12 July 2022 in Advances in Materials Science and Engineering
The impacts of three diameter/thickness (D/t) ratios (21.22, 25.46, and 31.83) and concrete strengths (40N/mm2, 50N/mm2, and 60N/mm2) on the strength capabilities of concrete-filled steel tubular (CFST) columns are investigated in this study. The central composite design (CCD) of the response surface methodology (RSM) was used to design the trials in order to complete the tests in a cost-effective manner. 13 (9 distinct tests) columns were evaluated according to the CCD experimental design, and the failure mode of the specimens, loaddeformation behavior, and ultimate strength capacity were investigated. Concrete strength improves, resulting in a decrease in steel tube confinement on the core. Because the steel tube longitudinal compressive stress (fsl) increases as the D/t ratio lowers, the confinement is reduced by inhibiting the circumferential tensile stress (fsc). The Reynolds stress models, analysis of variance (ANOVA), Pareto chart, and contour plot demonstrated that the column D/t ratio, rather than the in-filled concrete strength, has a considerable impact on the CFST columns strength capability. The proposed design models in different international codes and literature were evaluated for their effectiveness in predicting the strength capacities of CFST columns subjected to axial compression load. Using regression analysis, a simple design model was suggested to predict the axial strength capacities of CFST short columns, taking into account material strength and column shape. In comparison to other existing and suggested design models, the proposed design model of the present study delivers a more accurate and stable forecast.
1 January 2025 in Matéria (Rio de Janeiro)
A novel study on fibre-reinforced cement less geopolymer concrete with diverse molar concentrations has gained attention in recent years. The current study uniquely explores the combined influence of four distinct molar concentrations (6M, 8M, 10M, and 12M) and five fibre volume fractions (0%, 0.25%, 0.50%, 0.75%, and 1%) on the mechanical behaviour of GPC. An experimental investigation on 20 numbers of varied geopolymer concrete mixes was performed, and the mechanical properties were evaluated and reported. Also, A non-destructive test using ultrasonic pulse velocity was made, and the regression analysis with compressive strength is reported. The result indicates that 10M concentration provides the optimum results than other molar concentrations, with 0.75% as the optimum basalt fibre volume addition to the cementless geopolymer concrete. The basalt fibre addition improves the split tensile strength and flexural bending strengths considerably. Morphology studies indicate that the lower molar concentration gives a comparatively loose and voided concrete matrix with a loose packing of ingredients than the higher molar concentration. This research provides a comprehensive and optimised approach by simultaneous variation of Molar concentration and fibre volume to enhance geopolymer concrete, supported by both mechanical investigation and microstructural analysis.