Functionally graded ceramic systems consisted of Al2O3/(Al2O3–ZrO2) and Al2O3/(Al2O3–Nd2Ti2O7) have been produced by gel casting. In Al2O3/ZrO2 systems, Al2O3 was gathered with three different Al2O3/ZrO2 mixtures with varying ZrO2 contents. For Al2O3/Nd2Ti2O7 system, Al2O3 layer was combined with 3 mol% Nd2Ti2O7‐doped Al2O3. All samples sintered at 1480 and 1540°C showed strong adhesion between layers without any crack formation. In the Al2O3/ZrO2 systems, both layers were intact; a distinct separation was observed, whereas a large reaction zone was observed for the Al2O3/Nd2Ti2O7 system as a consequence of reaction between both phases. The separation between layers for both systems was identified by SEM–EDX analyses. The hardness and wear tests of the samples showed that functional grading approach ensures combining various physical properties in a monolithic body.
1 January 2018 in Processing and Application of Ceramics
Al2O3/Ni and Al2O3/Co nanopowder mixtures (with 3 vol.% of metallic phase) were synthesized by heterogeneous precipitation method. In order to increase the green strength, polypropylene carbonate (PPC) was used as a binder while preparing green compacts. Uniaxially pressed powder mixtures were sintered at 1550°C for 2 h in a reducing atmosphere. The effects of Ni and Co nanophases on the microstructure and mechanical properties of Al2O3 ceramics were studied by X-ray diffraction, scanning electron microscopy, Vickers indentation technique and three-point bending tests. The metallic phase hindered the densification of alumina matrix, yet hardness values of Al2O3, Al2O3/Ni, and Al2O3/Co composites were comparable. Vickers fracture toughness results indicate that the composites have higher fracture toughness, but the characteristic flexural strength and Weibull modulus are higher for the pure Al2O3.
15 December 2023 in Karadeniz Fen Bilimleri Dergisi
The effects of low amounts (0, 0.1, 0.3, 0.5, 0.8, 1, 2vol%) of Sm2O3 on the densification, microstructure, and bending strength of Al2O3 were studied for different sintering temperatures. Sm2O3 and Al2O3 powders were mixed by ball milling, and Al2O3-Sm2O3 ceramics were prepared by dry and cold isostatic pressing in disc form before pressureless sintering at 1550°C and 1600°C/2 h in the air, separately. Sm2O3 reacted with Al2O3 by forming SmAlO3. The rod-like morphology of the SmAlO3 was generally achieved for 0.8 and 1vol% Sm2O3 for sintering at 1600°C, whereas the rod-like form was more obvious for the samples sintered at 1550°C. Similar relative densities were attained for all Sm2O3 ratios at both sintering temperatures, but the Al2O3 sintered at 1550°C exhibited higher densification than the Al2O3 sintered at 1600°C. The strength values were close, while a strength increase of about 5% was obtained for 0.5 vol% Sm2O3 containing ceramics sintered at 1600°C caused by the higher densification compared to the Al2O3. The strength showed a prominent drop above the ratio of 0.1 vol% Sm2O3 for sintering at 1550°C. The addition of present amounts of Sm2O3 did not have a significant effect on the mechanical properties of Al2O3 but it changed the microstructure.