In this study, TiAlZrN films were coated on the hardened 1.2344 (X 40 CrMoV 5 1) steels using DC power supplied closed field unbalanced magnetron sputtering (CFUBMS) technique. Structural investigations of coatings were carried out using scanning electron microscope and X-ray diffraction. The thickness of coatings was measured from the cross-sectional scanning electron microscope images, and the grain size value and residual stress were calculated by using X-ray diffraction data in the Scherrer formula. Nano indentation method was used to investigate the surface hardness for reducing the substrate effect due to very thin coating thickness (∼2–3 µm). Scratch test was performed for determining the adhesion strength of the coatings. As a tribo-test, a ball-on-disk system was used. From the results, it was understood why TiAlZrN coatings were attractive. The highest hardness was observed as 50.67 GPa, and the highest scratch resistance was reached to 56 N. Also, it was determined that the coating having the highest tribological properties (5.46 × 10−5 mm3/Nm) increased the wear resistance of the substrate six times (3.06 × 10−4 mm3/Nm).
4 January 2021 in Journal of Materials Engineering and Performance
It is known that the interest in manufacturing in a vacuum environment has increased in recent years. Thus, the wear behavior of mechanical tools under vacuum conditions has critical importance. However, adhesion and cold-welding problems between tool and working piece in vacuum conditions lead to poor wear properties and severe coefficient of friction values. Surface treatment methods such as physical vapor deposition coatings can eliminate these undesirable consequences, especially transition metal nitrides. In this study, TiAlN, TiSiN, and TiAlN/TiSiN films were coated on AISI H13 tool steels employing the cathodic arc evaporation technique. Whether the coatings grown to the substrate surface have a positive contribution to the wear performance of the substrate in the ambient air and vacuum environment was answered. Scanning electron microscope, energy dispersive spectrometer, and X-ray diffractometer analyses were used to attain structural properties. The hardness was measured using a nano-hardness tester, and the adhesion properties were determined by a scratch test. The wear behavior of the substrate and coating samples are determined under 2 N constant normal load and using WC-6%Co counter bodies under ambient air and vacuum conditions. The hardness of samples improved owing to surface coatings, and the highest nano-hardness value was determined from the TiSiN coatings as 39.42 GPa, which is ∼700% greater than the substrate. It has been observed that coated samples have superior wear performance in both wear conditions. Besides, it is determined that those tested under a vacuum condition showed superior wear resistance than the samples tested under ambient air. While TiSiN film exhibits the highest wear resistance in ambient air, the TiAlN/TiSiN layer is the best in a vacuum environment. Owing to the deposited coatings, the seizure mechanism between the friction surfaces, which is frequently encountered in the vacuum environment, is prevented, and a fascinating improvement in terms of friction coefficient is achieved.
8 November 2022 in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
Recently, AZ31B magnesium alloy has been widely employed in automotive, aerospace, and bio implant industries due to its light-weight and biocompatibility properties. However, the equilibrium of ductility and strength of this material and the negativity brought by its poor wear behavior have limited its versatile use. Friction stir processing (FSP) has been commonly used as severe plastic deformation method for improving mechanical and tribological properties of metal sheets. The effect of this method on the biocompatibility of materials is a matter of curiosity that should be emphasized. So, the present study aims to investigate the effect of friction stir process on the mechanical, tribological, and biocompatibility properties of AZ31B magnesium alloy. It is observed that FSP enhanced the tensile properties of the alloy but decreased its elongation. It was determined that the base material exhibited ductile character on the fracture surface of the specimens, and mixed ductile/brittle fracture was evident with the FSP. In the FSP zone, the hardness value was improved by 17% compared to the base material. Also, the wear performance of the alloy enhanced in ambient air and Simulated Body Fluid (SBF) solution. Wear properties in SBF solution were better due to less adhesive bonds between the friction surfaces. This assessment was supported by SEM images of the wear path and surface of counter bodies. On the other hand, FSPed AZ31B alloy materials with improved strength properties were not cytotoxic for human gingival fibroblasts, and these results may suggest that the materials are safe for clinical uses.
18 October 2021 in Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications
In the present study, CrN, CrAlN and CrAlTiN coatings were deposited using the cathodic arc evaporation technique. The structural investigations of these CrN based coatings were performed by scanning electron microscopy, energy dispersive spectroscopy, atomic force microscopy, X-ray diffractometer. The hardness and adhesion strength values of coatings were determined via Vickers type microhardness tester and progressive load scratch tester, respectively. The wear performance of samples was established at ambient air and vacuum condition. All coatings grew in the “T zone” growth model and had a dense and columnar structure. The XRD patterns presented predominantly (220), (110), and (111) reflections. It was demonstrated that the quaternary coating had a higher texture parameter as 0.68, which was related to the highest thickness and hardness. Also, CrAlTiN coatings with the smallest mean crystallite size of ∼87 nm showed the best hardness, and this ensured relatively high scratch resistance. CrN and CrAlTiN coatings improved wear performance under ambient air condition but were not striking as under vacuum condition. The quaternary coating had a superior performance in the vacuum condition, but due to the high sensitivity of Ti to oxygen, it fell behind the CrN coating under ambient air condition.