The main aim of the present study was to prepare a-C:H:SiOx coatings with sufficient mechanical properties from the mixture of CH4 with trimethylsilyl acetate (TMSAc) or hexamethyldisiloxane (HMDSO) organosilicon precursor using plasmas of RF capacitively coupled glow discharge.Studied coatings were prepared using various precursor ratios in the reaction mixtures, ranging from 7.1 % to 92.9 %, at a constant discharge power of 75 W. The included research work discusses in detail the evolution of the chemical composition, structure, and mechanical characteristics of the resulting a-C:H:SiOx coatings as a function of the precursor ratio and precursor type. Particular emphasis is placed on elucidating the transition from hard SiOx-doped carbon films to soft organosilicon matrices and on understanding how this transition affects the film properties.In this study, various materials with a smooth surface structure with a root mean square roughness below 0.3 nm were produced. Gradual increase in the precursor ratio induced significant structural changes, resulting in the transition from a-C:H:SiOx coatings with a remarkable hardness of ∼11 GPa to soft polymer-like matrices reaching hardness below 1 GPa. Hard a-C:H:SiOx coatings with excellent fracture resistance exhibiting a low friction coefficient in the range 0.08±0.01 can be achieved using both organosilicon compounds and precursor ratios 7.1-14.3 %. Under these conditions, HMDSO may be replaced with TMSAc to produce hard a-C:H:SiOx coatings with comparable mechanical properties.