27 January 2016 in Journal of the Electrochemical Society
Gassing in lithium-ion batteries (LIBs) is a serious challenge, especially at high voltage and elevated temperature. In this study, we use On-line Electrochemical Mass Spectrometry (OEMS) and a two-compartment cell with a newly developed aluminum edge-seal to elucidate the origin of H2 evolution in LIBs. We demonstrate that the new sealing is entirely impermeable for gaseous and liquid species, thus allowing us to measure the true H2 evolution from H2O reduction at a graphite electrode, without interference from the lithium counter-electrode. We further report that graphite//NMC full-cells without any diffusion barrier between anode and cathode show enhanced H2 generation, especially for high charging potentials and at elevated temperature. We propose that the diffusion of protic electrolyte oxidation species (R-H+) from the cathode to the anode and their subsequent reduction is the origin of enhanced H2 gassing. To prove this hypothesis, methanesulfonic acid is added to the electrolyte as a chemical source of protons. At the negative graphite electrode, all H+ can be quantitatively reduced to H2. By the use of the electrolyte additives vinylene carbonate (VC) and lithium bis(oxalato) borate (LiBOB), less H2 evolution is observed, since the reduction of both H2O and R-H+ is hindered by a more effective SEI on graphite. Finally, we demonstrate that the Al-sealed diffusion barrier between anode and cathode can stop the diffusion of oxidation products to the anode and therefore essentially eliminates the generation of H2 caused by high cathode potentials.
22 December 2016 in Journal of the Electrochemical Society
14 November 2019 in Journal of the Electrochemical Society
Ni-rich layered oxides, like NCM-811, are promising lithium-ion battery cathode materials for applications such as electric vehicles. However, pronounced capacity fading, especially at high voltages, still lead to a limited cycle life, whereby the underlying degradation mechanisms, e.g. whether they are detrimental reactions in the bulk or at the surface, are still controversially discussed. Here, we investigate the capacity fading of NCM-811/graphite full-cells over 1000 cycles by a combination of in situ synchrotron X-ray powder diffraction, impedance spectroscopy, and X-ray photoelectron spectroscopy. In order to focus on the NCM-811 material, we excluded Li loss at the anode by pre-lithiating the graphite. We were able to find a quantitative correlation between NCM-811 lattice parameters and capacity fading. Our results prove that there are no considerable changes in the bulk structure, which could be responsible for the observed ≈20% capacity loss over the 1000 cycles. However, we identified the formation of a resistive surface layer, which is responsible for (i) an irreversible loss of capacity due to the material lost for its formation, and (ii) for a considerable impedance growth. Further evidence is provided that the surface layer is gradually formed around the primary NCM-811 particles.
3 December 2019 in Journal of the Electrochemical Society
Washing is a commonly used method to remove surface impurities of cathode materials for lithium-ion batteries. However, a clear mechanistic understanding of the washing process is missing in the literature. In this study, we will investigate the effect of washing and subsequent drying of nickel-rich NCM cathodes (85% nickel) with respect to gassing and impedance of the washed cathodes. By on-line electrochemical mass spectrometry (OEMS), we will show a drastic reduction of the O2 release above 80% SOC for the NCM washed with deionized water, suggesting the formation of an oxygen-depleted surface layer on the NCM particle surface. The modification of the surface can be confirmed by a strong impedance buildup of cathodes composed of washed NCM (using a micro-reference electrode in a full-cell), revealing that the impedance increases strongly with increasing drying temperature after washing. Last, we will propose a comprehensive mechanism on the processes occurring during the washing/drying process of nickel-rich NCM materials and identify the drying temperature after washing as the dominant factor influencing the surface properties.
3 May 2018 in Chemistry of Materials
14 April 2016 in Journal of the Electrochemical Society
This study deals with the decomposition of ethylene carbonate (EC) by H2O in the absence and presence of catalytically active hydroxide ions (OH−) at reaction conditions close to lithium-ion battery operation. We use On-line Electrochemical Mass Spectrometry (OEMS) to quantify the CO2 evolved by these reactions, referred to as H2O-driven and OH−-driven EC hydrolysis. By examining both reactions at various temperatures (10 – 80°C) and water concentrations (<20 ppm or 200, 1000, and 5000 ppm H2O) with or without catalytically active OH− ions in EC with 1.5 M LiClO4, we determine an Arrhenius relationship between the CO2 evolution rate and the cell temperature. While the apparent activation energy for the base electrolyte (<20 ppm H2O) is very large (app. Ea ≈153 kJ/mol), substantially lower values are obtained in the presence of H2O (app. Ea ≈99 ± 3 kJ/mol), which are even further decreased in the presence of catalytically active OH− (app. Ea ≈43 ± 5 kJ/mol). Our data show that OH−-driven EC hydrolysis is relevant already at room temperature, whereas H2O-driven EC hydrolysis (i.e., without catalytically active OH−) is only relevant at elevated temperature (≥40°C), as is the case for the base electrolyte. Thus, catalytic quantities of OH−, e.g., from hydroxide contaminants on the surface of transition metal oxide based active materials, would be expected to lead to considerable CO2 gassing in lithium-ion cells.