(CBTi144) thin films were prepared by spin coating a precursor solution of metal alkoxides. As-deposited thin films began crystallization below and reached full crystallinity of a single phase of layered perovskite at via rapid thermal annealing in oxygen. The annealed CBTi144 thin film showed random orientation on Pt-passivated Si substrate and exhibited hysteresis loops. The remanent polarization and coercive electric field were and 106 kV/cm, respectively, at 11 V. The dielectric constant and loss factor were 300 and 0.033, respectively, at 100 kHz.
Polar-axis-oriented (CBTi144) films were fabricated on Pt foils using a complex metal alkoxide solution. The 500-nm-thick film showed the columnar structure and consisted of well-developed grains. The -axis orientation of the ferroelectric films is considered to be associated with the preferred orientation of Pt foil. The film showed good ferro- and piezoelectric properties. The and were 25 and 306 kV/cm, respectively, at an applied voltage of 115 V. The was characterized as 30 pm/V by piezoresponse force microscopy. The values were twice as large as those of the CBTi144 thin film with random orientation. The polar-axis-oriented CBTi144 films would open up possibilities for devices as Pb-free piezoelectric materials.
1 September 2005 in Japanese Journal of Applied Physics
Lead-free ferroelectric Ba(Ti1-xZrx)O3 (BTZ, x=0.00–0.50) thin films were fabricated on Pt(111)/Ti/SiO2/Si(100) substrates by the chemical solution deposition (CSD) process using complex alkoxide solutions. When the Zr content x was increased, the crystallinity of BTZ thin films was changed from the typical random orientation to the (111) preferred orientation. From the composition dependence of the dielectric constant εr and piezoelectric constant d33, the pinching region at room temperature of BTZ thin films consisting of nano-crystals appeared around x=0.20. For the BTZ thin film (x=0.20) fabricated using an alkoxide solution with partial hydrolysis, the grain and crystallite size were increased, and the εr and d33 were improved to 253 and 8.9 pm/V, respectively.
1 September 2004 in Japanese Journal of Applied Physics
Lead- and bismuth-free Ba(Ti1-xZrx)O3 (BTZ) thin films were fabricated on Pt(111)/Ti/SiO2/Si(100) substrates by the chemical solution deposition (CSD) process. The BaTiO3 and BTZ005 thin films fabricated by the conventional process were observed to have a remarkable difference in grain size along the depth of the thin film. The microstructure of the BaTiO3 and BTZ005 thin films was improved by additional sintering process, and their grain sizes were increased to about 60 and 40 nm, respectively, by additional sintering at 800°C for 1 h. The dielectric constant εr and piezoelectric constant d33 of the BaTiO3 thin film consisting of large grains by the additional sintering at 800°C for 1 h were found to be about 375 and 14.5 pm/V. But, εr and d33 of the BTZ005 thin film changed negligibly with increasing of the grain size.