25 October 2024 in IEEE Transactions on Electron Devices
A novel doping technique with an initiated chemical vapor deposition (iCVD) process is applied to fabricate aluminum (Al)-doped zinc oxide (ZnO) channel thin-film ultraviolet (UV) phototransistor (PT). The iCVD doping technique can successfully introduce Al throughout the ZnO channel without any surface damage. The sub-bandgap states mainly due to oxygen vacancy (V $_{\text{O}}$ ) defects in the ZnO channel are effectively suppressed by Al doping; the subthreshold swing (SS) of the PT has been reduced by more than half to 168 mV/dec and under negative gate bias illumination stress, the threshold voltage shift is reduced by about half to $-$ 2.03 V, which improves the reliability. For the UV detection, the Al-doped ZnO PT exhibits a high responsivity of 358.93 A $\cdot$ W $^{-\text{1}}$ , an ultrahigh UV-to-visible rejection ratio of 4.81 $\times$ 10 $^{\text{6}}$ , a high detectivity ( D $^\ast)$ of 1.68 $\times$ 10 $^{\text{15}}$ Jones, a low noise equivalent power (NEP) of 2.98 $\times$ 10 $^{-\text{18}}$ W $\cdot$ Hz $^{-\text{1}}$ , and fast switching performance. The developed Al-doped ZnO PT can be used in low-cost and high-performed UV detection for various applications.
28 January 2026 in IEEE Transactions on Electron Devices
It is demonstrated that interface engineering in ZnO-based ultraviolet (UV) photodetectors (PDs) using an asymmetric Al2O3 interlayer can significantly enhance PD performance. The Al2O3 layer deposited by atomic layer deposition (ALD) only at the cathode/ZnO interface extends the electron tunneling distance and passivates oxygen vacancy ( ${V}_{\text{O}}$ )-related traps on the ZnO surface. This effectively suppresses the dark current ( ${I}_{\text {dark}}$ ), while the photocurrent ( ${I}_{\text {photo}}$ ) remains high due to the absence of the Al2O3 layer in the anode region. An asymmetric ZnO metal–insulator–semiconductor–metal (MISM) PD with an optimized Al2O3 layer thickness of 4 nm exhibits a high photo-to-dark current ratio (PDCR) of $2.31\times 10^{{5}}$ , a high specific detectivity of $7.80\times 10^{{14}}$ Jones, a rapid decay time of 0.12 s, and excellent performance in harsh environments.
13 April 2026 in Applied Physics Letters
In this work, a NiO/β-Ga2O3 heterojunction diode with an ultrathin (∼2 nm) amorphous boron nitride (a-BN) interfacial layer (IL) is presented. The NiO/a-BN/β-Ga2O3 heterojunction diode exhibited a lower turn-on voltage and a higher forward current, thereby reducing the power dissipation, compared to the NiO/β-Ga2O3 diode without an a-BN IL. It is also found that the a-BN IL reduces the interface states, leading to the improvement of the operational reliability after bias stress and reverse blocking characteristics.
5 December 2025 in IEEE Transactions on Electron Devices
Nanosecond annealing using a pulsed green laser is proposed to activate the source/drain of top-tier p-channel metal-oxide-semiconductor field-effect transistors (pMOSFETs) while avoiding the degradation of preexisting bottom-tier devices. Localized high temperatures generated by green laser annealing (GLA) in the top-tier layer improve crystallinity and increase the activated boron concentration in the source/drain of top-tier pMOSFETs compared to conventional rapid thermal annealing (RTA). These improvements result in a reduction of sheet resistance ( ${R}_{\text {sh}}\text {)}$ and specific contact resistivity ( $\rho _{\text {c}}\text {)}$ , thereby increasing the effective mobility ( $\mu _{\text {eff}}\text {)}$ of the top-tier Ge pMOSFETs by approximately 46%. As a result, heterogeneous 3-D sequential CFETs integrated using GLA achieve a high voltage gain ( ${V}_{\text {gain}}\text {)}$ of 68 V/V.
1 October 2026 in IEEE Transactions on Electron Devices