Electrical characteristics of self-aligned top-gate (SATG) amorphous InGaZnO (a-IGZO) thin-film transistors (TFTs) with 4 nm-thick atomic-layer-deposited (ALD) AlO x gate insulator (GI) are investigated. It is demonstrated that the SATG a-IGZO TFTs present high-performance metrics including a near-ideal subthreshold swing ( SS ) of 60.9 mV/dec, a low off-state current below 10 −12 A, a positive ${V}_{\text{th}}$ of 0.1 V, and a decent mobility of 14.1 cm 2 / $\text{V}\,\cdot $ s. In addition, the TFTs exhibit negligible ${V}_{\text{th}}$ shifts less than 0.02 V against electrical bias stresses. Both high performance and excellent stability are thus simultaneously achieved for the ultrathin GI of amorphous oxide semiconductor (AOS) TFTs.
We herein demonstrate a self-aligned top-gate (SATG) coplanar amorphous InGaZnO (a-IGZO) thin-film transistor (TFT) technology, with the gate length ( ${L}_{\text {g}}$ ) down-scaled to 97 nm, and gate insulator (GI) AlOx to 4 nm (equivalent oxide thickness = 2.4 nm). The fabricated TFT exhibits a large on-current ( ${I} _{\text {ON}}$ ) of $17.9~\mu \text{A}/\mu \text{m}$ , a high on/off current ratio over 109, a positive threshold voltage ( ${V} _{\text {TH}}$ ) of 0.07 V, and a minimum drain-induced barrier lowering (DIBL) of 77 mV/V. The well-maintained performances of the TFTs even in the nanoscale regime can be ascribed to the abrupt homojunction at source-drain sides and high-quality of ultrathin gate insulator of AlOx by atomic layer deposition (ALD). With the excellent scaling metrics and compatibility with modern integrated circuit (IC) process, the developed SATG a-IGZO TFT technology is compatible with the back-end-of-line(BEOL) and 3D integrations of advanced ICs.
18 April 2022 in IEEE Journal of the Electron Devices Society
The environmental stability of self-aligned top-gate (SATG) a-InGaZnO thin-film transistor (TFT) was studied by performing the high-temperature high-humidity (HTHH) test. Despite the maintenance of initial electrical characteristics, the stability under positive bias stress (PBS) was considerably deteriorated, including an abnormal negative ${V} _{\mathrm{ th}}$ shift ( $\boldsymbol{\Delta } {V} _{\mathrm{ th}}$ ), increased off current, and degraded SS . Moreover, the negative ${\Delta } {V} _{\mathrm{ th}}$ was consistently enhanced with the channel length ( ${L}$ ) decreasing. Such ${L}$ dependence was clarified to originate from the lateral diffusion of H 2 O in TG insulator during HTHH tests, and the PBS instabilities were caused by the ionization and migration of H 2 O molecules into the a-IGZO channel, as verified by the X-ray photoelectron spectroscopy, C-V characteristics, and recovery behaviors of PBS degradation.
The capacitor–less embedded dynamic random access memory (eDRAM) based on oxide semiconductor (OS) transistors exhibits a promising future and thus has lead to a growing demand for nanoscale OS thin–film transistors (TFTs). In this work, a self–aligned top–gate (SATG) amorphous InGaZnO (a‐IGZO) TFT is demonstrated by using the simplest 3‐masks (3M) process, and the downscaling‐related issues are carefully addressed to strengthen its back–end–of–line (BEOL) compatibility and mass producibility. The gate insulator (GI) and associated interface defects of the TFTs are jointly optimized with 4–nm atomic‐layer‐deposited (ALD) AlOx on the pre‐oxidized a‐IGZO. The defects in a‐IGZO channel are further manipulated with a rapid thermal anneal (RTA) in oxygen. By virtue of the strengthened gate controllability and modified channel properties, the fabricated TFT with 97‐nm gate length (Lg) exhibits decent performance, such as a maximum on–state current (ION) of 32.4 µA µm−1, as well as clear linear and saturation characteristics. Based on such 3M SATG a‐IGZO TFTs with high device performance and inherently minimal parasitic capacitances, the developed capacitor‐less eDRAM bit cell achieves a wide sensing margin and a long retention time of over 500 s. A highly manufacturable oxide TFT technology for high–performance and high–density monolithic–3D (M3D) integration is thus well established.
A deep sub-micron self-aligned bottom-gate (SABG) amorphous InGaZnO (a-IGZO) thin-film transistor (TFT) technology was developed. The implementation of a backside exposure technique enables the realization of a self-aligned structure, while an argon (Ar) plasma treatment minimizes the source/drain resistance ( R SD ). High-performance metrics were well maintained on the fabricated SABG a-IGZO TFT with a channel length of 302 nm (effective channel length of 208 nm), including a low off-state current around 10 -14 A/μm, a subthreshold swing of 103.8 mV/dec, a decent mobility of 7.48 cm 2 /V∙s, a minor drain-induced barrier lowering (DIBL) of 41.5 mV/V, a negligible channel length shrinking (Δ L ) of 47 nm and a record-low R SD of 0.86 Ω∙cm among self-aligned (SA) transistors. Such remarkable scalability and manufacturing capability pave a new cost-effective way for high integration-density oxide electronics.