Surface passivation effects were studied on AlGaN/GaN high-electron-mobility transistors (HEMTs) using and silicon oxynitride (SiON) formed by plasma enhanced chemical vapor deposition. An increase of and has been observed on the passivated and SiON) HEMTs when compared with the unpassivated HEMTs. About an order of magnitude low and three orders of magnitude high was observed on and passivated HEMTs, respectively, when compared with the unpassivated HEMTs. The increase of is due to the occurrence of surface related traps, which was confirmed by the observation of kink and hysteresis effect on dc and ac characteristics, respectively. Though the passivated HEMTs show better dc characteristics, the breakdown voltage characteristics are not comparable with SiON passivated and unpassivated HEMTs. The SiON is also a very promising candidate as a surface passivant for AlGaN/GaN HEMTs because it shows better with low hysteresis width and small collapse than passivated HEMTs.
The electrical properties of electron beam (EB) evaporated silicon dioxide plasma enhanced chemical vapor deposited (PECVD) and PECVD silicon nitride interfaces were investigated using high frequency capacitance–voltage measurements. Compositions of the deposited insulating layers and were analyzed using x-ray photoelectron spectroscopy. Metal-insulator-semiconductor structures were fabricated on the metalorganic chemical vapor deposition grown n-type GaN layers using EB, PECVD grown and PECVD grown layers. Minimum interface state density has been observed in the PECVD grown interface when it was compared with EB evaporated interface and PECVD interface The interface state density depends on the composition of deposited insulating layers.
The surface leakage currents and the surface trapping effects of the AlGaN/GaN high electron mobility transistors (HEMTs) on silicon with different passivation schemes, namely, a 120 nm plasma enhanced chemical vapor deposited SiN, a 10 nm atomic layer deposited (ALD) and a bilayer of (120/10 nm) have been investigated. After SiN passivation, the surface leakage current of the GaN HEMT was found to increase by about six orders; while it only increased by three orders after the insertion of between SiN and AlGaN/GaN. The surface conduction mechanism is believed to be the two-dimensional variable range hopping for all the samples. The leakage current in the etched GaN buffer layer with bilayer passivation was also much smaller than that with only SiN passivation. The pulse measurement shows that the bilayer of passivation scheme can effectively reduce the surface states and suppress the trapping effects.
The high-electron-mobility transistors (HEMTs) have been demonstrated on both sapphire and semi-insulating (SI) SiC substrates, and the dc characteristics of the fabricated devices were examined at temperatures ranging from 25 to 500 °C. The decrease in drain current and the transconductance with the increase of temperature have been observed. The decrease ratio of transconductance and drain current was similar for both the HEMTs on sapphire and SI–SiC substrates at and above 300 °C. The HEMTs on SiC substrates showed better dc characteristics after being subjected to thermal stress up to 500 °C. Although the SiC-based HEMTs showed better characteristics up to the temperature of 300 °C, compared with the sapphire-based HEMTs, similar dc characteristics were observed on both at and above 300 °C. For high-temperature applications (⩾300 °C), additional cooling arrangements are essential for both devices.
Enhancement of breakdown voltage (BV) with the increase of AlN buffer layer thickness was observed in AlGaN∕GaN high-electron-mobility transistors (HEMTs) grown by metalorganic chemical vapor deposition on 4in. Si. The enhancement of device performance with AlN buffer thickness (200 and 300nm) is due to the reduction of electrically active defects from Si substrate. The reduction of defects from Si with the increase of AlN thickness was confirmed by x-ray rocking curve measurements. Not much change has been observed in ON-state BV (BV:ON) values except in devices with 500-nm-thick buffer layer. About 46% enhancement in OFF-state BV (BV:OFF) was observed on 200μm wide HEMTs with 300nm thick AlN buffer layer when compared to HEMTs with 8nm thick AlN buffer layer. The location of junction breakdown in the device was identified as GaN∕AlN∕Si interface. The measured specific on-resistance (Ron) values for 200 and 400μm wide HEMTs with 300nm thick buffer layers were 0.28 and 0.33mΩcm2, respectively. About an order of low Ron was observed when compared with the reported values. The AlGaN∕GaN HEMTs on 4in. Si with thicker AlN buffer layers are suitable for high-power applications.
This Letter reports on the epitaxial growth, characterization, and device characteristics of crack-free AlGaN/GaN heterostructures on a 200 mm diameter Si(111) substrate. The total nitride stack thickness of the sample grown by the metal-organic chemical vapor deposition technique is about 3.3 ± 0.1 μm. The structural and optical properties of these layers are studied by cross-sectional scanning transmission electron microscopy, high-resolution x-ray diffraction, photoluminescence, and micro-Raman spectroscopy techniques. The top AlGaN/GaN heterointerfaces reveal the formation of a two-dimensional electron gas with average Hall mobility values in the range of 1800 to 1900 cm2/Vs across such 200 mm diameter GaN on Si(111) samples. The fabricated 1.5 μm-gate AlGaN/GaN high-electron-mobility transistors exhibited the drain current density of 660 mA/mm and extrinsic transconductance of 210 mS/mm. These experimental results show immense potential of 200-mm diameter GaN-on-silicon technology for electronic device applications.