This work presents a complete analysis of Raman active modes of Sb 2 Se 3 measured by six different excitation wavelengths from NIR to UV, under different polarization configurations and at low temperature. Simultaneous fitting of spectra allowed the deconvolution and identification of the 28 Raman peaks obtained in monocrystalline Sb 2 Se 3 sample from the 30 modes predicted by the group theory analysis for this crystalline structure. Analysis of the spectra measured under different polarization configurations yielded the preliminary assignment of the peaks symmetry, while the measurements under low temperature resulted in a fine resolution of the peaks in Raman spectra. Additionally, evaluation of the spectra of the most probable secondary phases under different excitation wavelengths allowed to define the most appropriate measurement conditions for experimental discrimination of their Raman peaks in the spectra of Sb 2 Se 3 based thin films solar cells. The combination of different wavelength allows a non-destructive methodology for high sensitivity detection of main secondary phases of the Sb 2 Se 3 .
The efficiency of kesterite-based solar cells is limited by various non-ideal recombination paths, amongst others by a high density of defect states and by the presence of binary or ternary secondary phases within the absorber layer. Pronounced compositional variations and secondary phase segregation are indeed typical features of non-stoichiometric kesterite materials. Certainly kesterite-based thin film solar cells with an off-stoichiometric absorber layer composition, especially Cu-poor/Zn-rich, achieved the highest efficiencies, but deviations from the stoichiometric composition lead to the formation of intrinsic point defects (vacancies, anti-sites, and interstitials) in the kesterite-type material. In addition, a non-stoichiometric composition is usually associated with the formation of an undesirable side phase (secondary phases). Thus the correlation between off-stoichiometry and intrinsic point defects as well as the identification and quantification of secondary phases and compositional fluctuations in non-stoichiometric kesterite materials is of great importance for the understanding and rational design of solar cell devices. This paper summarizes the latest achievements in the investigation of identification and quantification of intrinsic point defects, compositional fluctuations, and secondary phases in non-stoichiometric kesterite-type materials.
A non-destructive Raman spectroscopy has been widely used as a complimentary method to X-ray diffraction characterization of Cu2ZnSnS4 (CZTS) thin films, yet our knowledge of the Raman active fundamental modes in this material is far from complete. Focusing on polarized Raman spectroscopy provides important information about the relationship between Raman modes and CZTS crystal structure. In this framework the zone–center optical phonons of CZTS, which is most usually examined in active layers of the CZTS based solar cells, are studied by polarized resonant and non-resonant Raman spectroscopy in the range from 60 to 500 cm−1 on an oriented single crystal. The phonon mode symmetry of 20 modes from the 27 possible vibrational modes of the kesterite structure is experimentally determined. From in-plane angular dependences of the phonon modes intensities Raman tensor elements are also derived. Whereas a strong intensity enhancement of the polar E and B symmetry modes is induced under resonance conditions, no mode intensity dependence on the incident and scattered light polarization configurations was found in these conditions. Finally, Lyddane-Sachs-Teller relations are applied to estimate the ratios of the static to high-frequency optic dielectric constants parallel and perpendicular to c-optical axis.
Polycrystalline kesterite Cu2ZnSnSe4 (CZTSe) semiconductors have drawn attention as promising absorber candidates for the next generation of thin film photovoltaics. However, the narrow tolerance to stoichiometry variations, which favours the formation of secondary phases and cluster defects, is a challenging drawback that restrains the device performance. In this context Raman spectroscopy has been demonstrated to be a powerful tool for the characterization of CZTSe, allowing the assessment of relevant parameters such as structure, crystal quality and secondary phases. In this work, multiwavelength Raman scattering measurements using nine excitation wavelengths (from 325 to 1064 nm) were performed on CZTSe polycrystalline thin films in order to give a detailed identification of all the active Raman modes expected in this crystalline structure. The experimental results compare well with the vibrational properties that have been computed by first-principles calculations based on density functional theory. Calculations of the phonon density of states (PDOS), as well as the simulation of the Raman spectra, have allowed a better understanding of the experimentally observed vibrational modes. A “non-band gap resonant” Raman effect was observed under 325 nm excitation conditions, making ultra-violet (UV) Raman spectroscopy a very promising characterization technique due to its high sensitivity to the surface region which provides information on the buffer/absorber interface. Strong intensity enhancement of spectral regions around 176 cm−1 and 250 cm−1 is observed. Calculated PDOS and combinatorial experiments on more than 200 samples with stoichiometries close to the high efficiency device compositions lead to the correlation of these intensities with the concentration of VCu and ZnSn point defects, respectively. Correlation with the optoelectronic properties of the devices allowed identification of the optimal concentration of VCu and ZnSn point defects for the highest performance devices. The application of the presented methodology has been confirmed by performing the same Raman analysis on the CZTSe absorber with 11% device efficiency. This work demonstrates that defect engineering in CZTSe is of the foremost importance for the improvement of solar cell performance, and that UV-based Raman spectroscopy is an effective technique for the non-destructive assessment of defects in kesterite materials.
24 December 2020 in Energy & Environmental Science
This work provides a detailed analysis of a high efficiency Cu2ZnSnSe4 device using a combination of advanced electron microscopy and spectroscopy techniques. In particular, a full picture of the different defects present at the interfaces of the device and in the bulk of the absorber is achieved through the combination of high resolution electron microscopy techniques with Raman, X-ray fluorescence and Auger spectroscopy measurements at the macro, micro and nano scales. The simultaneous investigation of the bulk and the interfaces allows assessing the impact of the defects found in each part of the device on its performance. Despite a good crystalline quality and homogeneous composition in the bulk, this work reports, for the first time, direct evidence of twinning defects in the bulk, of micro and nano-voids at the back interface and of grain-to-grain non-uniformities and dislocation defects at the front interface. These, together with other issues observed such as strong absorber thickness variations and a bilayer structure with small grains at the bottom, are shown to be the main factors limiting the performance of CZTSe devices. These results open the way to the identification of new solutions to further developing the kesterite technology and pushing it towards higher performances. Moreover, this study provides an example of how the advanced characterization of emergent multilayer-based devices can be employed to elucidate their main limitations.