Zhangjing Chen

Zhangjing Chen

Auto-generated profile, based on publicly available information

Zhangjing Chen

Department of Sustainable Biomaterials, Virginia Polytechnic Institute and State University, Blacksburg, VA 24060, USA

Research Focus & Metrics

Academic Career Length

24Years (2003-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
5 April 2016 in Wood Science and Technology
Verified
Journal Article
Closed access
PDF file
ZGZhiqiang Gao
Zhiqiang Gao
RHRongfeng Huang
Rongfeng Huang
JLJianxiong Lu
Jianxiong Lu
ZCZhangjing Chen
Zhangjing Chen
FGFei Guo
Fei Guo
TZTianyi Zhan
Tianyi Zhan

XZXiaotao Zhang
Xiaotao Zhang
XWXiming Wang
Ximing Wang
ZCZhangjing Chen
Zhangjing Chen
A lignocellulose/montmorillonite (LMT) nanocomposite was prepared as a reusable adsorbent for cobalt(II) ions, and characterized by nitrogen (N2) adsorption/desorption isotherm, X-ray Diffraction (XRD), Scanning Electron Microscope (SEM), Transmission Electron Microscopy (TEM), and Fourier Transform Infrared Spectroscopy (FTIR). LMT exhibited efficient adsorption of cobalt ions (Co(II)), and the adsorbed Co(II) was readily desorbed by nitric acid (HNO3). All parameters affecting the adsorption and/or desorption of Co(II), including initial Co(II) concentration, pH value, temperature, HNO3 concentration, and time, were optimized. The kinetic data analysis showed that the adsorption followed the pseudo-second-order kinetic model and fit well into the Langmuir isotherm equation. Notably, the nanocomposite can be used four times without significantly losing adsorbent capability. The Energy-Dispersive X-ray (EDX) and FTIR spectra analysis also revealed that the adsorption mechanism may be mainly a chemical adsorption dominated process.

28 August 2017 in Materials
Verified
Journal Article
Open access
PDF file
XZXiaotao Zhang
Xiaotao Zhang
YHYinan Hao
Yinan Hao
XWXiming Wang
Ximing Wang
ZCZhangjing Chen
Zhangjing Chen
A low-cost activated carbon (XSBLAC) prepared from Xanthoceras Sorbifolia Bunge hull via chemical activation was investigated to determine its adsorption and desorption properties for zinc(II) ions from aqueous solutions. XSBLAC was characterized based on its N2-adsorption/desorption isotherm, EDX, XRD, SEM and FTIR results. An adsorption study was conducted in a series of experiments to optimize the process variables for zinc(II) removal using XSBLAC. Modeling the adsorption kinetics indicated good agreement between the experimental data and the pseudo-second-order kinetic model. The Langmuir equilibrium isotherm fit the experimental data reasonably well. The calculated enthalpy (ΔH0), entropy (ΔS0) and Gibbs free energy (ΔG0) values revealed the endothermic and spontaneous nature of the adsorption process. HNO3 displayed the best desorption performance. The adsorption mechanism was investigated in detail through FTIR and SEM/EDX spectroscopic analyses. The results suggested that XSBLAC is a potential biosorbent for removing zinc(II) from aqueous solutions.

