5 September 2022 in Applied Physics Letters
The performance of vertical-cavity surface-emitting lasers (VCSELs) is strongly dependent on the spectral detuning between the gain peak and the resonance wavelength. Here, we use angle-resolved photoluminescence spectroscopy to investigate the emission properties of AlGaN-based VCSELs emitting in the ultraviolet-B spectral range with different detuning between the photoluminescence peak of the quantum-wells and the resonance wavelength. Accurate setting of the cavity length, and thereby the resonance wavelength, is accomplished by using doping-selective electrochemical etching of AlGaN sacrificial layers for substrate removal combined with deposition of dielectric spacer layers. By matching the resonance wavelength to the quantum-wells photoluminescence peak, a threshold power density of 0.4 MW/cm2 was achieved, and this was possible only for smooth etched surfaces with a root mean square roughness below 2 nm. These results demonstrate the importance of accurate cavity length control and surface smoothness to achieve low-threshold AlGaN-based ultraviolet VCSELs.
23 March 2020 in Applied Physics Letters
We demonstrate a thin-film flip-chip (TFFC) light-emitting diode (LED) emitting in the ultraviolet B (UVB) at 311 nm, where substrate removal has been achieved by electrochemical etching of a sacrificial N layer. The electroluminescence spectrum of the TFFC LED corresponds well to the as-grown LED structure, showing no sign of degradation of structural and optical properties by electrochemical etching. This is achieved by a proper epitaxial design of the sacrificial layer and the etch stop layers in relation to the LED structure and the electrochemical etch conditions. Enabling a TFFC UV LED is an important step toward improving the light extraction efficiency that limits the power conversion efficiency in AlGaN-based LEDs.
29 October 2019 in Physica Status Solidi (a)
Herein, a systematic study of the morphology and local defect distribution in epitaxially laterally overgrown (ELO) AlN on c‐plane sapphire substrates with different off‐cut angles ranging from 0.08° to 0.23° is presented. Precise measurements of the off‐cut angle α, using a combination of optical alignment and X‐ray diffraction with an accuracy of ±5° for the off‐cut direction and ±0.015° for the off‐cut angle, are carried out. For ELO AlN growth, a transition from step flow growth at α < 0.14° with height undulations on the surface to step bunching with step heights up to 20 nm for α > 0.14° is observed. Furthermore, the terraces of the step‐bunched surface exhibit curved steps. An analysis of the local defect distribution by scanning transmission electron microscopy and a comparison with atomic force microscopy reveal a bunching of defects in line with the ELO pattern and a roughening of step edges in highly defective regions. In addition, a reduction in the threshold excitation power density for optically pumped ultraviolet‐C (UVC) lasers with smooth surface morphologies is observed.
11 October 2018 in Journal of Physics D: Applied Physics
In this paper the internal electric fields of nearly lattice matched InAlN/GaN heterostructures were determined. Pin -diodes containing InAlN/GaN heterostructures grown on sapphire substrates by metalorganic vapour phase epitaxy were fabricated by standard lithography and metallization techniques. To determine the polarization fields in the InAlN quantum wells capacitance-voltage-measurements were performed on the pin -diodes. To reduce the measurement error, the heterostructure thicknesses were accurately determined by transmission electron microscopy. Large polarization fields, which correspond mainly to the spontaneous polarizations, for In 0.15 Al 0.85 N ( MV cm −1 ), In 0.18 Al 0.82 N ( MV cm −1 ) and In 0.21 Al 0.79 N ( MV cm −1 ) quantum wells were observed. The results of the internal field strength and field direction are in excellent agreement with values predicted by theory and a CVM-based coupled Poisson/carrier transport simulation approach.
16 April 2019 in Japanese Journal of Applied Physics
Consistent studies of the quaternary composition are rare as it is impossible to fully determine the quaternary composition by X-ray diffraction or deduce it from that of ternary alloys. In this paper we determined the quaternary composition by wavelength dispersive X-ray spectroscopy of In
x
Al
y
layers grown by metal organic vapor phase epitaxy. Further insights explaining the peculiarities of In
x
Al
y
Ga
1−
x
−
y
N growth in a showerhead reactor were gained by simulations of the precursor decomposition, gas phase adduct formation and indium incorporation including desorption. The measurements and simulations agree very well showing that the indium incorporation in a range from 0% to 2% is limited by desorption which is enhanced by the compressive strain to the relaxed Al 0.5 Ga 0.5 N buffer layer as well as indium incorporation into AlN particles forming in the gas phase. Utilizing In
x
Al
y
Ga
1−
x
−
y
N layers containing 2% of indium for multiple quantum wells (MQWs), it was possible to show an almost five times higher photoluminescence intensity of InAlGaN MQWs in comparison to AlGaN MQWs.
5 July 2021 in Microscopy and Microanalysis
Wavelength-dispersive X-ray (WDX) spectroscopy was used to measure silicon atom concentrations in the range 35–100 ppm [corresponding to (3–9) × 1018 cm−3] in doped AlxGa1–xN films using an electron probe microanalyser also equipped with a cathodoluminescence (CL) spectrometer. Doping with Si is the usual way to produce the n-type conducting layers that are critical in GaN- and AlxGa1–xN-based devices such as LEDs and laser diodes. Previously, we have shown excellent agreement for Mg dopant concentrations in p-GaN measured by WDX with values from the more widely used technique of secondary ion mass spectrometry (SIMS). However, a discrepancy between these methods has been reported when quantifying the n-type dopant, silicon. We identify the cause of discrepancy as inherent sample contamination and propose a way to correct this using a calibration relation. This new approach, using a method combining data derived from SIMS measurements on both GaN and AlxGa1–xN samples, provides the means to measure the Si content in these samples with account taken of variations in the ZAF corrections. This method presents a cost-effective and time-saving way to measure the Si doping and can also benefit from simultaneously measuring other signals, such as CL and electron channeling contrast imaging.