS structure with thicker top SiO2 has poorer retention characteristics. This is attributed to the de-trapping of interfacial charges trapped at the top SiO2/Hf0.5Zr0.5O2 interface and the depolarization field of the ferroelectric. By inserting a 3.4 nm SiO2 dielectric interlayer between the gate metal TiN and the ferroelectric Hf0.5Zr0.5O2, we achieve a MW of 6.3 V and retention over 10 years. Our work is helpful in the device design of FeFET.
15 November 2024 in IEEE Transactions on Electron Devices
In this work, we propose a gate structure to enhance the memory window (MW) of Si-channel Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ FeFETs. We achieve an MW of 10.04 V by inserting an Al $_{\text{2}}$ O $_{\text{3}}$ /HfO $_{\text{2}}$ /Al $_{\text{2}}$ O $_{\text{3}}$ (AHA) top dielectric interlayer between the ferroelectric Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ layer and the metal gate, where the gate-stack thickness is 14.8 nm. The physical origin is that the Al $_{\text{2}}$ O $_{\text{3}}$ /HfO $_{\text{2}}$ , HfO $_{\text{2}}$ /Al $_{\text{2}}$ O $_{\text{3}}$ , and Al $_{\text{2}}$ O $_{\text{3}}$ /Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ interfaces can trap charges from the metal gate, contributing to the MW enhancement. This AHA top dielectric multilayer effectively suppresses charge loss compared with a single Al $_{\text{2}}$ O $_{\text{3}}$ top dielectric interlayer. Moreover, the de-trapping of charges injected from the metal gate is the primary factor for the degradation of the MW in this structure. Our work provides a guide for improving the MW of FeFET.
1 July 2024 in IEEE Transactions on Electron Devices
This study demonstrates annealing-free TiN/Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ (HZO)/TiN (MFM) ferroelectric (FE) capacitors using a low thermal budget process (300 $^{\circ}$ C), without post deposition annealing (PDA) or post metal annealing (PMA). The remnant polarizations (2 $\textit{P}_{\text{r}}$ ) are 17.6 and 21.8 $\mu$ C/cm $^{\text{2}}$ at the atomic layer deposition (ALD) temperatures ( $\textit{T}_{\text{dep}})$ of 280 $^{\circ}$ C and 300 $^{\circ}$ C, respectively. The in-plane stress induced by the distorted TiN electrode could be the origin contributing to the emergence of low-thermal-budget ferroelectricity. In addition, as the $\textit{T}_{\text{dep}}$ decreases, there is a reduction in crystallinity, orthorhombic phase (o-phase) composition, $\textit{P}_{\text{r}}$ , dielectric permittivity ( $\kappa)$ , and leakage current (J), leading to an enhancement in reliability. The demonstration of annealing-free ferroelectricity at temperatures as low as 300 $^{\circ}$ C is helpful for the back-end-of-line (BEOL) process and the reliability of FE nonvolatile memory.
12 June 2024 in IEEE Transactions on Electron Devices
In this study, we investigate the impact of nitridation in Hf $_{\text{0}.\text{5}}$ Zr $_{\text{0}.\text{5}}$ O $_{\text{2}}$ -based ferroelectric field-effect transistors (FeFETs) with a SiON interfacial layer (IL). We fabricated the SiON IL using decoupled plasma nitridation. Compared with the SiO $_{\textit{x}}$ interlayer, the SiON interlayer can reduce interfacial state density (D $_{\text{\text{it}}}\text{)}$ at the interlayer/Si interface, suppress the degradation of I $_{\text{on}}$ and subthreshold swing (SS), and improve endurance under the same electric field across the IL. The physical origin is that the nitridation can reduce trap generation rates at both the Hf $_{\text{0}.\text{5}}$ Zr $_{\text{0}.\text{5}}$ O $_{\text{2}}$ /interlayer and interlayer/Si interfaces.
16 October 2024 in IEEE Transactions on Electron Devices
In this work, we investigate the effect of nitridation of the bottom interlayer in HfO $_{\text{2}}$ -based ferroelectric silicon channel field-effect transistors (HfO $_{\text{2}}$ Si-FeFETs) with the TiN/top interlayer/ferroelectric/bottom interlayer/Si substrate (MIFIS) structure. We find that the SiON bottom interlayer induces a smaller memory window (MW) compared with the case of SiO $_{\text{2}}$ as a bottom interlayer in the MIFIS structure. The origin is the reduced barrier height at the bottom interlayer induced by the positive charges in the SiON layer, which makes the charges injected from the metal gate cannot remain after erasing operation. However, the SiON bottom interface in the MIFIS structure shows higher endurance and stable retention than the SiO $_{\text{2}}$ bottom interface. Thus, for the ferroelectric field-effect transistor (FeFET) gate stacks with a top interlayer (MIFIS structure), the SiO $_{\text{2}}$ is more suitable than the SiON as a bottom interlayer to realize larger MW, while the SiON bottom interlayer can improve retention and endurance at the expense of MW.