Akram Sayed Ahmed

Dr. Akram Sayed Ahmed

orcid

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
21 September 2020 in Oral Surgery
Verified
Journal Article
Open access
PDF file
Abanoub RiadAbanoub Riad
Abanoub Riad
AAAkram Sayed Ahmed
Akram Sayed Ahmed
BHBarbora Hockova
Barbora Hockova
Miloslav KlugarMiloslav Klugar
Miloslav Klugar
Click on the article title to read more.

28 February 2024 in Materials
Verified
Journal Article
Open access
PDF file
AAAkram Sayed Ahmed
Akram Sayed Ahmed
NLNathaniel Lawson
Nathaniel Lawson
CFChin-Chuan Fu
Chin-Chuan Fu
Pranit V BoraPranit V Bora
Pranit V Bora
EKEdwin Kee
Edwin Kee
ANAmir Hossein Nejat
Amir Hossein Nejat
Background: Determination of the eligibility of several tooth analog materials for use in crown fracture testing. Methods: A standardized premolar crown preparation was replicated into three types of resin dies (C&B, low modulus 3D printed resin; OnX, high modulus 3D printed resin composite; and highest modulus milled resin composite). 0.8 mm zirconia crowns were bonded to the dies and the maximum fracture load of the crowns was tested. Twelve extracted human premolars were prepared to a standardized crown preparation, and duplicate dies of the prepared teeth were 3D printed out of C&B. Zirconia crowns were bonded to both the dies and natural teeth, and their fracture load was tested. Results: There was no statistical difference between the fracture load of zirconia crowns bonded to standardized dies of C&B (1084.5 ± 134.2 N), OnX (1112.7 ± 109.8 N) or Lava Ultimate (1137.5 ± 88.7 N) (p = 0.580). There was no statistical difference between the fracture load of crowns bonded to dentin dies (1313 ± 240 N) and a 3D-printed resin die (C&B, 1156 ± 163 N) (p = 0.618). Conclusions: There was no difference in the static fracture load of zirconia crowns bonded to standardized resin dies with different moduli or between a low modulus resin die and natural dentin die.

1 August 2023 in Journal of Prosthodontics
Verified
Journal Article
Open access
Carlos Alberto JuradoCarlos Alberto Jurado
Carlos Alberto Jurado
AAAkram Sayed Ahmed
Akram Sayed Ahmed
NLNathaniel Lawson
Nathaniel Lawson
Francisco X. Azpiazu-FloresFrancisco X. Azpiazu-Flores
Francisco X. Azpiazu-Flores
CGConley Green
Conley Green
SCSeok‐Hwan Cho
Seok‐Hwan Cho
Purpose: To determine the fracture resistance of chairside computer‐aided design and computer‐aided manufacturing (CAD‐CAM) zirconia surveyed crowns for a mandibular first molar without occlusal rest and with four different rest seat designs.Materials and Methods: Seventy CAD‐CAM zirconia 4Y‐PSZ (IPS e.max ZirCAD MT for CEREC A1, C15, Ivoclar Vivadent) crowns (14 specimens/group) were designed and fabricated with a dental chairside CAD‐CAM system (CEREC PrimeScan, and CEREC MCXL Dentsply Sirona). The restorations were divided into groups according to the following rest seat designs: (1) Surveyed crown without rest seat, (2) surveyed crowns with disto‐occlusal rest seat, (3) surveyed crowns with disto‐occlusal extended rest seat, (4) surveyed crowns with interproximal rest seat, and (5) continuous rest seat. Crowns were treated with a primer system (Monobond Plus, Ivoclar Vivadent) and cemented using resin luting cement (Multilink Automix, Ivoclar Vivadent) to resin‐printed dies (Grey Resin V4, FormLabs). Subsequently, the crowns were subjected to 200,000 load cycles at 1 Hz with 20 N force and then loaded with a steel indenter until fracture. The test results were analyzed with one‐way Analysis of Variance (ANOVA) and HSD Tukey post‐Hoc test.Results: The mean fracture resistance of surveyed crowns without and with different rest seats was significantly different from each other. Surveyed crowns with no rest seat displayed the highest resistance (4238 N) followed by crowns with continuous rest seat (3601 N), crowns with disto‐occlusal extended rest seat (3283 N), and crowns with disto‐occlusal rest seat (3257 N). Crowns with interproximal rest seat displayed the lowest fracture resistance (2723 N).Conclusions: Surveyed crowns without rest seats had a higher fracture resistance than crowns with rest seats Surveyed crowns with interproximal rest seats presented the lowest fracture resistance among all rest seat designs. Crowns with disto‐occlusal rest seats, disto‐occlusal extended rest seats, and continuous rest seats displayed similar fracture resistance.

11 January 2024 in Materials
Verified
Journal Article
Open access
PDF file
PCPo-Hsu Chen
Po-Hsu Chen
EEEsra Elamin
Esra Elamin
AAAkram Sayed Ahmed
Akram Sayed Ahmed
DGDaniel A. Givan
Daniel A. Givan
CFChin-Chuan Fu
Chin-Chuan Fu
NLNathaniel Lawson
Nathaniel Lawson
Background: To determine what thickness of 5 mol% yttria zirconia (5Y-Z) translucent crowns cemented with different cements and surface treatments would have equivalent fracture resistance as 3 mol% yttria (3Y-Z) crowns. Methods: The study included 0.8 mm, 1.0 mm, and 1.2 mm thickness 5Y-Z (Katana UTML) crowns and 0.5 and 1.0 mm thickness 3Y-Z (Katana HT) crowns as controls. The 5Y-Z crowns were divided among three treatment subgroups (n = 10/subgroup): (1) cemented using RMGIC (Rely X Luting Cement), (2) alumina particle-abraded then luted with the same cement, (3) alumina particle-abraded and cemented using a resin cement (Panavia SA Cement Universal). The 3Y-Z controls were alumina particle-abraded then cemented with RMGIC. The specimens were then loaded in compression at 30° until failure. Results: All 5Y-Z crowns (regardless of thickness or surface treatment) had a similar to or higher fracture force than the 0.5 mm 3Y-Z crowns. Only the 1.2 mm 5Y-Z crowns with resin cement showed significantly similar fracture force to the 1 mm 3Y-Z crowns. Conclusion: In order to achieve a similar fracture resistance to 0.5 mm 3Y-Z crowns cemented with RMGIC, 5Y-Z crowns may be as thin as 0.8 mm. To achieve a similar fracture resistance to 1.0 mm 3Y-Z crowns cemented with RMGIC, 5Y-Z crowns must be 1.2 mm and bonded with resin cement.

14 August 2020 in British Dental Journal
Verified
Journal Article
Closed access
PDF file
Abanoub RiadAbanoub Riad
Abanoub Riad
AAAkram Sayed Ahmed
Akram Sayed Ahmed
Michela BoccuzziMichela Boccuzzi
Michela Boccuzzi
SCS. Cosola
S. Cosola