Bartłomiej SZWED

Bartłomiej SZWED

Auto-generated profile, based on publicly available information

Bartłomiej SZWED

Kielce University of Technology, Kielce, Poland, EU

Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 June 2016 in Archives of Metallurgy and Materials
Verified
Journal Article
Open access
PDF file
BSB. Szwed
B. Szwed
MKMarek Konieczny
Marek Konieczny
Diffusion brazing was performed between titanium (Grade 2) and stainless steel (X5CrNi18-10) using as a filler a nickel foil at the temperatures of 850, 900, 950 and 1000°C. The microstructure was investigated using light microscopy and scanning electron microscopy equipped with an energy dispersive X-ray system (EDS). The structure of the joints on the titanium side was composed of the eutectoid mixture αTi+Ti2Ni and layers of intermetallic phases Ti2Ni, TiNi and TiNi3. The stainless steel-nickel interface is free from any reaction layer at 850°C, above this temperature thin layer of reaction appears. The microhardness measured across the joints reaches higher values than for titanium and stainless steel, and it achieves value from 260 to 446 HV. The highest shear strength (214 MPa) was achieved for joints brazed at 900°C

10 December 2018 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
BSB Szwed
B Szwed
MKMarek Konieczny
Marek Konieczny
In the present investigation, transient liquid-phase bonding was performed between pure titanium (Grade 2) and stainless steel (X5CrNi 18-10) using nickel foil as an intermediate material. The process was carried out at the temperatures of: 950, 975 and 1000 ° C for 60 minutes under the compressive stress of 2 MPa in a vacuum. The microstructure was investigated using light microscopy and scanning electron microscopy equipped EDS. The metallographic examination shows that the diffusion interfaces are free from cracks. However, Kirkendall voids were observed at the borders of materials. Especially large voids were formed in middle section of the joint prepared using the highest bonding temperature. The structure of the joints on the titanium side was composed of the eutectoid mixture αTi+Ti2Ni and layers of intermetallic phases Ti2Ni, TiNi and TiNi3. The nickel interlayer blocked the diffusion of titanium to stainless steel side at 950 °C bonding temperature and prevented from formation of the Fe-Ti intermetallic layers. The layer of a solid solution γFe+Ni between nickel and stainless steel was observed at the 950 °C processing temperature. The mixture of λ+FeTi+Ti, FeTi+Ti, λ+αFe and λ+χ+αFe phases was formed at 975 and 1000 °C at the nickel-stainless steel interlayer.

10 December 2018 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
BSB Szwed
B Szwed
MKMarek Konieczny
Marek Konieczny
The purpose of this study is to compare corrosion resistance of the joints between commercially pure titanium (Grade 2) and stainless steel (X5CrNi18-10) bonded by interlayers made of pure metals. Three different interlayers were used in the study, which were made of aluminium (Al 99.5), copper (Cu 99.99) and nickel (Ni 99.6). The diffusion bonding process has been employed to join those dissimilar materials. The microstructure of the joints were investigated using scanning electron microscopy equipped with an energy dispersive X-ray system (EDS). The phases of the reaction layers in the diffusion zone were identified by means of an X-ray diffraction (XRD).The structures of the joints varied importantly depending on the interlayer. The galvanic corrosion test was carried out in two solutions one in a 3,5% NaCl and second one in 1M Na2SO4 solution. The potentiodynamic polarization curves in a 3,5% NaCl solution show that the higher corrosion potential as well as a lower corrosion current were registered for the joints performed by nickel. The test carried out in 1M Na2SO4 solution show that that the lowest corrosion current was registered for the joints performed by copper and also all investigated samples have a tendency towards passivation.

6 April 2023 in Communications - Scientific letters of the University of Zilina
Verified
Journal Article
Open access
PDF file
PKPiotr Kurp
Piotr Kurp
HDHubert Danielewski
Hubert Danielewski
BSBartłomiej Szwed
Bartłomiej Szwed
KBKrzysztof Borkowski
Krzysztof Borkowski
AZAndrej Zrak
Andrej Zrak
OGOksana P. Gaponova
Oksana P. Gaponova
In this paper, the authors discuss the method of deformations compensation (resulting from the impact of variable temperatures and pressure) in pipelines intended for fluids transport (liquids and gases). Classical methods of compensation thro...

1 January 2023
Verified
Conference Paper
Open access
STSzymon Tofil
Szymon Tofil
PKPiotr Kurp
Piotr Kurp
HDHubert Danielewski
Hubert Danielewski
BSBartłomiej SZWED
Bartłomiej SZWED