An electric field–temperature (E-T) phase diagram for a lead-free 0.5 mol. % Mn-doped Bi(Na0.1K0.9)TiO3 ceramics was investigated. The x-ray diffraction, dielectric and polarization measurements revealed relaxor behavior and were used to characterize the stability regions of the non-ergodic relaxor, ergodic relaxor and electric field induced ferroelectric states. As indicated by the polarization–current density profiles, transformation between two electric fields, induced ferroelectric states with opposite polarization direction arise via a two-step process through an intermediate relaxor state. Interplay between the ferroelectric state conversion and intermediate relaxor state is governed by the dynamics of polarization relaxation. The presented E-T phase diagram revealed the effects of the applied electric field and temperature on stability regions. This is of special interest since the Bi0.5(Na0.1K0.9)0.5TiO3 ceramics were proposed as a potential piezoceramic material.
1 June 2011 in Science and Technology of Advanced Materials
We have studied the strain field around the 90° domains and misfit dislocations in PbTiO3/SrTiO3 (001) epitaxial thin films, at the nanoscale, using the geometric phase analysis (GPA) combined with high-resolution transmission electron microscopy (HRTEM) and high-angle annular dark field--scanning transmission electron microscopy (HAADF-STEM). The films typically contain a combination of a/c-mixed domains and misfit dislocations. The PbTiO3 layer was composed from the two types of the a-domain (90° domain): a typical a/c-mixed domain configuration where a-domains are 20-30 nm wide and nano sized domains with a width of about 3 nm. In the latter case, the nano sized a-domain does not contact the film/substrate interface; it remains far from the interface and stems from the misfit dislocation. Strain maps obtained from the GPA of HRTEM images show the elastic interaction between the a-domain and the dislocations. The normal strain field and lattice rotation match each other between them. Strain maps reveal that the a-domain nucleation takes place at the misfit dislocation. The lattice rotation around the misfit dislocation triggers the nucleation of the a-domain; the normal strains around the misfit dislocation relax the residual strain in a-domain; then, the a-domain growth takes place, accompanying the introduction of the additional dislocation perpendicular to the misfit dislocation and the dissociation of the dislocations into two pairs of partial dislocations with an APB, which is the bottom boundary of the a-domain. The novel mechanism of the nucleation and growth of 90° domain in PbTiO3/SrTiO3 epitaxial system has been proposed based on above the results.
Lead zirconate titanate, Pb(Zr,Ti)O3 or PZT, is one of the most widely investigated ferroelectric and piezoelectric materials due to its superior properties. However, the intrinsic properties of PZT have not been directly measured due to the lack of fabrication of single crystals even though a basic understanding of intrinsic properties has been of interest developing lead-free piezoelectric materials. We demonstrated the direct observation of the intrinsic piezoelectric property by means of the detection of electric-field induced crystal lattice distortion of thick Pb(Zr0.35Ti0.65)O3 single-crystalline films with single polar-axis orientation and negligible residual strain using the time-resolved X-ray diffraction (XRD) together with the polarization response. Consequently, the effective converse piezoelectric response was experimentally revealed; hence, the electrostrictive coefficient, which is the conversion coefficient between the electrical and mechanical response, was determined. The obtained effective electrostrictive coefficient was 5.2–6.3 × 10−2 m4/C2, which agrees with theoretical prediction.
The effects of bipolar pulse poling on the ferroelastic domain structure and their contribution to the electrical and piezoelectric properties of Pb(Ti0.7Zr0.3)O3 films are investigated. Micro x-ray diffraction measurements clearly show that the volume fraction of the c-domain increases irreversibly as the poling field is increased, leading to changes in the remanent polarization, dielectric constant, and piezoelectric coefficient. Theoretical estimations well explain the changes of remanent polarization and dielectric constant, but the increase in piezoelectric coefficient is much larger than the theoretical estimation. In-situ x-ray diffraction analysis under an electric field reveals that this disagreement is due to the unexpected activation of the ferroelastic domain wall motion. Our results provide new insight into the poling effect on the electric and piezoelectric properties of ferroelectric films.
An approach for probing dynamic phenomena during hysteresis loop measurements in piezoresponse force microscopy (PFM) is developed. Dynamic PFM (D-PFM) necessitates development of 5-dimensional (5D) data acquisition protocols and associated methods for analysis and visualization of multidimensional data. Using a combination of multivariate statistical analysis and phenomenological fitting, we explore dynamic behavior during polarization switching in model ferroelectric films with dense ferroelastic domain structures and in ferroelectric capacitors. In polydomain films, multivariate analysis of the switching data suggests that ferroelectric and ferroelastic components can be decoupled and time dynamics can be explored. In capacitors, a strong correlation between polarization dynamics and microstructure is observed. The future potential of D-PFM for probing time-dependent hysteretic phenomena in ferroelectrics and ionic systems is discussed.
The ferroelectric property, crystal structure, and soft mode of almost strain-free epitaxial polar axis-oriented tetragonal lead zirconate titanate thick films grown on substrates were investigated by changing the ratio and the temperature. The square of spontaneous polarization , , monotonically increased as tetragonal distortion, , increased where and are the lattice parameters of the films and as the square of frequency in , , increased. Additionally, the relationships of , , and were experimentally obtained, which confirmed the value obtained from and without direct polarization measurements.