King Saud University, College of Dentistry, Department of Prosthetic Dental Sciences, Riyadh, Saudi Arabia

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2019 in Brazilian Oral Research
Verified
Journal Article
Open access
PDF file
SHSyed Rashid Habib
Syed Rashid Habib
AAAbdul Sadekh Ansari
Abdul Sadekh Ansari
MAMohammed Alqahtani
Mohammed Alqahtani
IAIbrahim F Alshiddi
Ibrahim F Alshiddi
AAAbdulaziz Alqahtani
Abdulaziz Alqahtani
SHSyed Hammad Hassan
Syed Hammad Hassan
The objective of the study was to analyze the surface area (SA) of the wear caused by simulated chewing on human enamel and opposing restorative material, namely: composite resin (CR), porcelain fused to metal (PFM), lithium disilicate (LD), or monolithic zirconia (MZr). Forty-eight premolars were selected as enamel specimens and divided randomly into 4 groups (n = 48; n =12) used as antagonists in chewing simulation (250,000 loading cycles) against one of the four selected test materials. Enamel and material specimens were scanned and evaluated under digital microscope, and wear SA (mm2) were recorded. Descriptive statistics, paired t-test, one-way ANOVA, and post-hoc Tukey-HSD tests were used for statistics (p < 0.05). The smallest and largest SA were exhibited by enamel against LD (0.80 mm2) and PFM (1.74 mm2), respectively. PFM (3.48 mm2) showed the largest SA and CR (2.28 mm2) showed the smallest SA. Paired t-test for SA values showed significant difference (p < 0.05) in all wear comparisons between materials and enamel antagonists. The wear of materials were greater than that of their respective enamel antagonists (p < 0.05). One-way ANOVA of the logarithmic means of wear SA revealed significant differences (P<0.05). Post-hoc Tukey test revealed significance for PFM (p < 0.05) with other materials. Wear of all test materials was greater compared to the wear of enamel antagonists. PFM and LD caused the largest and the smallest enamel wear, respectively. CR, LD, and MZr are more resistant than PFM to wear after simulated chewing against enamel.