Scandium-alloyed aluminum nitride (AlScN) is a potential material for micro-electromechanical systems because of its unique advantages, such as strong piezoelectric effect and high thermal stability. However, issues related to its stability and interaction with other materials in multilayer systems require investigation. The formation of new phases at the interface between piezomaterial and electrode material can lead to the device failure. In this study, multilayer structures Si substrate/AlN/Ti-Mo/Al 0.8 Sc 0.2 N/top electrode (TE) were studied after annealing at a wide range of temperatures and durations. Four different TE materials (i.e. Al, AlSi (1%), Mo/Al, and Mo) were examined to determine the most reliable electrode material for the structure. The phase stability, interfacial quality, and piezoelectric response of the multilayer systems after thermal annealing were investigated. The structure with Mo TE layer was stable after annealing at 800 °C for 300 h and at 1000 °C for 100 h. None of the structures formed any new phases at the interface between the electrode layer and AlScN. The transverse piezoelectric coefficient (e 31,f ) was determined for Al 0.8 Sc 0.2 N before and after annealing. The absolute value of the e 31,f was -1.39 C/m 2 for as-deposited structure and -1.67 C/m 2 for the same structure annealed for 300 h at 800 °C. [2020-0361]
It is more difficult to nucleate AlN-ScN alloy thin films (AlScN) in pure (0001)-texture than it is with pure AlN thin films. AlN thus can serve as seed layer for AlScN. Equipment limitations may lead to the problem of a vacuum break between AlN and AlScN deposition, as it leads to oxidation of the AlN surface. This issue was studied with high resolution TEM and electron diffraction. The formed oxide layer disturbed a lot the epitaxial growth, leading to additional grain orientations. A mild RF etching step introduced before AlScN deposition was able to remove the oxide layer, and allowed for growing Al 0.84 Sc 0.16 N in local epitaxy on AlN, as shown by Hyper map EDX images. The resulting AlScN films show a pure (0001) texture. Double beam laser interferometry and finite element modeling were used to determine d 33, f of both layers together as 6.6 pm/V, and of 6.85 pm/V for AlScN alone when using the standard value of 3.9 pm/V for pure AlN. At the same time, the relative dielectric constant of Al 0.84 Sc 0.16 N was determined as 14.1.