Hunan Engineering Technology Research Center in Special Titanium Alloys for High-end Equipment, Hunan Goldsky Titanium Industry Technology Co., Ltd., Changde 415001, China
Auto-generated profile, based on publicly available information
Chao Li
Hunan Engineering Technology Research Center in Special Titanium Alloys for High-end Equipment, Hunan Goldsky Titanium Industry Technology Co., Ltd., Changde 415001, China
The dynamic spheroidization mechanism and its orientation dependence in Ti-6Al-2Mo-2V-1Fe alloys during subtransus hot deformation were studied in this work. For this purpose, hot compression tests were carried out at temperatures of 780–880 °C, with strain rates of 0.001–0.1 s−1. Based on SEM, EBSD and TEM characterization, the results showed that the aspect ratio of the α phase decreased with increasing deformation temperatures and decreasing strain rates. At 880 °C/0.001 s−1, the aspect ratio of the α phase was the smallest at 2.05. The proportion of HAGBs decreased with increasing temperatures and strain rates, which was different from the trend of the spheroidization; this indicated that the formation of HAGBs was not necessary for the spheroidization process. Furthermore, the formation of the α/α interface was related to the evolution of dislocations and twin boundaries at high (880 °C) and low temperatures (780 °C), respectively. Moreover, the dependence of lamellar spheroidization on the crystallographic orientation tilt from the compression direction (θ) was clarified: when θ was between 45° and 60°, both the prism slip and basal slip systems were activated together, which was more favorable for spheroidization. This study could provide guidance for titanium alloy process designs and microstructure regulation.
The α variant selection and microstructure evolution in a new metastable β titanium alloy TB17 were studied in depth by DTA, microhardness, XRD, SEM, and EBSD characterization methods. Under the rapid cooling rate conditions (150 °C/min–400 °C/min), only a very small amount of granular αWM (α Widmanstatten precipitates within the grains) precipitated within the grains. The secondary α phase precipitated in the alloy changed from granular to fine needle-like at moderate cooling rates (15 °C/min–20 °C/min). When continuing to slow down the cooling rates (10 °C/min and 1 °C/min), the αGB (α precipitates along the β grain boundaries), αWGB (α Widmanstatten precipitates that developed from β grain boundaries or αGB) and αWM grew rapidly. Moreover, the continuous cooling transformation (CCT) diagram illustrated the effect of cooling rate on the β/α phase transition. EBSD analysis revealed that the variants selection of α near the original β grain boundary is mainly divided into three categories. (i) The double-BOR (Burgers orientation relationship) αWGB colonies within neighboring β grains grow in different directions but have the same crystallographic orientation. (ii) The double-BOR αWGB colonies within neighboring β grains have different growth directions and different crystallographic orientations. (iii) The double-BOR αWGB colonies within the same grain have the same growth direction, but different crystallographic directions. And these double-BOR αWGB colonies correspond to two variants of the given {0001}α//{110}β.