Energy-efficient memory elements having a non-volatile memory window (MW) with a non-destructive read operation are highly desirable for both random access memory and compute-in-memory applications. In this work, we demonstrate a record high non-volatile capacitive MW and non-destructive read in hafnium zirconate-based metal-ferroelectric-metal capacitors (FeCAPs). Firstly, we show that a non-zero capacitive MW at zero read voltage can be realized by engineering an asymmetry between the top and bottom ferroelectric-metal interfaces and demonstrate a record high MW of ~4.71×ϵ 0 at 0 V. Secondly, we show that the capacitive MW can be further improved by optimizing a non-zero read voltage. This allows to achieve a record high MW of ~7.5×ϵ 0 for the asymmetric FeCAP, and even opens up a MW as high as ~8.0×ϵ 0 for the symmetric FeCAP. Finally, we demonstrate that the MW can be reliably read non-destructively as long as the read voltage is carefully selected to avoid partial or full polarization switching during the read operation.
Integration density is one of the major criteria that ferroelectric (FE) capacitors must meet before they can be deployed in FeRAM memory arrays that can replace the conventional DRAM memories. In this work we demonstrate, for the first time, back-end-of-line compatible 3D-trench FE La doped hafnium zirconium oxide (HZO) based capacitors fabricated with a foot-print area of 200nm x 200nm for FeRAM applications. The capacitors are based on a trilayer stack (TiO2/La doped HZO/Nb2O5) with TiN as top and bottom electrodes. The initial wake-up of the films is dominated by domain de-pinning effect followed by other mechanisms. Pre-cycling scheme is demonstrated to wake-up the capacitor using higher bias (2.85V, 833KHz, $10^{{5}}$ cycles). Post wake-up, the device survives $10^{{12}}$ cycles with 2P $_{\text {R}}26~\mu \text{C}$ /cm2 till the end of endurance cycling. Retention measurements performed at $85^{\text {o}}\text{C}$ show retention of >70% of the initial polarization at the end of $10^{{5}}\text{s}$ and ~30% polarization is projected to remain at the end of 10 years. The retention was found to be limited by the imprint effect. Our demonstration brings HZO based FE capacitors one step closer to nonvolatile FeRAM applications.
Density functional theory predicts an abrupt drop in the stability, in the kinetic barrier for polarization reversal and spontaneous polarization of a ScxAl1−xN wurtzite phase, when the Sc:Al ratio approaches 50:50. The same effect is obtained by the application of a tensile strain. The resulting polarization reversal barrier correlates with experimental coercive fields, and highly textured film measurements exhibit polarization values close to the theoretically predicted ones. Film thickness below 5 nm has a significant impact on the elastic properties.
23 March 2023 in IEEE Transactions on Electron Devices
This article focuses on in- depth examination of the imprint effect in lanthanum-doped Hf $_{{0}.{5}}$ Zr0.5O2 (La:HZO) capacitors. The first part shows the imprint effect in a single positive up negative down (PUND) measurement caused by different delays between pulses. In addition, a unique wake-up reversal behavior (i.e., current peak split in the ${I}$ ,– ${V}$ curve and pinched ${P}$ ,– ${V}$ loop) induced by imprint has been investigated in devices with two different prepolarized states (positive and negative). The results have shown that this behavior is accelerated by the bake temperature. Quantitative evaluation of the observed current peak split at each bake time and bake temperature yielded activation energy, suggesting that the wake-up reversal is due to oxygen vacancy redistribution. Moreover, corresponding models explaining how these charged defects and the polarization dipoles interact at each measurement step are proposed. Lastly, analysis of temperature-dependent field cycling characteristics suggests that the degraded wake-up of La:HZO film at high temperature can be attributed to the wake-up reversal effect being concurrent with wake-up.
15 May 2018 in IEEE Journal of the Electron Devices Society
Discrepancies exist between the theoretically predicted and experimentally measured performance of band-to-band tunneling devices, such as Esaki diodes and tunnel field-effect transistors (TFETs). We resolve this discrepancy for highly-doped, direct-bandgap Esaki diodes by successfully calibrating a semi-classical model for high-doping-induced ballistic band-tails tunneling currents at multiple temperatures with two In0.53Ga0.47As Esaki diodes using their SIMS doping profiles, C-V characteristics and their forward-bias current density in the negative differential resistance (NDR) regime. The current swing in the NDR regime is shown not to be linked to the band-tails Urbach energy. We further demonstrate theoretically that the calibrated band-tails contribution is also the dominant band-tails contribution to the subthreshold swing of the corresponding TFETs. Lastly, we verify that the presented procedure is applicable to all direct-bandgap semiconductors by successfully applying it to InAs Esaki diodes in literature.