Thin films by atomic layer deposition (ALD) raise global interest through unparalleled conformality. Saturation profiles of the archetypical trimethylaluminum-water ALD process in narrow rectangular channels create a benchmark for future studies.
Atomic layer deposition (ALD) is gaining attention as a catalyst preparation method able to produce metal (oxide, sulphide, etc.) nanoparticles of uniform size down to single atoms. This work reports our initial experiments to support nickel on mesoporous zirconia. Nickel (2,2,6,6-tetramethyl-3,5-heptanedionate)2 [Ni(thd)2] was reacted in a fixed-bed ALD reactor with zirconia, characterised with BET surface area of 72 m2/g and mean pore size of 14 nm. According to X-ray fluorescence measurements, the average nickel loading on the top part of the support bed was on the order of 1 wt%, corresponding to circa one nickel atom per square nanometre. Cross-sectional scanning electron microscopy combined with energy-dispersive spectroscopy confirmed that in the top part of the fixed support bed, nickel was distributed throughout the zirconia particles. X-ray photoelectron spectroscopy indicated the nickel oxidation state to be two. Organic thd ligands remained complete on the surface after the Ni(thd)2 reaction with zirconia, as followed with diffuse reflectance infrared Fourier transform spectroscopy. The ligands could be fully removed by oxidation at 400 °C. These initial results indicate that nickel catalysts on zirconia can likely be made by ALD. Before catalytic testing, in addition to increasing the nickel loading by repeated ALD cycles, optimization of the process parameters is required to ensure uniform distribution of nickel throughout the support bed and within the zirconia particles.
1 March 2026 in Journal of Vacuum Science & Technology A
Zinc oxide is a wide bandgap semiconductor with a variety of applications as a thin film material. In this work, a set of zinc oxide thin films were grown on lateral high-aspect-ratio test structures using atomic layer deposition. Diethylzinc and water were used as precursors, and several processing conditions were examined. The grown films were characterized for conformality using energy-dispersive electron probe x-ray microanalysis supported by x-ray reflectometry studies of additional reference samples. To analyze growth kinetics and film thickness profiles, diffusion-reaction simulations were made. Most importantly, it was found that at the 200 °C growth temperature, the film thickness profile followed nearly perfectly the ideal saturation profile expected for self-terminating reactions. The obtained result, thus, establishes an excellent reference case for process optimization.
Stable and conformal Ti–organic thin films from titanium isopropoxide and organic precursors (hydroquinone or benzene dicarboxylic acid) via ALD/MLD technique is reported; conformality is verified with lateral high-aspect-ratio structures.
1 September 2021 in Applied Surface Science Advances
The self-terminating chemistry of atomic layer deposition (ALD) ideally enables the growth of homogeneously distributed materials on an atomic scale. This study investigates the ALD of zinc oxide (ZnO) on mesoporous zirconium oxide (ZrO2) using zinc acetylacetonate [Zn(acac)2] and synthetic air in a fixed-bed powder ALD reactor. A broad variety of methods, including thermogravimetry analysis, scanning electron microscopy with energy dispersive X-ray spectroscopy, low energy ion scattering, X-ray absorption near edge structure, X-ray photoelectron spectroscopy, in situ diffuse reflectance infrared Fourier transform spectroscopy-mass spectrometry, and density functional theory calculations were used to analyze the reactant and the resulting samples. The factors affecting the zinc loading (wt%) on ZrO2 were investigated by varying the ALD reaction temperature (160 °C–240 °C), the calcination temperature of zirconium oxide (400 °C–1000 °C) and the ALD cycle number (up to three). The studied process showed self-terminating behavior, with the areal number density of zinc of approximately two atoms per square nanometer per cycle. Zinc was distributed throughout ZrO2. After the Zn(acac)2 reaction, acac ligands were removed using synthetic air at 500 °C. In the following cycles, the already-deposited ZnO acted as nuclei for further ZnO growth. This study demonstrates the potential of Zn(acac)2 as an ALD reactant and provides an initial understanding of ZnO growth via ALD on high surface area porous particles as an example for catalytic applications.