In this work, we report the successful growth of high-quality SiO2 films by low-temperature plasma-enhanced atomic layer deposition using an oxidant which is compatible with moisture/oxygen sensitive materials. The SiO2 films were grown at 90 °C using CO2 and Bis(tertiary-butylamino)silane as process precursors. Growth, chemical composition, density, optical properties, and residual stress of SiO2 films were investigated. SiO2 films having a saturated growth-per-cycle of ~ 1.15 Å/cycle showed a density of ~ 2.1 g/cm3, a refractive index of ~ 1.46 at a wavelength of 632 nm, and a low tensile residual stress of ~ 30 MPa. Furthermore, the films showed low impurity levels with bulk concentrations of ~ 2.4 and ~ 0.17 at. % for hydrogen and nitrogen, respectively, whereas the carbon content was found to be below the measurement limit of time-of-flight elastic recoil detection analysis. These results demonstrate that CO2 is a promising oxidizing precursor for moisture/oxygen sensitive materials related plasma-enhanced atomic layer deposition processes.
Structural and photoluminescence studies were carried out on Eu-doped Y2O3−xSx thin films grown by atomic layer deposition at 300 °C. (CH3Cp)3Y, H2O, and H2S were used as yttrium, oxygen, and sulfur precursors, respectively, while Eu(thd)3 was used as the europium precursor. The Eu oxidation state was controlled during the growth process by following the Eu(thd)3 pulse with either a H2S or O3 pulse. The Eu(thd)3/O3 pulse sequence led to photoluminescence emission above 550 nm, whereas the Eu(thd)3/H2S pulse sequence resulted in emission below 500 nm.