We propose an in situ ${V}_{\text {th}}$ measurement method to investigate the endurance fatigue mechanism of Si ferroelectric field-effect transistor (FeFET) with HfZrO ferroelectric. The in situ ${V}_{\text {th}}$ measurement method means that a pulsed current-voltage measurement is embedded during the quasi-static capacitance-voltage (QSCV) measurement. Based on this method, the trapped charges can be extracted as a function of the gate voltage ( ${V}_{g}{)}$ . We find that: First, the trapped electrons and holes show asymmetric de-trapping dynamics. Excess electrons continuously de-trap within the ${V}_{g}$ ranging from the maximum positive value to ferroelectric reverse switching. However, the trapped holes do not de-trap when the ${V}_{g}$ changes from the minimum negative value to 0 V. Second, the increase of donor trap density is the key to endurance fatigue. During endurance fatigue, the total amounts of trapped electrons are unchanged near the maximum positive voltage, but the amounts of de-trapped electrons decrease when the ${V}_{g}$ returns to 0 V due to donor trap density increases. In addition, we apply our method in the scaled FeFET to overcome the measurement limitation of gate charges ( ${Q}_{m}{)}$ by the nowadays equipment.
25 September 2024 in IEEE Transactions on Electron Devices
We study the impact of top SiO2 interlayer thickness on the memory window (MW) of Si channel ferroelectric field-effect transistor (FeFET) with TiN/SiO2/ Hf0.5Zr0.5O2/SiOx/Si (MIFIS) gate structure. We find that the MW increases with the increasing thickness of the top SiO2 interlayer, and such an increase exhibits a two-stage linear dependence. The physical origin is the presence of the different interfacial charges trapped at the top SiO2/Hf0.5Zr0.5O2 interface. Moreover, we investigate the dependence of endurance characteristics on initial MW. We find that the endurance characteristic degrades with increasing the initial MW. Meanwhile, we study the impact of the top SiO2 interlayer thickness on the retention characteristics of the MIFIS structure. The results of retention characteristics show that the MIFIS structure with thicker top SiO2 has poorer retention characteristics. This is attributed to the de-trapping of interfacial charges trapped at the top SiO2/Hf0.5Zr0.5O2 interface and the depolarization field of the ferroelectric. By inserting a 3.4 nm SiO2 dielectric interlayer between the gate metal TiN and the ferroelectric Hf0.5Zr0.5O2, we achieve a MW of 6.3 V and retention over 10 years. Our work is helpful in the device design of FeFET.
19 January 2024 in IEEE Transactions on Electron Devices
We investigate charge trapping induced trap generation in Si ferroelectric field-effect transistor (FeFET) with ferroelectric Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ /SiO $_{\text{2}}$ gate stacks by split I – V measurement. We find that the recombination of electrons and holes within the gate stacks induces the generation of traps and consequently results in the degradation of the endurance characteristics of the FeFET. Therefore, by floating the body terminal, we suppress the hole injection into the gate stacks and the recombination and improve the endurance characteristics.
15 November 2024 in IEEE Transactions on Electron Devices
In this work, we propose a gate structure to enhance the memory window (MW) of Si-channel Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ FeFETs. We achieve an MW of 10.04 V by inserting an Al $_{\text{2}}$ O $_{\text{3}}$ /HfO $_{\text{2}}$ /Al $_{\text{2}}$ O $_{\text{3}}$ (AHA) top dielectric interlayer between the ferroelectric Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ layer and the metal gate, where the gate-stack thickness is 14.8 nm. The physical origin is that the Al $_{\text{2}}$ O $_{\text{3}}$ /HfO $_{\text{2}}$ , HfO $_{\text{2}}$ /Al $_{\text{2}}$ O $_{\text{3}}$ , and Al $_{\text{2}}$ O $_{\text{3}}$ /Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ interfaces can trap charges from the metal gate, contributing to the MW enhancement. This AHA top dielectric multilayer effectively suppresses charge loss compared with a single Al $_{\text{2}}$ O $_{\text{3}}$ top dielectric interlayer. Moreover, the de-trapping of charges injected from the metal gate is the primary factor for the degradation of the MW in this structure. Our work provides a guide for improving the MW of FeFET.
16 October 2024 in IEEE Transactions on Electron Devices
In this work, we investigate the effect of nitridation of the bottom interlayer in HfO $_{\text{2}}$ -based ferroelectric silicon channel field-effect transistors (HfO $_{\text{2}}$ Si-FeFETs) with the TiN/top interlayer/ferroelectric/bottom interlayer/Si substrate (MIFIS) structure. We find that the SiON bottom interlayer induces a smaller memory window (MW) compared with the case of SiO $_{\text{2}}$ as a bottom interlayer in the MIFIS structure. The origin is the reduced barrier height at the bottom interlayer induced by the positive charges in the SiON layer, which makes the charges injected from the metal gate cannot remain after erasing operation. However, the SiON bottom interface in the MIFIS structure shows higher endurance and stable retention than the SiO $_{\text{2}}$ bottom interface. Thus, for the ferroelectric field-effect transistor (FeFET) gate stacks with a top interlayer (MIFIS structure), the SiO $_{\text{2}}$ is more suitable than the SiON as a bottom interlayer to realize larger MW, while the SiON bottom interlayer can improve retention and endurance at the expense of MW.
3 May 2024 in IEEE Transactions on Electron Devices
In this work, the switching dynamics of HfO2–ZrO2 nanolaminate ferroelectric (FE) films with different laminate thicknesses are investigated. Metal/FE layer/metal capacitors with HfO2–ZrO2 alternate cycle ratios n ( ${n} =1$ , 8, 15, 25, and 37) are fabricated, and the hysteresis loop and switching dynamics of these devices are measured. All nanolaminate samples exhibit ferroelectricity and show reduced spontaneous polarization compared with the controlled Hf0.5Zr0.5O2 (HZO) sample. The differences in switching dynamics are analyzed by the inhomogeneous field mechanism (IFM). It is found that: 1) the switching becomes slower with laminate thickness increases. The HZO sample shows the fastest switching due to fewer pinned domains. 2) Decreasing the laminates within a certain range to form a laminate structure is beneficial for higher remanent polarization, better endurance, and fast switching speed. The improvement in the HfO2–ZrO2 alternate laminate device with 8 and 15 cycle ratios could be attributed to higher orthorhombic fraction, grain boundary interruption, and enhanced nucleation. This work provides guidelines for designing devices with HfO2–ZrO2 nanolaminate layers.