22 September 2017 in Materials
Verified
Journal Article
Open access
PDF file
XZXiaotao Zhang
Xiaotao Zhang
XWXiming Wang
Ximing Wang
ZCZhangjing Chen
Zhangjing Chen
A sulfhydryl-lignocellulose/montmorillonite (SLT) nanocomposite was prepared using a chemical intercalation reaction. The SLT nanocomposite was characterized by Fourier Transform Infrared Spectroscopy (FTIR), X-Ray Diffraction (XRD), Scanning Electron Microscope (SEM), and Transmission Electron Microscopy (TEM), the results demonstrated that an intercalated-exfoliated nanostructure was formed in the SLT nanocomposite. Batch experiments were conducted to optimize parameters such as SLT nanocomposite dosage, the initial concentration of Ni(II), solution pH, temperature, and time. The results indicated that the attractive adsorption capacity reached 1134.08 mg/g with 0.05 g of SLT at an initial concentration of Ni(II) of 700 mg/L, solution pH of 5.5, adsorption temperature of 50 °C, and adsorption time of 40 min, meanwhile, the Ni(II) adsorption capacity significantly decreased with the increase in ionic strength. The pseudo-second order kinetic model could describe the whole adsorption process well, and the isotherm adsorption equilibrium conformed to the Freundlich model. The adsorption mechanism of SLT was also discussed by means of FTIR and Energy-Dispersive X-Ray (EDX). Dramatically, the introduction of sulfhydryl achieves the increased activated functional groups content of SLT nanocomposite, leading to remarkably higher adsorption amount on Ni(II). The desorption capacity of SLT was dependent on parameters such as HNO3 concentration, desorption temperature, and ultrasonic desorption time. The satisfactory desorption capacity and desorption efficiency of 458.21 mg/g and 40.40% were obtained at an HNO3 concentration, desorption temperature, and ultrasonic desorption time of 0.4 mol/L, 40 °C, and 30 min, respectively. The regeneration studies showed that the adsorption capacity of SLT was consistent for four cycles without any appreciable loss and confirmed that the SLT was reusable. Owing to such outstanding features, the novel SLT nanocomposite proved the great potential in adsorption for Ni(II) removal from aqueous solution, and exhibited an extremely significant amount of Ni(II), compared to pristine lignocellulose/montmorillonite and the conventional spent adsorbents.

4 January 2022 in Forests
Verified
Journal Article
Open access
PDF file
YZYuan Zhong
Yuan Zhong
YAYuhong An
Yuhong An
KWKebing Wang
Kebing Wang
WZWanqi Zhang
Wanqi Zhang
ZHZichu Hu
Zichu Hu
XWXiming Wang
Ximing Wang
Heavy metal wastewater treatment is a huge problem facing human beings, and the application degree of Salix psammophila resources produced by flat stubble is low. Therefore, it is very important to develop high-value products of Salix psammophila resources and apply them in the removal heavy metal from effluent. In this work, we extracted the cellulose from Salix psammophila, and cellulose nanofibers (CNFs) were prepared through TEMPO oxidation/ultrasound. The aerogel spheres derived from Salix psammophila (ASSP) were prepared with the hanging drop method. The experimental results showed that the Cu(II) adsorption capacity of the ASSP composite (267.64 mg/g) doped with TOCNF was significantly higher than that of pure cellulose aerogel spheres (52.75 mg/g). The presence of carboxyl and hydroxyl groups in ASSP enhanced the adsorption capacity of heavy metals. ASSP is an excellent heavy metal adsorbent, and its maximum adsorption values for Cu(II), Mn(II), and Zn(II) were found to be 272.69, 253.25, and 143.00 mg/g, respectively. The abandoned sand shrub resource of SP was used to adsorb heavy metals from effluent, which provides an important reference value for the development of forestry in this sandy area and will have a great application potential in the fields of the adsorption of heavy metals in soil and antibiotics in water.

25 January 2013 in Drying Technology
Verified
Journal Article
Closed access
RHRongfeng Huang
Rongfeng Huang
YWYanmei Wu
Yanmei Wu
YZYouke Zhao
Youke Zhao
JLJianxiong Lu
Jianxiong Lu
JJJiali Jiang
Jiali Jiang
ZCZhangjing Chen
Zhangjing Chen
Radio-frequency (RF) heating has been widely used in the wood industriesand it is essential to understand the factors affecting the heating rates. In this article, Chinese fir (Cunning hamialanceolata) was heated with RF energy intermittently at 2 min per cycle to study the effect of wood moisture content (MC), sample thickness, and RF power level on heating rates. The study revealed that wood MC significantly affected the RF heating rate (p < 0.01). The heating rate was the highest (5.0°C/cycle) at an MC around the wood fiber saturation point (FSP). The heating rates were lower with a lower MC of 15% (0.89°C/cycle) and a higher MC of 70% (1.2°C/cycle). Lumber thickness did not have a significant effect on the RF heating rate at the center of the lumber; however, the heating rates at various locations along the thickness direction were significantly different. The temperature at the lumber center was 20°C higher than the temperature at 10 mm below the surface during heating. The heating rate for lower RF power level was initially greater than the rate at higher power RF level and then rapidly decreased. However, the heating rate at the higher RF power level remained constant during the whole heating process. RF power levels had a significant effect on the internal heating rate of wood (p < 0.01).