A near-equiatomic FeCoNiCuAl High-entropy alloy (HEA) was produced using laser powder bed fusion (L-PBF) pre-alloy powder. Microstructural characteristics and tribological properties of L-PBF specimens under various volumetric energy densities (VEDs) were investigated in detail. The results showed that the phase of L-PBF specimen consisted of BCC matrix + Cu-rich B2 precipitate. The microstructure of L-PBF specimen largely consisted of columnar grains perpendicular to the melt pool boundary (MPB) direction owing to the epitaxial growth along the temperature gradient. The preferred orientation of the L-PBF specimen was gradually transformed from the order of to as the VED rose. Larger size precipitates re-appeared and wider MPB were formed upon faster remelting and steeper cooling as a result of higher VED. Compared to the components produced by Spark Plasma Sintering, L-PBF specimens presented better wear resistance owing to the ultra-fine substructure and nano-scaled precipitates. In addition, the L-PBF specimen produced with 83 J/mm3VED exhibits the highest elastic strain to failure (H/Er) and yield stress (H2/Er3).
Background: Even though the modulatory effects of Magnisum (Mg) and its alloys on bone-healing cells have been widely investigated during the last two decades, relatively limited attention has been paid on their inflammation-modulatory properties. Understanding the activation process of macrophages in response to the dynamic degradation process of Mg as well as the relationship between macrophage phenotypes and their osteogenic potential is critical for the design and development of advanced Mg-based or Mg-incorporated biomaterials. Methods: In this work, a Ti-0.625 Mg (wt.%) alloy fabricated by mechanical alloying (MA) and subsequent spark plasma sintering (SPS) was employed as a material model to explore the inflammatory response and osteogenic performance in vitro and in vivo by taking pure Ti as the control. The data analysis was performed following Student’s t-test. Results: The results revealed that the macrophages grown on the Ti-0.625 Mg alloy underwent sequential activation of M1 and M2 phenotypes during a culture period of 5 days. The initially increased environmental pH (~ 8.03) was responsible for the activation of M1 macrophages, while accumulated Mg 2+ within cells contributed to the lateral M2 phenotype activation. Both M1 and M2 macrophages promoted osteoblast-like SaOS-2 cell maturation. In vivo experiment further showed the better anti-inflammatory response, regenerative potentiality and thinner fibrous tissue layer for the Ti-0.625 Mg alloy than pure Ti. Conclusion: The results highlighted the roles of Mg degradation in the Ti-0.625 Mg alloy on the sequential activation of macrophage phenotypes and the importance of modulating M1-to-M2 transition in macrophage phenotypes for the design and development of inflammation-modulatory biomaterials.
Mussel-derived nacre and pearl, which are natural composites composed CaCO3 platelets and interplatelet organic matrix, have recently gained interest due to their osteogenic potential. The crystal form of CaCO3 could be either aragonite or vaterite depending on the characteristics of mineralization template within pearls. So far, little attention has been paid on the different osteogenic capacities between aragonite and vaterite pearl. In the current work, aragonite or vaterite pearl powders were incorporated into poly-l-lactic acid (PLLA) scaffold as bio-functional fillers for enhanced osteogenesis. In intro results revealed that PLLA/aragonite scaffold possessed stronger stimulatory effect on SaOS-2 cell proliferation and differentiation, evidenced by the enhanced cell viability, alkaline phosphatase activity, collagen synthesis and gene expressions of osteogenic markers including osteocalcin, osteopotin and bone sialoprotein. The bone regeneration potential of various scaffolds was evaluated in vivo employing a rabbit critical-sized radial bone defect model. The X-ray and micro-CT results showed that significant bone regeneration and bridging were achieved in defects implanted with composite scaffolds, while less bone formation and non-bridging were found for pure PLLA group. Histological evaluation using Masson's trichrome and hematoxylin/eosin (H&E) staining indicated a typical endochondral bone formation process conducted at defect sites treated with composite scaffolds. Through three-point bending test, the limbs implanted with PLLA/aragonite scaffold were found to bear significantly higher bending load compared to other two groups. Together, it is suggested that aragonite pearl has superior osteogenic capacity over vaterite pearl and PLLA/aragonite scaffold can be employed as a potential bone graft for bone regeneration.