Adriana Peles-Tadic

Adriana Peles-Tadic

Auto-generated profile, based on publicly available information

Adriana Peles-Tadic

Institute of Technical Sciences of the Serbian Academy of Sciences and Arts, Belgrade, Serbia

Research Focus & Metrics

Academic Career Length

14Years (2013-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
24 August 2018 in Physica Scripta
Verified
Journal Article
Open access
PDF file
APAdriana Peles
Adriana Peles
OAObrad Aleksic
Obrad Aleksic
VPV P Pavlović
V P Pavlović
VDVladimir Djokovic
Vladimir Djokovic
RDRadovan Dojcilovic
Radovan Dojcilovic
VPV B Pavlović
V B Pavlović
The influence of the mechanical activation of ZnO nanoparticle fillers on the structural and electrical properties of the matrix of poly(vinylidenefluoride)–ZnO (PVDF–ZnO) films was investigated. Transmission electron microscopy and scanning electron microscopy analyses showed that mechanical activation in a high energy planetary ball mill reduces the size of ZnO particles. X-ray diffraction and Raman spectroscopy revealed that PVDF crystallized predominantly as the γ -phase. Non-activated ZnO filler reduces the degree of the crystallinity of the matrix and promotes crystallization of α -phase of PVDF in the film, while the fillers activated for 5 and 10 min induce crystallization of β -phase, indicating that mechanical activation of the filler can be used as a general method for fabrication of PVDF composites with increased content of piezoelectric β -phase crystals. Dielectric spectroscopy measurements show that polymer composite with the high content of β -phase (with ZnO filler activated for 5 min) exhibits the highest value of dielectric permittivity in 150–400 K range of temperatures. Kinetic analysis shows combined effects of increased surface area and increased concentration of surface defects on the interactions between polymer chains and activated nanoparticles.

1 November 2015 in Journal of Alloys and Compounds
Verified
Journal Article
Open access
APA. Peleš
A. Peleš
VPV.P. Pavlović
V.P. Pavlović
SFSuzana Filipović
Suzana Filipović
NONina Obradovic
Nina Obradovic
Lidija MancicLidija Mancic
Lidija Mancic
VPV.B. Pavlović
V.B. Pavlović

1 July 2014 in Microelectronic Engineering
Verified
Journal Article
Open access
ZDZoran Djurić
Zoran Djurić
IJIvana Jokić
Ivana Jokić
APAdriana Peleš
Adriana Peleš
In this study we have developed, for the first time, the comprehensive theoretical model of the fluctuations of the number of adsorbed molecules in MEMS chemical and biological sensors, taking into account the processes of mass transfer, adsorption and desorption, and surface diffusion of adsorbed molecules. It is observed that the shape of the fluctuations spectrum contains information about various parameters of the adsorbed analyte and that even the analytes with the same affinity for the same binding sites have different spectra. The numerical calculations performed using the derived theory show that the influence of surface diffusion on the fluctuations spectrum can be significant. The practical value of this work stems from the fact that the fluctuations of the number of adsorbed molecules can be a dominant noise component in affinity-based bio/chemical sensors. Therefore, the derived theory is useful for development of the methods for the detection of analytes based on frequency domain analysis of the measured fluctuations. The recognition of an adsorbed analyte using sensors with non-functionalized sensing surface will also be considered using the presented theory

1 January 2013 in Science of Sintering
Verified
Journal Article
Open access
PDF file
APA. Peles
A. Peles
NDN. Djordjevic
N. Djordjevic
NONina Obradovic
Nina Obradovic
NTN. Tadic
N. Tadic
VPVladimir Pavlovic
Vladimir Pavlovic
Mechanical activation is a commonly used and relatively fast and inexpensive procedure for sample preparation before the sintering process. Cordierite, a stoichiometric mixture of three different oxides (2MgO?2Al2O3?5SiO2) is a very attractive, widely used high-temperature ceramic material. The mechanical activation of the starting mixtures with 5.00 mass% TiO2 was performed in a high energy ball mill during 10-80 min. The applied compaction pressure before the sintering process was 2t/cm2, based on our recent investigation. The sintering process was performed at 1350oC for 2h and 4h in air atmosphere. X-ray diffraction was used to analyze the phase composition of non-activated and 80 min activated samples, sintered for 2 and 4h, respectively. Scanning electron microscopy was performed to analyze the microstructure of both compacted and sintered samples. Atomic force microscope was used to investigate the surface of the sintered samples. This paper investigates the influence of prolonged sintering time on the densities of the sintered samples, along with electrical properties.

1 January 2020 in Science of Sintering
Verified
Journal Article
Open access
PDF file
DKDarko Kosanović
Darko Kosanović
NLNebojša J. Labus
Nebojša J. Labus
JŽJelena Živojinović
Jelena Živojinović
APAdriana Peles-Tadic
Adriana Peles-Tadic
VBVladimir A. Blagojević
Vladimir A. Blagojević
VPVladimir B. Pavlović
Vladimir B. Pavlović
The influence of mechanical activation on the formation, sintering kinetics and morphology was investigated in sintered barium strontium titanate (BST) ceramics with different Ba-to-Sr ratios. Initial powders were mechanically activated for 20 and 120 min, leading to mechano-chemical reaction and formation of BaxSr1-xTiO3 phases. Agglomeration was found to represent an important factor in the process of formation of BaxSr1-xTiO3 phases around 800?C and during sintering. It reduces the effectiveness of mechanical activation on formation of BaxSr1-xTiO3 phases beyond the short period (20 min), while in the process of sintering, prolonged mechanical activation (120 min) leads to a significant reduction in sintering temperature and the corresponding value of activation energy. In addition, all three systems show a phase transformation around 1100?C, attributed to the hexagonal-to-cubic phase transition. Morphology of the final sintered ceramics can be correlated primarily with the state of the pre-sintered powder, where mechanically activated powders with smaller particle size produced more compact and less porous final product.

1 September 2014 in Ceramics International
Verified
Journal Article
Open access
DKDarko Kosanović
Darko Kosanović
JŽJelena Živojinović
Jelena Živojinović
NONina Obradovic
Nina Obradovic
VPV.P. Pavlović
V.P. Pavlović
VPV.B. Pavlović
V.B. Pavlović
MRM.M. Ristić
M.M. Ristić
Ferroelectric barium strontium titanate (Ba0.77Sr0.23TiO3), BST, was prepared by solid-state reactions using as the starting compounds powder of barium carbonate (BaCO3), strontium carbonate (SrCO3) and titanium dioxide (TiO2–anatase). Non-activated mixtures and mixtures mechanically activated in a high-energy planetary ball mill (0, 5, 10, 20, 40, 80 and 120 min) were sintered at 1100, 1200, 1300 and 1400 °C for 2 h in air atmosphere. Defects and the effect of the beginning of the sintering process on the microstructure were investigated by scanning electron microscopy (SEM). Electrical measurements (loss tangent and resistivity as the function of frequency XC=f(log ν)) were performed for ceramics sintered at 1400 °C for 2 h. It has been found that mechanical activation can reduce the sintering temperature by around 100 °C, which leads to significant energy savings. Furthermore, activated for 80 min and sintered at 1400 °C for 2 h exhibit the largest density values and have about 36% lower dielectric loss at a frequency of 1 kHz and about 57% at a frequency of 10 kHz than the samples obtained from the initial non-activated powder sintered under the same conditions