We attempted to clarify relationship between grain boundary structures in Si multicrystals and generation of dislocations during crystal growth. Systematic variation of grain boundary structures was realized by employing dendritic nucleation at the initial stage of crystal growth. Etch-pit observation revealed that the contact angle of adjacent dendrite crystals to form a grain boundary affects generation of dislocations. Experimentally observed dislocation density was found to be well correlated with shear stress around the grain boundary calculated by finite element analysis.
β-Ga2O3 is a well-known semiconductor material for power devices and other applications. Recently, β-Ga2O3 has also been reported as a scintillator material with a light yield of approximately 8400 ph./MeV, scintillation decay time of <1 μs, and density of 6.44 g/cm3. In this study, 45 cm diameter β-Ga2O3 single crystals were prepared via oxide crystal growth using the cold crucible (OCCC) method under various oxygen partial pressures. In the OCCC method, as in the cold crucible method, a high frequency is applied directly to the oxide materials, which are heated and melted, and the melt is held by the outermost solid material itself that is cooled by water using a copper hearth. In the OCCC method, crystal growth is performed while rotating the seed crystal, as in the Czochralski method, to increase the crystal diameter. The optical properties and radiation responses of the crystals grown under various oxygen partial pressures were evaluated.
We investigated impact of type of crystal defects in multicrystalline Si (mc-Si) on electrical properties and their change after gettering process of impurities. A bundle of dislocations gives negative impact on the gettering process, while grain boundaries does not affect at all. In addition, we categorized random grain boundaries in mc-Si by the contact angle between adjacent dendrite crystals to form the grain boundary. Change in the contrast of photoluminescence intensity around the grain boundary was found to systematically vary by the contact angle, which showed good correlation with calculated interface energy of the grain boundary. Grain boundaries with low interface energy are concluded to be preferable to weaken recombination activity by the gettering process and improvement of solar cell performance based on mc-Si.
We carried out small-scale crystal growth experiment to apply faceted dendrite growth at the top of the melt to floating cast method in order to grow high-quality multicrystalline Si (mc-Si) ingot for solar cells. By appropriate cooling at the initial stage, the most part of the top surface was covered by a single faceted dendrite crystal followed by directional solidification from the top to the bottom. As a consequence, the cross-section of the ingot was dominated by a single crystal grain. The crystal grain was found to be almost free from subgrain boundaries as evidenced by spatially resolved single-peak x-ray rocking curve profiles. The minority carrier diffusion length was found to be much longer than that in a control sample grown from the bottom to the top presumably due to the minimized contact with the crucible wall. This shows that the floating cast method combined with formation of faceted dendrite crystals at the initial stage is a promising route to realize high-quality mc-Si ingot for high-efficiency solar cells.