The formation of a columnar grain structure in high chromium nickel based alloy welds can be associated with cracking and poor resolution for ultrasonic non-destructive examination. The objective of this research was to characterise the effects of circular magnetic arc deflection (arc stirring) on grain structure of gas tungsten arc weld overlays made on Inconel 690 substrates with 52M filler wire. Welds and weld overlays were made at various arc stirring frequencies, and microstructures were analysed using optical and electron backscattered diffraction microscopy. Significant refinement of grain size occurred at a stirring frequency of 7 Hz. Ultrasonic non-destructive examination confirmed 100% improvement in signal/noise ratio in weld overlays made with magnetic stirring.
1 October 2010 in Science and Technology of Welding and Joining
The objectives of this work were to characterise and understand the effects of circular magnetic arc deflection (arc stirring) on grain structure refinement of gas tungsten arc weld beads made in Inconel 690 substrates. Welds were made at various arc stirring frequencies (1·5–50 Hz), and microstructures were analysed using optical and electron backscattered diffraction microscopy. Optimum refinement of grain size occurred at a stirring frequency of ∼7 Hz. Analysis of computational fluid flow, heat transfer and solidification model results suggested that grain detachment was the primary mechanism for grain refinement.
30 November 2007 in Journal of Physics D: Applied Physics