In the development of dynamic random access memory (DRAM) with a device size of 20 nm or less, the leakage current of a capacitor with high-k dielectrics is one of the main factors causing the failure of a device. To reduce the failure rate of the device, we conducted experiments to reduce the boron impurities, which form defect sites in the dielectrics of the capacitor. The boron source flux was reduced during the deposition process of the capping layer after the formation of the capacitor, and the actual boron concentration in the capping layer was measured by an atom probe tomography. The leakage current characteristics of the samples were confirmed through the dielectric leakage failure test, which is a mass production test technique. In addition, the resistance failure test was performed to measure the risk of increased resistance. From these results, it was confirmed that the failure rate due to the leakage current of the capacitor decreased linearly with reduced boron concentration and the increase in failure rate due to the cell node resistance was negligible. In addition, the results show that the failure rate of mass-produced DRAM products can be significantly reduced without any change in the structure or materials of the capacitor. This is expected to contribute greatly to the development of DRAM with dimensions on the scale of 20 nm or less.
In this paper, the dependence of threshold voltage (Vth) changes to amorphous-indium gallium zinc oxide (a-IGZO) thin film transistors (TFTs) under positive bias light illumination (PBIS) on the height of the conduction band offset was studied. Using SiO2, HfO2, and Al2O3 as gate dielectrics, three different types of a-IGZO TFTs were used in the experiment. Electrical parameters and the density of states of each TFT were measured. Of the devices studied, the interface characteristics between the a-IGZO and the gate dielectric were the best using SiO2 and the worst using Al2O3. HfO2 had the smallest conduction band offsets (CBO) of 2.26 eV. We also performed PBS and PBIS evaluation to confirm the stability of TFTs. The Vth shift in the three samples was insignificant under PBS, but the Vth shifts occurred under PBIS in the order of HfO2, Al2O3, and SiO2. The interfacial characteristics of a-IGZO and the dielectric did not change after PBIS in all three devices; the lower the CBO height, the greater the Vth shift after PBIS. The predominant cause of the Vth shift under PBIS is the accumulation of injected photoelectrons that have sufficient energy to tunnel the CBO barrier into the gate dielectric by positive gate bias.
1 September 2015 in Journal of the Korean Physical Society
Multicrystalline silicon (mc-Si) solar cells were developed by using a direct laser texturing method. Approximately 10-μm-deep and 10-μm-diameter cone-shaped grooves, with an aspect ratio (determined by the depth-to-diameter ratio) of one, were produced on the wafer’s surface by using a 355-nm-wavelength ultraviolet (UV) laser process. After slag removal and chemical etching, V-shaped cross-sectional microstructures were regularly arranged in a honeycomb disposition on the surface. Compared to the mc-Si solar cell textured by using isotropic acidic etching, the surface reflectance was reduced to 3.3% and the short-circuit current increased to 0.8 mA/cm2 when the cell was treated with UV laser ablation. The solar cell values were achieved from the increased electron-hole pairs (EHPs) generated by the enhanced bouncing of incident light, which was aided by the V-shaped microstructures. The cell efficiency of a UV-laser-textured cell was improved to 16.1% compared to the 15.5% for an acidic-solution-textured cell.
Vertical cell transistor is necessary to drastically reduce the chip size of the dynamic random access memory. This structure has a great advantage in terms of shrinkage, but it also has the disadvantage of increasing the OFF‐state current by causing floating body effect (FBE). For the first time, it is demonstrated that a stretched tunnelling diode, which consists of a p + layer next to the n + active layer in the buried body, leads to a drastically suppressed FBE. The OFF‐state current is sharply reduced by about seven orders compared with a conventional structure. Furthermore, the decrease in the OFF‐state current is at minimum when the length of the stretched p + region is approximately half the channel length ( Lp / L =1/2).