It is an attributed fact that magnesium, in normal conditions, behaves as active or anodic material and steel as a noble or cathodic material in a galvanic cell. In the current study, various experiments have been conducted to investigate the electrochemical behavior of magnesium and mild steel galvanic couples in tap water and 0.1M NaHCO3 corrosive environments at different temperatures (40 ℃ to 80 ℃). The potentiodynamic results have confirmed that in tap water, magnesium acts as an anode as it corrodes itself and protects steel surfaces under the influence of galvanic action at selected temperatures. However, magnesium became passive under 0.1M NaHCO3 making steel anodic, which deteriorates aggressively at higher temperatures in 0.1M NaHCO3. The polarity reversal phenomenon was also observed in the magnesium-steel couple when exposed to this environment. The microstructural examination has shown that passivation occurred due to the formation of an oxide layer that grew towards the steel side in the galvanic couple as the temperature increased. Thus, the study revealed that the magnesium would be more damaging to steel in a NaHCO3 environment if utilized in the temperature range of 60 ℃to 80 ℃.
26 March 2026 in Journal of Advanced Electronic Materials
This study focuses on the solid-state processing optimization of SrTi\(_{1-x}\)Fe\(_x\)O\(_3\) (STFO) ceramics with \(0.00 \leq x \leq 0.11\). X-ray diffraction reveals a single-phase cubic structure (space group Pm\(\bar{3}m\)) with lattice constant \(a = b = c = 3.91{Å}\) and a maximum relative density of \(\sim\)94%. SEM confirms well-formed grains in both pure and Fe\(^{3+}\)-doped SrTiO\(_3\). TGA/DSC indicates low weight loss and high thermal stability for the \(x = 0.09\) composition. Electrical conductivity increases with frequency, accompanied by higher dielectric losses for \(x = 0.09\) and \(x = 0.11\). FTIR verifies the Ti-O octahedral stretching frequency at \SI{530}{\cm^{-1}}, consistent with the cubic perovskite structure. The maximum Seebeck coefficient is observed at \(x = 0.09\), aligning with electrical data and confirming semiconducting behavior. Notably, calcined powders exhibit soft ferromagnetic loops, whereas sintered solids display antiferromagnetic loops, revealing intriguing magnetic properties. Overall, the optimized \(x = 0.09\) composition shows significant promise for applications requiring enhanced electrical and magnetic characteristics.
19 August 2026 in Journal of Advanced Electronic Materials
A series of non-stoichiometric BaK$_{1-x}$Na$_x$Gd$_3$Fe$_5$O$_{15}$ ($x = 0.00$, 0.10, 0.20, 0.30) tetragonal tungsten bronze (TTB) ceramics were synthesized via solid-state reaction, cold sintering at 150$^\circ$C, and assisted sintering at 400$^\circ$C and 500$^\circ$C. XRD confirmed single-phase TTB formation. Enhanced crystallinity and sharper diffraction peaks with increasing assisted sintering temperature indicated improved grain growth and ordering. Density measurements revealed Na$^+$ substitution combined with salt-assisted processing significantly influenced densification, with BKGF-1NST$_2$ achieving the highest bulk density of 4.32g/cm$^3$. Dielectric characterization showed frequency-dependent behavior with decreasing loss at higher frequencies, while selected compositions exhibited stable dielectric response after 500$^\circ$C assisted sintering. Magnetic measurements confirmed ferrimagnetic behavior via Fe$^{3+}$-mediated interactions. BKGF-2NT$_2$ ($x = 0.20$, assisted sintered at 500$^\circ$C) delivered optimal magnetic performance: $M_s = 4.97$emug$^{-1}$, $M_r = 1.59$emug$^{-1}$, $H_c = 1435.84$Oe, attributed to optimized exchange interactions, improved crystallinity, and enhanced grain connectivity. Co-doping with cold-assisted sintering governs the structural, dielectric, and magnetic properties of TTB ceramics.