10 February 2020 in Journal of Applied Physics
Hydrogen (H) is thought to be strongly involved in the light and elevated temperature-induced degradation observed predominantly in p-type silicon wafers, but the nature of the defect or defects involved in this process is currently unknown. We have used infrared (IR) spectroscopy to detect the vibrational signatures due to the H–B, H–Ga, and H2*(C) defects in thin, hydrogenated, p-type multicrystalline silicon wafers after increasing the optical path length by preparation and polishing the edges of a stack of wafers. The concentrations of the H–B and H–Ga acceptor complexes are reduced to 80% of their starting values after low intensity (5 mW/cm2) illumination at room temperature for 96 h. Subsequent high intensity illumination (70 mW/cm2) at 150 °C for 7–8 h further decreases the concentrations of these defects; to ∼40% (H–B) and ∼50% (H–Ga) of their starting values. Our results show that, with careful sample preparation, IR spectroscopy can be used in conjunction with other techniques, e.g., quasisteady-state photoconductance, to investigate the involvement of different H-related point defects on degradation in solar-grade silicon wafers.
7 February 2023 in IEEE Journal of Photovoltaics
Operation and maintenance (O&M) is needed to limit losses caused by soiling and degradation in PV power plants, but accurate estimates of both mechanisms are necessary to inform decisions made by the O&M team. In the present work, we propose a novel performance metric, ${\boldsymbol{CP}}{{\boldsymbol{R}}}_{{\boldsymbol{soiling}}}$ , that can be used as input to algorithms that estimate soiling and degradation, e.g., combined degradation and soiling (CODS), stochastic rate and recovery (SRR), and the year-on-year (YOY) method, from performance time series data. We show that the proposed metric is robust even for locations with much cloud-cover where a clear-sky filter would remove too much of the data for the CODS algorithm to be effective. ${\boldsymbol{CP}}{{\boldsymbol{R}}}_{{\boldsymbol{soiling}}}$ values have been calculated with daily resolution using 3-years of data acquired from a 150+ MWp utility-scale solar power plant located in a semiarid landscape with a tropical wet and dry climate (“ As ” in the Köppen–Geiger climate classification system). Estimates of the daily soiling ratio obtained from the SRR and CODS algorithms have been compared with independent measurements carried out with 12 soiling stations and the results are in very good agreement. The average soiling rate for the soiling stations is $ - 0.07$ %/day, and the corresponding estimate is $ - 0.09$ and $ - 0.11$ %/day with the SRR and CODS algorithms, respectively. With CODS, the distribution of degradation rates is centered at $ - 0.12$ %/year, is less dispersed, and has fewer values outside the range reported in the literature for the “ As ” climate in comparison with the other state-of-the-art algorithms.
22 February 2019 in Journal of Applied Physics
Sequential degradation measurements have been performed on passivated high performance multicrystalline silicon wafers, first at room temperature under low intensity illumination followed by a higher intensity illumination at an elevated temperature. The presence of two main degradation mechanisms, affecting the lifetime under different conditions has been demonstrated, namely, the well-studied light induced degradation caused by boron-oxygen-complexes and the less understood light and elevated temperature induced degradation. Light and elevated temperature induced degradation is the main lifetime limiting the recombination path when fully activated, but the contribution from boron-oxygen complexes is not negligible. This separation of the two degradation mechanisms might, therefore, be necessary for proper evaluation of the dominant recombination mechanism. Experiments also show regeneration of the minority carrier lifetimes caused by deactivation of both the lifetime limiting defects at comparable time scales, and under similar illumination and temperature conditions. Wafers from different heights in a high performance multicrystalline silicon ingot have been evaluated to better understand the underlying causes for the different degradation mechanisms. Effects of the iron-boron-splitting on the carrier lifetime are only visible in ungettered wafers.
23 December 2020 in IEEE Journal of Photovoltaics
Accurate performance modeling of utility-scale PV plants is crucial for reducing the risk of investment, as well as improving operations and maintenance. In spite of much research, the precise rate at which PV plants degrade is still not well known. This article uses a well-known methodology for calculating degradation rates to assess the impact of climate on long-term performance. The RdTools analytic approach is used to perform a comparative case study of two utility-scale PV plants with the same setup and almost identical technology yet located in distinct climates. A significant difference is observed between the degradation rates of each park. The median of the nominal system degradation rate measured at the dc-side of the inverters in the hotter and more humid climate is -1.4%/yr, with 95% of the inverters between -1.5%/yr and -1.3%/yr, whereas in the temperate climate the median rate is -0.94%/yr, with 95% of the inverters between -1.0%/yr and -0.9%/yr. These results suggest that climate zones must be included when evaluating the long-term performance of PV plants.
29 September 2023 in IEEE Journal of Photovoltaics
Owing to the well-known temperature dependence of photovoltaic (PV) module performance, it is important to correct the performance ratio with respect to temperature. In this study, temperature coefficients given by the manufacturer for three different PV cell technologies are compared with experimentally obtained temperature coefficients for a PV park situated in southern Norway. Three irradiance estimation methods are used to calculate these experimental temperature coefficients. The results show that they can differ significantly from the ones provided in the datasheet of the manufacturer for all three PV systems, but whether the temperature coefficient value increases or decreases depends on the systems and/or the irradiance estimation method. Furthermore, by analyzing nine clear sky days at different times of the year, it is found that the seasonality of the performance ratio can be significantly reduced when employing the experimental temperature coefficient rather than the datasheet temperature coefficient. As such, it may be more relevant to correct the performance ratio with experimental temperature coefficients rather than with the temperature coefficient from the system datasheet, especially for systems that experience large temperature differences. It is also found that the irradiance estimation method can significantly impact the experimental temperature coefficient. This study shows that the choice of irradiance estimation method and temperature coefficient can affect the performance interpretation of solar PV systems and must then be considered carefully.
27 May 2021 in IEEE Journal of Photovoltaics
The rate at which silicon solar cells and wafers degrade and regenerate when subjected to light and elevated temperatures (LeTID) is known to depend on the minority carrier concentration. In this article, we utilize spatial differences in the rate of degradation and regeneration in multicrystalline silicon wafers to estimate the dependence of these rates on minority carrier concentration. We apply the relation obtained from spatial investigations in a model describing temporal LeTID defect evolution. With the updated model in which the evolving minority charge carrier density during degradation and regeneration is considered, we obtain a drastically improved fit between measured and modeled data. The activation energy for the regeneration process determined from our proposed model (0.56±0.12eV at 1 sun) is lower than most values reported in the literature but correspond perfectly to the activation energy reported by Graf et al. by whom evolving carrier injection is accounted for experimentally. Hence, our results underpin the importance of taking the evolution of charge carrier injection into account in the evaluation of LeTID kinetics. Finally, we use our updated model to obtain spatial maps of degradation and regeneration parameters. Clear correlations are shown between LeTID kinetics parameters and local processing conditions.