Władysław Zielecki

Władysław Zielecki

Auto-generated profile, based on publicly available information

Władysław Zielecki

The Faculty of Mechanical Engineering and Aeronautics, Rzeszów University of Technology, Powstańców Warszawy 12, 35-959 Rzeszów

Research Focus & Metrics

Academic Career Length

14Years (2013-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 June 2013 in Archives of Civil and Mechanical Engineering
Verified
Journal Article
Closed access
WZW. Zielecki
W. Zielecki
PPP. Pawlus
P. Pawlus
RPR. Perłowski
R. Perłowski
Andrzej DzierwaAndrzej Dzierwa
Andrzej Dzierwa

1 March 2017 in International Journal of Adhesion and Adhesives
Verified
Journal Article
Closed access
WZWładysław Zielecki
Władysław Zielecki
AKAndrzej Kubit
Andrzej Kubit
Tomasz TrzepiecińskiTomasz Trzepieciński
Tomasz Trzepieciński
NNNARKIEWICZ NARKIEWICZ
NARKIEWICZ NARKIEWICZ
ZCZbigniew Czech
Zbigniew Czech

6 September 2016 in Journal of Adhesion Science and Technology
Verified
Journal Article
Closed access
WZWładysław Zielecki
Władysław Zielecki
AKAndrzej Kubit
Andrzej Kubit
RKRafał Kluz
Rafał Kluz
Tomasz TrzepiecińskiTomasz Trzepieciński
Tomasz Trzepieciński
This paper presents the results of research undertaken to determine the possibility of improving the fatigue properties of peel-loaded adhesive-bonded joints by the constructional modification of the adherend. Fatigue strength tests were carried out on the electromagnetic inductor at the resonance frequency of the adhesive-bonded joint specimens. The tests were carried out on the specimens bonded by means of Bison Epoxy and Epidian 57 epoxy compositions with poly-aluminium chloride hardener. The joined elements were modified by making the chamfer or fillet to enlarge the thickness of the adhesive layer with the aim of reducing the stress concentration in the frontal part of the joint. This modification is the result of a research that confirms the existence of a stress concentration on the short section of the frontal part of an adhesive joint. This phenomenon can lead to the rapid initiation of adhesive joint destruction. The fatigue strength tests revealed a significant improvement in fatigue endurance.

1 July 2016 in Strength of Materials
Verified
Journal Article
Closed access
PDF file
AKAndrzej Kubit
Andrzej Kubit
WZW. Zielecki
W. Zielecki
MDM. Drabczyk
M. Drabczyk

5 January 2022 in The International Journal of Advanced Manufacturing Technology
Verified
Journal Article
Open access
PDF file
WZWładysław Zielecki
Władysław Zielecki
Tomasz TrzepiecińskiTomasz Trzepieciński
Tomasz Trzepieciński
ŁBŁukasz Bąk
Łukasz Bąk
EOEwelina Ozga
Ewelina Ozga
The goal of the work reported was to determine the influence of selected shot peening parameters on the deflection of the Almen strip and the load capacity of single-lap adhesive joints made of 2-mm-thick aluminium alloy EN AW-2024-T3. Moreover, the research was aimed at checking the possibility of using the Almen strip deflection indicator to predict the load capacity of adhesive joints after shot peening. The analysis was carried out according to Hartley’s PS/DS-P:Ha3 plan. The input factors were the shot peening parameters: treatment time t (60–180 s), ball diameter dk (0.5–1.5 mm) and compressed air pressure p (0.3–0.5 MPa). It has been proved in this work that shot peening treatment of the outer surface of single-lap adhesive joints can be used to strengthen the joint. The maximum increase in the load capacity of the shot peened joints was 33.4%. It was observed that the load capacity of the joints decreases with an increase in the deflection of the Almen strip (in the assumed area of variability of technological parameters). Moreover, the results obtained indicate that the adoption of too intensive treatment, manifested in high values of deflection of the Almen strip, may weaken single-lap adhesive joints.

1 January 2023 in Technologia i Automatyzacja Montażu
Verified
Journal Article
Open access
PDF file
AKAndrzej Kubit
Andrzej Kubit
RTRzeszow University of Technology
Rzeszow University of Technology
WZWładysław Zielecki
Władysław Zielecki
Ľuboš KaščákĽuboš Kaščák
Ľuboš Kaščák
PSPaulina Szawara
Paulina Szawara
The paper presents the influence of simple structural modifications of the adherend on the fatigue properties of adhesive joints subjected to peel. The considered modifications consisted in making a chamfer and fillet on the front edge of the adherend. The purpose of such modifications was to locally increase the thickness of the adhesive layer in the area of stress concentration. Fatigue strength tests were carried out using an electrodynamic shaker at the resonant frequency of the flexible adherend. On the basis of fatigue strength tests carried out at the limited number of cycles equal to 2×106, it was shown that a local increase in the thickness of the adhesive layer in the front part of the joint allows a significant increase in the joint's fatigue lifetime and fatigue strength. The greatest effect was shown for the variant with the fillet R2. In this case, an increase in fatigue strength of 33.1% compared to the base variant was demonstrated. For the fatigue stress level of 20.25 MPa, an increase in fatigue lifetime of 337.7% was also demonstrated. Based on the conducted research, it was shown that the reason for the improvement of the fatigue properties of the joints due to the local increase in the thickness of the adhesive layer is the phenomenon of energy absorption in the frontal area of the joint. Absorption of energy that inhibits the process of fatigue results from, among others, local flexibility of the joint, as well as nucleation of cracks in the locally increased volume of the adhesive.