To investigate the permeability of deep dentin following immediate sealing with different etch-and-rinse and self-etch adhesives (Single Bond 2, Adper Prompt L-Pop, Clearfil Protect Bond, Clearfil S3 Bond, G-Bond) and a dentin desensitizer (Gluma). Fluid-transport model was used to measure fluid conductance during and after application of adhesives. Polyvinylsiloxane impressions of bonded dentin were taken to monitor fluid transudation from the surface of the adhesives. The area and number of dentinal fluid droplets and/or blisters were calculated using image analysis. None of the adhesives were able to block fluid conductance completely. The fluid conductance values of the adhesives displayed the following statistical ranking (p<0.05): G-Bond≤Clearfil Protect Bond<Smear-layer-covered dentin<S3 Bond≤Single Bond 2≤Adper Prompt L-Pop<Gluma Desensitizer<Acid-etched dentin. Highly significant correlation was observed between the permeability of the tested adhesives and the area fraction of fluid droplets/blisters on the adhesive surfaces (r=0.99, p<0.01).
Objectives: This study aims to evaluate the effect of built layer thickness (BLT) on the surface roughness, color stability, and microbial adhesion of 3D-printed interim restorations, comparing them with conventional and milled resin materials. Materials and Methods: Disk-shaped samples (2 mm thickness, 10 mm diameter) were fabricated using three different manufacturing methods: conventional, 3D printing, and milling. The 3D-printed samples were produced using a Digital Light Processing (DLP) printer with BLTs of 30 μm, 50 μm, and 70 μm. Surface roughness was measured using confocal microscopy. Color stability was assessed after immersion in artificial saliva, coffee, and red wine for 14 days, with color differences determined using a dental spectrophotometer. Microbial adhesion was evaluated using bacterial and fungal strains, and adherence levels were classified. Results: Statistical analysis showed that BLT significantly influenced surface roughness, with 30 μm BLT exhibiting the smoothest surfaces. The highest discoloration was observed in the 70 μm BLT group, while the least discoloration was in the milling group. Microbial adhesion was higher on milled samples compared to 3D-printed materials and conventional acrylic resin. Conclusion: BLT significantly affects the surface properties of 3D-printed interim restorations. A 30 μm BLT provided the best surface characteristics with lower roughness and reduced discoloration. However, the monomer content of 3D printing resins remains unclear, necessitating further investigation. More comprehensive studies are required to optimize 3D-printed dental materials.