In this letter, self-aligned top-gate (SATG) amorphous In-Ga-Zn-O (a-IGZO) thin-film transistors (TFTs) with an 8.62-nm SiO 2 gate dielectric grown by conventional plasma enhanced chemical vapor deposition (PECVD) at 300 °C are fabricated. The results show that the ultrathin PECVD SiO 2 film has excellent dielectric properties, such as a low leakage current density of 10 −8 A/cm 2 at 2 MV/cm, a high breakdown electric field of 9.3 MV/cm, and an almost independent capacitance of bias frequency. The fabricated SATG a-IGZO TFTs with the ultrathin SiO 2 gate dielectric exhibit high electrical performances, with major parameters, including a low gate leakage current of 10 −13 A, a small subthreshold swing value of 124 mV/decade, a decent field-effect mobility of 10.13 cm 2 / $\text{V}\cdot \text{s}$ , and a high ON/OFF current ratio up to 10 8 . Furthermore, the TFTs also show a good electrical stability under positive and negative gate bias stresses.
5 March 2020 in IEEE Transactions on Electron Devices
Magnesium (Mg)-induced metallization of amorphous indium-gallium-zinc-oxide (a-IGZO) films is investigated to develop a self-aligned (SA) top-gate (SATG) a-IGZO thin-film transistor (TFT) technology. The high-conductive and SA a-IGZO source/drain (S/D) regions are well realized by a short time of sputtered deposition of Mg onto the a-IGZO film on a heated substrate, followed by the removal of the spare Mg on the surface in hot water. It is shown that the resistivity of the a-IGZO films is lowered to about 4 x 10⁻³ Ω cm from over 10⁴ Ω cm with a 36-s Mg deposition at 300°C. The metallization effect is believed to be the consequence of a large number of donor-like defects (oxygen vacancies) generated by oxidation-reduction reaction at the interface between the Mg and a-IGZO films. The SATG a-IGZO TFTs fabricated by the proposed technology show excellent electrical characteristics, such as a field-effect mobility of 19.5 cm²V⁻¹s⁻¹, a subthreshold swing of 0.19 V/dec, an on-/off-current ratio of over 10⁹, a low S/D series resistance of 2.1 Ω cm, a small channel length shrinking of around 0.1 μm, and a high stability against electrical stresses.
18 April 2022 in IEEE Journal of the Electron Devices Society
The environmental stability of self-aligned top-gate (SATG) a-InGaZnO thin-film transistor (TFT) was studied by performing the high-temperature high-humidity (HTHH) test. Despite the maintenance of initial electrical characteristics, the stability under positive bias stress (PBS) was considerably deteriorated, including an abnormal negative ${V} _{\mathrm{ th}}$ shift ( $\boldsymbol{\Delta } {V} _{\mathrm{ th}}$ ), increased off current, and degraded SS . Moreover, the negative ${\Delta } {V} _{\mathrm{ th}}$ was consistently enhanced with the channel length ( ${L}$ ) decreasing. Such ${L}$ dependence was clarified to originate from the lateral diffusion of H 2 O in TG insulator during HTHH tests, and the PBS instabilities were caused by the ionization and migration of H 2 O molecules into the a-IGZO channel, as verified by the X-ray photoelectron spectroscopy, C-V characteristics, and recovery behaviors of PBS degradation.