Edwin Kee

Edwin Kee

Auto-generated profile, based on publicly available information

Edwin Kee

Division of Prosthodontics, LSU School of Dentistry, New Orleans, LA 70119, USA

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
28 February 2024 in Materials
Verified
Journal Article
Open access
PDF file
AAAkram Sayed Ahmed
Akram Sayed Ahmed
NLNathaniel Lawson
Nathaniel Lawson
CFChin-Chuan Fu
Chin-Chuan Fu
Pranit V BoraPranit V Bora
Pranit V Bora
EKEdwin Kee
Edwin Kee
ANAmir Hossein Nejat
Amir Hossein Nejat
Background: Determination of the eligibility of several tooth analog materials for use in crown fracture testing. Methods: A standardized premolar crown preparation was replicated into three types of resin dies (C&B, low modulus 3D printed resin; OnX, high modulus 3D printed resin composite; and highest modulus milled resin composite). 0.8 mm zirconia crowns were bonded to the dies and the maximum fracture load of the crowns was tested. Twelve extracted human premolars were prepared to a standardized crown preparation, and duplicate dies of the prepared teeth were 3D printed out of C&B. Zirconia crowns were bonded to both the dies and natural teeth, and their fracture load was tested. Results: There was no statistical difference between the fracture load of zirconia crowns bonded to standardized dies of C&B (1084.5 ± 134.2 N), OnX (1112.7 ± 109.8 N) or Lava Ultimate (1137.5 ± 88.7 N) (p = 0.580). There was no statistical difference between the fracture load of crowns bonded to dentin dies (1313 ± 240 N) and a 3D-printed resin die (C&B, 1156 ± 163 N) (p = 0.618). Conclusions: There was no difference in the static fracture load of zirconia crowns bonded to standardized resin dies with different moduli or between a low modulus resin die and natural dentin die.

1 January 2021 in Australasian Orthodontic Journal
Verified
Journal Article
Open access
PDF file
HKHannah Knott
Hannah Knott
XXXiaoming Xu
Xiaoming Xu
EKEdwin Kee
Edwin Kee
QYQingzhao Yu
Qingzhao Yu
PAPaul Armbruster
Paul Armbruster
RBRichard Ballard
Richard Ballard
Purpose: The objective of this study was to compare the shear bond strength (SBS) of ceramic orthodontic brackets bonded to highly translucent zirconia surfaces following the use of two different primers. Materials and methods:<Three types of highly translucent zirconia crowns, Cercon xt ML, e.max ZirCAD, and STML-ML Katana Zirconia, were milled, sandblasted, and primed using two zirconia primers, Monobond Etch and Prime and Z-Prime Plus. A ceramic bracket (Radiance) was bonded onto the facial surface of each crown. Shear bond strength was evaluated using a universal testing machine. Results: There was no significant overall difference across the six experimental groups regarding shear bond strength. The use of the two tested zirconia primers resulted in comparable and clinically acceptable shear bond strengths. Conclusions: Both tested zirconia primers were associated with adequate bond strength when bonding a ceramic orthodontic bracket to the three highly translucent zirconia substrates.