Engineering Institute of Advanced Manufacturing and Modern Equipment Technology, Jiangsu University, Jiangsu University, No. 301,Xuefu Road, Jingkou District, Zhenjiang, 212013, People's Republic of China, Zhenjiang, CHINA
Auto-generated profile, based on publicly available information
Chenyu Zhu
Engineering Institute of Advanced Manufacturing and Modern Equipment Technology, Jiangsu University, Jiangsu University, No. 301,Xuefu Road, Jingkou District, Zhenjiang, 212013, People's Republic of China, Zhenjiang, CHINA
Al-Zn-Mg-Cu extruded aluminum alloy was processed by multistage solid solution aging process to obtain excellent mechanical properties.Such as Strength, plasticity, corrosion resistance,and the microstructure and properties of the materials were characterized by metallographic microscope,XRD,hv-1000 microhardness tester and wdw-200 microcomputer controlled universal testing machine.The experimental results show that the aging temperature T7X-1 has lower strength but higher plasticity compared with T6.With the increase of the solid solution temperature, the strength showed a certain regularity, the maximum tensile strength of the alloy can reach 787.1 MPa.The multi-stage solid solution process can increase the dislocation density and improve the intergranular corrosion resistance of the alloy.And by comparison, the alloy in the solution treatment system (460 ℃×2 h+470 ℃×2 h+480 ℃×2 h and aging system(121 ℃×5 h+153 ℃×16 h) heat treatment state has a good comprehensive mechanical properties.
Effect of Mg on microstructure and properties of 7000 high strength rolled aluminum alloy was studied by XRD and EBSD analysis, hardness and electric conductivity test, tensile test and intergranular corrosion experiments. The results show that for Al-8.95Zn-(1.9~2.6)Mg-1.18Cu-0.44Zr 7000 series aluminum alloy, it has excellent comprehensive performance in T76 state with high tensile strength of 585~645MPa and elongation of 10.2~15.4%, and the resistance to intergranular corrosion is excellent(≤ 72μm). When the content of Mg is 2.21%, the aluminum alloy has the highest degree of recrystallization, and the strength and elongation rates of aluminum alloy with T6 and T76 aging state can reach 651.7MPa and 10.7%, 645.6MPa and 15.4%, respectively, but the resistance to intergranular corrosion is relatively poor. At the same time, the resistance to intergranular corrosion of the alloy decreases as the degree of recrystallization increases.