Bioactive manganese (Mn)-doped ceramic coatings for intraosseous titanium (Ti) implants are developed. Arc plasma deposition procedure is used for coatings preparation. X-ray Diffraction, Scanning Electron Microscopy-Energy Dispersive X-ray Spectroscopy, and Electron Paramagnetic Resonance (EPR) methods are applied for coatings characterization. The coatings are homogeneous, composed of the main phase α-tricalcium phosphate (α-TCP) (about 67%) and the minor phase hydroxyapatite (about 33%), and the Mn content is 2.3 wt%. EPR spectroscopy demonstrates that the Mn ions are incorporated in the TCP structure and are present in the coating in Mn2+ and Mn3+ oxidation states, being aggregated in clusters. The wetting contact angle of the deposited coatings is suitable for cells’ adhesion and proliferation. In vitro soaking in physiological solution for 90 days leads to a drastic change in phase composition; the transformation into calcium carbonate and octacalcium phosphate takes place, and no more Mn is present. The absence of antibacterial activity against Escherichia coli, Enterococcus faecalis, and Pseudomonas aeruginosa bacteria strains is observed. A study of the metabolic activity of mouse fibroblasts of the NCTC L929 cell line on the coatings using the MTT (dye compound 3-(4,5-Dimethylthiazol-2-yl)-2,5-diphenyltetrazolium bromide) test demonstrates that there is no toxic effect on the cell culture. Moreover, the coating material supports the adhesion and proliferation of the cells. A good adhesion, spreading, and proliferative activity of the human tooth postnatal dental pulp stem cells (DPSC) is demonstrated. The developed coatings are promising for implant application in orthopedics and dentistry.
1 May 2016 in Inorganic Materials: Applied Research
Four types of three-dimensional plasma capillary-porous titanium coatings for model intraosseous implants are developed. By means of pulsed microplasma oxidation in solutions or plasma spraying of...
1 July 2016 in Inorganic Materials: Applied Research
The effect of the heating of a Ti substrate to 300 and 550°C on the microhardness of a hydroxyapatite (HA) plasma coating, Ti, and their interface is investigated in specimens in different states (as sprayed, after hydrothermal (650°C, 3 h) and vacuum heat treatment (800, 1000, 1100°C, 3 h)). It is shown that the preliminary heating of the substrate to 550°C leads to the interface microhardness increasing from 2.32 to 3.07 GPa, while the following heat treatment has a weak influence on that. After the heat treatment, the microhardness of the HA coating is increased from 3.0 to 3.8 GPa and the microhardness of the Ti substrate near the boundary is increased from 2.5 to 6.9 GPa. A slight effect of the heat treatment on the interface microhardness is explained by preservation of the interface structure formed under HA plasma spraying on the heated substrate. The distribution of chemical elements near the interface between the coating and substrate is studied by Auger electron spectroscopy (AES).