1 December 2020 in Dental Materials
Verified
Journal Article
Closed access
GGGenine Moreira de Freitas Guimarães
Genine Moreira de Freitas Guimarães
EBErika Soares Bronze-Uhle
Erika Soares Bronze-Uhle
PLPaulo Noronha Lisboa-Filho
Paulo Noronha Lisboa-Filho
AFAna Paula Piovezan Fugolin
Ana Paula Piovezan Fugolin
ABAna Flavia Sanches Borges
Ana Flavia Sanches Borges
AFAdilson Yoshio Furuse
Adilson Yoshio Furuse

26 September 2022 in Journal of Esthetic and Restorative Dentistry
Verified
Journal Article
Closed access
MVMariele Vertuan
Mariele Vertuan
VMVictor Mosquim
Victor Mosquim
GGGenine Moreira de Freitas Guimarães
Genine Moreira de Freitas Guimarães
AOAlyssa Teixeira Obeid
Alyssa Teixeira Obeid
JBJuliana Fraga Soares Bombonatti
Juliana Fraga Soares Bombonatti
AFAdilson Yoshio Furuse
Adilson Yoshio Furuse

9 March 2020 in Brazilian Journal of Oral Sciences
Verified
Journal Article
Open access
PDF file
AFAdilson Yoshio Furuse
Adilson Yoshio Furuse
CNConstantino Fernandes Neto
Constantino Fernandes Neto
GGGenine Moreira de Freitas Guimarães
Genine Moreira de Freitas Guimarães
BTBianca Rodrigues Terrabuio
Bianca Rodrigues Terrabuio
FRFabio Antonio Piola Rizzante
Fabio Antonio Piola Rizzante
LWLinda Wang
Linda Wang
Aim: To evaluate the color stability of bovine enamel with artificial white spot lesions treated with resin infiltration (ICON) or remineralization with fluoride using two storage methods. Methods: Sixty incisors were submitted to artificial white spot lesion induced by demineralization-remineralization (DE-RE) cycling. Initial color was evaluated with CIE-Lab to measure ΔEab. Demineralized teeth were divided according to the treatment of the white spot lesion (n = 20): 1) Remineralization with 2% neutral fluoride gel for 4min (control); 2) ICON application following manufacturer’s recommendations; and 3) ICON with decreased drying time after the application of ethanol. After 24h, color was evaluated and samples were subdivided (n = 10) according to storage: 1) distilled water for 1 month; 2) grape juice for 10min daily. After storage, color was evaluated. L*, a* and b* data were analyzed by one-way ANOVA and ∆Eab data by two-way ANOVA followed by Tukey’s HSD (α = 0.05). Results: L* was affected by juice storage, and decreased when ICON was applied with decreased drying time after the ethanol application. The same behavior occurred with a* (increase with reduced drying time), while b* was not affected. For ∆Eab significant differences were observed between groups (p = 0.0219) and storage methods (p = 0.0007). There was no interaction effect (p = 0.1118). Remineralization with fluoride presented the lowest color changes after storage in water. Conclusion: Treatment of artificial carious lesions with resin infiltration presented greater color changes than fluoride remineralization after storage in both solutions in vitro.

8 February 2021 in Brazilian Journal of Oral Sciences
Verified
Journal Article
Open access
PDF file
GGGenine Moreira de Freitas Guimarães
Genine Moreira de Freitas Guimarães
KMKarin Cristina da Silva Modena
Karin Cristina da Silva Modena
CSCarolina Yoshi Campos Sugio
Carolina Yoshi Campos Sugio
TBTamires de Luccas Bueno
Tamires de Luccas Bueno
MAMaria Angélica Silvério Agulhari
Maria Angélica Silvério Agulhari
MAMaria Teresa Atta
Maria Teresa Atta
Aim: The aim of this study was to compare the microtensile bond strength (μTBS) and the characteristics of the adhesive interface of Scotchbond Universal - SU – etch-and-rise mode (3M ESPE) and Adper Scotchbond Multi-Purpose - MP (3M ESPE) to dentin over time. Methods: Class I cavity preparations were performed in 60 human molars that were randomly divided according to the dentin bonding system (DBS) used (n=30): (1) Acid conditioning + SU and (2) Acid conditioning + MP. For bonding strength (BS) analysis, 30 teeth (n = 15) were sectioned into sticks and submitted to the microtensile test in a universal testing machine after 24 hours and 12 months. The adhesive interface of the others 30 teeth was analyzed in a confocal microscope after 24 hours and 12 months. The data of μTBS were analyzed by two-way repeated measures ANOVA and Tukey’s HSD (α = 0.05). Results: SU presented the lowest DBS compared to MP (p=0.000). Time did not influenced DBS for both adhesive systems (p=0.177). Confocal microscopy analysis showed no cracks between both adhesive systems tested. Conclusion: The results indicate that MP - μTBS showed a better performance compared to SU in total-etch mode.

3 November 2026 in Journal of Dentistry
Verified
Journal Article
Closed access
GGGenine Moreira Freitas Guimarães
Genine Moreira Freitas Guimarães
FLFernanda Sandes de Lucena
Fernanda Sandes de Lucena
SLSteven Lewis
Steven Lewis
AFAdilson Yoshio Furuse
Adilson Yoshio Furuse
CPCarmem S Pfeifer
Carmem S Pfeifer

13 September 2018 in RSBO
Verified
Journal Article
Open access
PDF file
GNGisele Maria Correr Nolasco
Gisele Maria Correr Nolasco
GGGenine Moreira De Freitas Guimarães
Genine Moreira De Freitas Guimarães
RBRicardo Bressan
Ricardo Bressan
RRRafaella Ronchi
Rafaella Ronchi
CGCarla Castiglia Gonzaga
Carla Castiglia Gonzaga
OBOctávio Pinheiro Brisola
Octávio Pinheiro Brisola
Introduction: Lithium disilicate reinforced glass ceramics are materials that require good adhesion to ensure clinical success. Objective: To evaluate the bond strength of resin cements to lithium-disilicateenhanced vitroceramics using different cleaning techniques of recently conditioned ceramics. Material and methods: Twelve ceramic discs (IPS Empress II) were made and inserted into PVC pipes using acrylic resin. The ceramic surface was designed and submitted to a 10% hydrofluoric acid conditioning process for 20s. Then, the specimenswere divided into 3 groups (n = 16) according to the cleaning techniques of recently conditioned ceramics: 1) control - conventional technique (no cleaning after the conditioning process); 2) application of 37% phosphoric acid for 20s; 3) 90% ethyl alcohol bath in a ultrasound tub for 4 min. After cleaning, the silane agent was applied for 1 minute and silicon matrices (1 mm in diameter x 1 mm in height) were made for further application of the resin cement (Vitique, DMG), which was handled according to the manufacturer’s instructions. Four cylinders were prepared on each ceramic surface. The specimens were storedin distilled water for 48 hours and subjected to the micro-shear test in a universal testing machine. After the micro-shear test, a failure analysis of the specimens was performed. Data were submitted to ANOVA (analysis of variance for a criterion) with a significance level of 5%. Results: There was no significant difference between groups (p > 0.05). Conclusion: the cleaning technique of the recently conditioned ceramics does not interfere with the resin/cement bond strength values