Bioactive manganese (Mn)-doped ceramic coatings for intraosseous titanium (Ti) implants are developed. Arc plasma deposition procedure is used for coatings preparation. X-ray Diffraction, Scanning Electron Microscopy-Energy Dispersive X-ray Spectroscopy, and Electron Paramagnetic Resonance (EPR) methods are applied for coatings characterization. The coatings are homogeneous, composed of the main phase α-tricalcium phosphate (α-TCP) (about 67%) and the minor phase hydroxyapatite (about 33%), and the Mn content is 2.3 wt%. EPR spectroscopy demonstrates that the Mn ions are incorporated in the TCP structure and are present in the coating in Mn2+ and Mn3+ oxidation states, being aggregated in clusters. The wetting contact angle of the deposited coatings is suitable for cells’ adhesion and proliferation. In vitro soaking in physiological solution for 90 days leads to a drastic change in phase composition; the transformation into calcium carbonate and octacalcium phosphate takes place, and no more Mn is present. The absence of antibacterial activity against Escherichia coli, Enterococcus faecalis, and Pseudomonas aeruginosa bacteria strains is observed. A study of the metabolic activity of mouse fibroblasts of the NCTC L929 cell line on the coatings using the MTT (dye compound 3-(4,5-Dimethylthiazol-2-yl)-2,5-diphenyltetrazolium bromide) test demonstrates that there is no toxic effect on the cell culture. Moreover, the coating material supports the adhesion and proliferation of the cells. A good adhesion, spreading, and proliferative activity of the human tooth postnatal dental pulp stem cells (DPSC) is demonstrated. The developed coatings are promising for implant application in orthopedics and dentistry.
1 March 2016 in Materials Science and Engineering: C
A Ti–25Nb–13Ta–5Zr alloy was produced and studied in this work, and plates and wires were made from this alloy. It is shown that the Ti–25Nb–13Ta–5Zr alloy has the required mechanical properties and a β-crystal phase. Microstructures were present on the surface of the alloy with a height of several hundred nm, located at a distance of 1.5–2 μm from each other. Ti–25Nb–13Ta–5Zr was superior to nitinol in terms of the formation of long-living reactive protein species and the generation of reactive oxygen species. Cell cultivation on Ti–25Nb–13Ta–5Zr alloy surfaces revealed a significant mitotic index (2%) and a small number of nonviable cells (<5%). The cells were actively attached and spread over the alloy. The biocompatibility of Ti–25Nb–13Ta–5Zr was verified by experiments on the implantation of the alloy in the form of plates and coiled wires. The surface morphology of the specimens after biological trials was not significantly altered. The experimental data we obtained suggest that Ti–25Nb–13Ta–5Zr is suitable for potential applications in biology and medicine.
1 May 2013 in Inorganic Materials: Applied Research
The processes of thermoplastic treatment of plasma sprayed coatings made of 10R6M5 high speed steel, Kh20N80 nichrome, FBKh6-2 cast iron, and WC-Co and TiC-NiMo cermets upon resistance spot welding...
Phosphate coatings have been produced by plasma-spraying hydroxyapatite (HA) and tricalcium phosphate (TCP) powders onto Ti substrates at initial temperatures of 20, 300, and 550°C, followed by hydrothermal treatment (HTT) at 650°C, and the variation in the phase composition of the coatings has been examined in relation to the phase composition of the plasma-sprayed powders: 100 wt % HA, 100 wt % α‑TCP, and 100 wt % β-TCP. The as-prepared coatings produced by plasma-spraying the HA powder consisted of 87–91 wt % HA and 9–13 wt % CaO, and after HTT their phase composition was 89–93 wt % HA and 7–11 wt % CaO. The coatings produced by plasma-spraying the α-TCP powder at initial substrate temperatures from 20 to 550°C consisted entirely of a crystalline α-TCP phase. The coatings produced by plasma-spraying the β-TCP powder consisted of both β-TCP and α-TCP, and the content of the latter phase decreased from 100 to 80% as the substrate temperature was raised from 20 to 550°C. After HTT, the coatings contained 26–28% HA, independent of the phase composition of the starting TCP powders.
About Me
Baikov Institute of Metallurgy and Materials Science RAS
Baikov Institute of Metallurgy and Materials Science RAS