HongJin Wang

HongJin Wang

Auto-generated profile, based on publicly available information

HongJin Wang

Department of Materials Engineering, Jiangsu University of Technology, Changzhou, 213100, People’s Republic of China

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
24 August 2022 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
HWHongJin Wang
HongJin Wang
SSShunPing Sun
ShunPing Sun
XLXiaoPing Li
XiaoPing Li
JWJianHua Wang
JianHua Wang
XSXuPing Su
XuPing Su

1 August 2021 in Materials Research Express
Verified
Journal Article
Open access
BWBin Wang
Bin Wang
SSshunping sun
shunping sun
HWHongJin Wang
HongJin Wang
XLXiaoPing Li
XiaoPing Li
WLWeiNing Lei
WeiNing Lei
Different proportions of Al and Cr alloying MoSi2 were prepared by arc cladding with different mass fractions of MoSi2, Al, and Cr as raw materials. The work studied the effects about of Al and Cr on the phase, high-temperature oxidation morphology, products, and high-temperature oxidation property of MoSi2. The results confirmed that the volume expansion coefficient of Al2O3 generated by material oxidation was low which could reduce the degree of mismatch and the cracks in the oxide film. Cr element had a poor effect on enhancing the continuity and compactness of the oxide film, however, it could improve the stability of t-MoSi2 formation after arc cladding. MoO3 was not formed in the MoSi2 material added with Al and Cr show the surface oxidation. A dense and continuous Al2O3–SiO2 oxide film was formed, and no cracks holes were found in the oxide film. After oxidation at 800 °C–1200 °C for 120 h, the sample still maintained good oxidation protection. According to the calculation of oxidation kinetics, the MoSi2 material added with Al and Cr had good oxidation resistance. 3% Al + 9% Cr + 88% MoSi2 had the optimal high-temperature oxidation resistance about four times than pure MoSi2.

1 October 2025 in Materials Research Express
Verified
Journal Article
Open access
YWYiqi Wang
Yiqi Wang
XLXiao Liu
Xiao Liu
CZChunkai Zhou
Chunkai Zhou
HWHongjin Wang
Hongjin Wang
HNHongwei Niu
Hongwei Niu
BZBin Zhu
Bin Zhu
In this study, thin-walled 7075 aluminum alloy samples were fabricated using Single-Bead Multi-Layer Wire Arc Additive Manufacturing (WAAM) with self-developed 7075 aluminum alloy welding wire and metal inert gas (MIG) welding. The samples underwent solid solution treatment followed by double-stage aging heat treatment. The metallographic structure, precipitate phases, and mechanical properties of the additive samples before and after heat treatment were investigated using optical microscopy (OM), electron backscatter diffraction (EBSD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS). The results indicate that, without heat treatment, the grains in the WAAM 7075 aluminum alloy samples exhibited a distinct weld structure with noticeable orientation. The precipitated phases, such as η(MgZn2), S (Al2CuMg), and T (AlZnMgCu), were observed to form along the grain boundaries, with high-melting-point compounds like AlMnFeSi, Al13Fe4, and Mg2Si serving as nuclei. The weak fusion zones between adjacent weld beads contributed to poor mechanical properties in the as-deposited state, with no significant difference in mechanical performance between the Y(deposition direction) and X(cladding direction). After heat treatment, the η, S, and T phases were completely dissolved into the matrix, resulting in solid solution strengthening and aging. The interlaminar fusion zone (IFZ) grains recrystallized into equiaxed structures, improving the tensile strength and elongation in the cladding direction to 464.2 MPa and 13.11%, respectively. However, the presence of residual insoluble Fe and Si compounds limited further mechanical property improvements, and large pores densely distributed within the interlayer caused lower mechanical properties in the deposition direction compared to the cladding direction.

1 January 2022 in SSRN Electronic Journal
Verified
Preprint
Open access
PDF file
HWHongjin Wang
Hongjin Wang
SSShunPing Sun
ShunPing Sun
XLXiaoPing Li
XiaoPing Li
JWJianhua Wang
Jianhua Wang
XSXuPing Su
XuPing Su
Interfacial reaction and morphology are investigated between pure iron sheet and aluminum alloy with different silicon additions in hot-dip aluminizing at 700°C. The intermetallic reaction layer hot-dipped in a pure aluminum bath is mainly governed by the diffusion controlled growth of the η-Al 5 Fe 2 phase, which changes with time according to a parabola rule. Al atoms can diffuse rapidly in a preferred [001] direction, thereby causing the continuous growth of η phase with a tongue-like morphology. The thickness of the θ-Al 13 Fe 4 phase layer exhibits a slow linear growth with the increase of dipping time. Adding silicon into aluminum baths reduces the growth rate of the reaction layer and eliminates the rough interface. The effect of Si inhibiting the growth of η phase can be attributed to the segregation of Si atoms at the Fe/Al interface. The Si concentration segregation in θ and η phase hinders the rapid diffusion of Al atoms, resulting in the structural vacancy obstruction, which is responsible for the thickness reduction. The investigation reveals that the continuous τ 1 -Al 2 Fe 3 Si 3 ternary phase layer will be formed as the segregation concentration of the Si atoms reach 5 at.% at the interface between Al-4Si alloy and θ phase. The continuous τ 5 -Al 8 Fe 2 Si layer is observed in the reaction layer of Al-6Si and Al-10Si. The continuous Al-Fe-Si ternary phase layer can reduce the growth rate of η phase as a diffusion barrier. The diffusion of Si at the interface will control the phase transformation of θ phase with a low Si content to higher Si containing τ 1 and τ 5 phase.